Trends in the development of modern manufacturing technologies and methods for improving the surface properties of magnesium alloys (review)

Uridiya Z.P., Tokarev M.S., Leonov A.A., Trofimov N.V.
Uridiya Z.P., Tokarev M.S., Leonov A.A., Trofimov N.V. Trends in the development of modern manufacturing technologies and methods for improving the surface properties of magnesium alloys (review) // Proceedings of VIAM. 2022. No. 11. DOI: 10.18577/2307-6046-2022-0-11-37-47. URL: https://www.viam-works.ru/en/journal/2022/11/4
Keywords
magnesium alloy, additive manufacturing, selective laser melting, laser cladding and sputtering, gas-dynamic spraying
Abstract

The trends of modern technologies for the manufacture of magnesium alloys and products from them are considered. The results of research and developed technologies of foreign scientists and world companies in the field of magnesium alloys and magnesium-based materials are presented. Research is focused on selective laser melting (SLM), since it is possible to form high-precision parts of any shape with it help. The fine magnesium or magnesium alloy powders used for SLM are difficult to manufacture due to their rapid oxidation. In connection with this feature, more and more attention is paid to the technology of using wire. The review considers such technologies as laser cladding and gas-dynamic spraying. The presented research and development will expand the scope of application and, in the future, master improved traditional and modern promising additive technologies.

Reference list
  1. Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), paper no. 03. Available at: http://www.journal.viam.ru (accessed: May 11, 2022). DOI: 10.18577/2713-0193-2021-0-2-24-34.
  2. Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kablov E.N., Lukina E.A., Zavodov A.V., Efimochkin I.Yu. The formation of structure in ultrafine WC–Cо carbide material in the presence of inhibitory additives. Trudy VIAM, 2020, no. 4–5 (88), paper no. 10. Available at: http://www.viam-works.ru (accessed: May 05, 2022). DOI: 10.18577/2307-6046-2020-0-45-89-99.
  5. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  6. Kozlov I.A., Vinogradov S.S., Tarasova K.G., Kulyushina N.V., Manchenko V.A. Plasma electrolytic oxidation of magnesium alloys (review). Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 23–36. DOI: 10.18577/2071-9140-2019-0-1-23-36.
  7. Istomin A.V., Kolyshev S.G. Electrostatic method of forming ultrathin fibers of refractory oxides. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 40–46. DOI: 10.18577/2071-9140-2019-0-2-40-46.
  8. Song B., Dong S., Zhang B., Liao H., Coddet C. Effects of processing parameters on microstructure and mechanical property of selective laser melted Ti6Al4V. Materials Desing, 2012, no. 35, pp. 120–125.
  9. Takagi H., Sasahara H., Abe T. et al. Material-property evaluation of magnesium alloys fabricated using wire-and-arcbased additive manufacturing. Additive Manufacturing, 2018, no. 24, pp. 498–507.
  10. Wei K., Wang Z., Zeng X. Influence of element vaporization on formability, composition, microstructure, and mechanical performance of the selective laser melted Mg–Zn–Zr components. Materials letters, 2015, no. 156, pp. 187–190.
  11. Bär F., Berger L., Jauer L. et al. Laser additive manufacturing of biodegradable magnesium alloy WE43: a detailed microstructure analysis. Acta Biomaterialia, 2019, no. 98, pp. 36–49.
  12. Manakari V., Parande G., Gupta M. Selective laser melting of magnesium powders and magnesium alloys. Review. Metally, 2016, no. 7, pp. 2–3.
  13. Lin X., Huang W. Highly efficient metal additive manufacturing technology applied in the field of aviation. Materials China, 2015, no. 34, pp. 684–688.
  14. Dong H., Yong B., Chjan D. et al. Experimental study of selective laser melting of bulk pure. Manufacturing process, 2015, no. 30, pp. 1298–1304.
  15. Guo J., Zhou Y., Liu K. et al. Additive manufacturing by magnesium alloy AZ31 wire arc: grain grinding by adjusting pulse frequency. Materials, 2016, no. 9, pp. 823–824.
  16. Knezovis N., Topis A. Additive production of wire and arc – new achievement in production. Springer international publishing, 2019, no. 36, p. 65–71.
  17. Zhang H., Hu S., Wang Z., Liang Y. The effect of welding speed on the microstructures of the deposited coating of magnesium alloy AZ31 by cold metal transfer. Materials Design, 2015, no. 86, pp. 894–901.
  18. Hu S., Zhang H., Wang Z. et al. Arc characteristics during cold metal transfer welding with magnesium alloy wire AZ31. Journal Manufacturing process, 2016, no. 24, pp. 298–306.
  19. Vyasaraj M., Gururaj P., Manoj G. Selective Laser Melting of Magnesium and Magnesium Alloy Powders: A Review. Metals, 2016, no. 51, pp. 1–35.
  20. Vorndran E., Moseke C., Gbureck U. 3D printing of ceramic implants. Materials Research Society Bulletin, 2015, no. 40, pp. 127–136.
  21. Meininger S., Moseke C., Spatz K. et al. Effect of strontium substitution on the material properties and osteogenic potential of 3D powder printed magnesium phosphate scaffolds. Materials Science and Engineering, 2019, no. 98, pp. 1145–1158.
  22. Meininger S., Mandal S., Kumar A. et al. Strength reliability and in vitro degradation of three-dimensional powder printed strontium-substituted magnesium phosphate scaffolds. Acta Biomaterialia, 2016, no. 31, pp. 401–411.
  23. Salehi M., Maleksaeedi S., Sapari M.A.B. et al. Additive manufacturing of magnesium–zinc–zirconium (ZK) alloys via capillary-mediated binderless three-dimensional printing. Materials Desing, 2019, no. 169, pp. 115–124.
  24. Mukhina I.Yu., Mukhametov A.A.-Kh., Koshelev A.O. Elimination of surface casting defects on magnesium alloy castings by gas-dynamic spraying. Vse materialy. Entsiklopedicheskiy spravochnik, 2018, no. 4, pp. 34–39.