Investigation of the influence of heat treatment modes on the structure and properties of sheets of aluminum-lithium alloy V-1469

Antipov K.V., Oglodkova Yu.S., Kuryntsev S.V., Safiullin E.I.
Antipov K.V., Oglodkova Yu.S., Kuryntsev S.V., Safiullin E.I. Investigation of the influence of heat treatment modes on the structure and properties of sheets of aluminum-lithium alloy V-1469 // Proceedings of VIAM. 2022. No. 11. DOI: 10.18577/2307-6046-2022-0-11-16-26. URL: https://www.viam-works.ru/en/journal/2022/11/2
Keywords
Al–Li alloys, alloy V-1469, heat treatment, microstructure, microhardness
Abstract

The effect of heat treatment regimes for sheets 2 mm thick of aluminum-lithium alloy V-1469 on the microstructure and microhardness has been studied. Hardening and one- and two-stage artificial aging with various holding times (from 1 to 12 hours) were carried out. Using optical and scanning electron microscopes, the microstructure was studied and a local chemical analysis of the phase components of the alloy was carried out. It is shown that with an increase in the time of one-stage artificial aging, the microhardness increases from 93 to 175 HV, and with an increase in the total exposure during two-stage aging, from 91 to 180 HV, as a result of structural-phase changes and an increase in the proportion of strengthening phases. Inclusions of a regular triangular shape, found after hardening, contain up to 17 % (by mass) of copper and have a size of 1.5–3.0 µm.

Reference list
  1. Klochkova Yu.Yu., Klochkov G.G., Romanenko V.A., Popov V.I. Structure and properties of sheets from high-strength aluminum-lithium alloy V-1469. Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 3–8. DOI: 10.18577/2071-9140-2015-0-4-3-8.
  2. Kablov E.N., Antipov V.V., Oglodkova Yu.S., Oglodkov M.S. Experience and prospects for the use of aluminum-lithium alloys in products of aviation and space technology. Metallurg, 2021, no. 1, pp. 62–70.
  3. Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  4. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  5. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  6. Oglodkov M.S., Shchetinina N.D., Rudchenko A.S., Panteleev M.D. Directions of the development of promising aluminum-lithium alloys for aero-space engineering (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 19–29. DOI: 10.18577/2071-9140-2020-0-1-19-29.
  7. Antipov V.V. Scientific and technological foundations for the development of a new generation of layered aluminum-glass plastics with variable physical and mechanical properties based on low-density aluminum-lithium alloy sheets: thesis abstract, Dr. Sc. (Tech.). Moscow, 2020, 44 p.
  8. Fridlyander I.N., Grushko O.E., Antipov V.V., Kolobnev N.I., Khokhlatova L.B. Aluminum-lithium alloys. 75 years. Aviation materials. Selected works of "VIAM" 1932–2007: anniversary. sci.-tech. coll. Moscow: VIAM, 2007, pp. 163–171.
  9. Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.
  10. Fomin V.M., Malikov A.G., Orishich A.M., Antipov V.V., Klochkov G.G., Skupov A.A. Heat treatment effect on structure of joint weld sheets from V-1469 alloy of Al–Cu–Li system manufactured by laser welding. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 9–18. DOI: 10.18577/2071-9140-2018-0-1-9-18.
  11. Gordeeva M.I. Investigation of the influence of deformation, heat treatment and welding on the phase composition, texture and anisotropy of the mechanical properties of aircraft materials from aluminum-lithium alloys 1441, 1461 and 1469: thesis abstract, Cand. Sc. (Tech.). Moscow, 2017, 24 p.
  12. Kablov E.N., Nochovnaya N.A., Shiryaev A.A., Davydova E.A. Investigation of structural and phase transformations in metastable β-titanium alloys and effect of cooling rate from homogenization temperature on structure and properties of VT47 alloy. Part 2. Trudy VIAM, 2020, no. 8 (90), paper no. 02. Available at: http://www.viam-works.ru (accessed: November 25, 2020). DOI: 10.18577/2307-6046-2020-0-8-20-34.
  13. Knyazev M.I. Development of quantitative methods for studying the phase composition, texture and anisotropy of the properties of aluminum-lithium alloys: thesis, Cand. Sc. (Tech.). Moscow, 2016, 178 p.
  14. Betsofen S.Ya., Antipov V.V., Knyazev M.I. Phase composition, texture and anisotropy of mechanical properties of Al–Cu–Li and Al–Mg–Li alloys (review). Deformatsiya i razrusheniye materialov, 2015, no. 11, pp. 10–26.
  15. Bulina N.V., Malikov A.G., Orishich А.М., Klochkov G.G. Research of the structural-phase composition of laser weld joint depending on the thermal processing of the aluminum alloy V-1469. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 31–39. DOI: 10.18577/2071-9140-2019-0-2-31-39.
  16. Novikov I.I. Theory of heat treatment of metals: textbook for universities. 4th ed., rev. and add. Moscow: Metallurgiya, 1986, 480 p.
  17. Istomin-Kastrovskii V.V., Shamrai V.F., Grushko O.E. et al. Effect of additives of silver, magnesium, zirconium on the aging of the V-1469 alloy of the Al–Cu–Li system. Metally, 2010, no. 5, pp. 73–78.