Powder chromium plating and cromium aluminizing of nickel alloy surface

Kashin D.S., Azarovskiy E.N.
Kashin D.S., Azarovskiy E.N. Powder chromium plating and cromium aluminizing of nickel alloy surface // Proceedings of VIAM. 2022. No. 10. DOI: 10.18577/2307-6046-2022-0-10-90-99. URL: https://www.viam-works.ru/en/journal/2022/10/8
Keywords
nickel alloy, powder chromium aluminizing, diffusion coating, thermal diffusion saturation, scanning electron microscopy
Abstract

Investigations of the surface of a nickel alloy after the penetration of diffusion coatings from powders were carried out. Application of chrome and chromoaluminide screens on atmospheric devices according to the parameters of the temperature-time interval. Determining the values of change in the mass of samples and the degree of diffusion of the surface. Given metallographicl and X-ray microspectral analysis of samples. According to the research results, it was found that after powder chromium plating, the depth of the diffusion zone reaches 18 microns with a chromium concentration of up to 92 %. With the appearance of chromoaluminide surfaces, aluminization mainly takes place, while the diffusion of chromium and iron is not observed.

Reference list
  1. Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  2. Kablov E.N. Developments of VIAM for gas turbine engines and installations. Krylya Rodiny, 2010, no. 4, pp. 31–33.
  3. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 04, 2022). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  4. Bazyleva O.A., Arginbayeva E.G., Lutskaya S.A., Dmitriev N.S. Foundry intermetallic alloy based on Ni3Al compound for turbine blades gas turbine engines. Aviation materials and technologies, 2022, no. 2 (67), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 4, 2022). DOI: 10.18577/2713-0193-2022-0-2-5-17.
  5. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  6. Kolomytsev P.G. Gas corrosion and strength of nickel alloys. Moscow: Metallurgy, 1984, 215 p.
  7. Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  8. Muboyadzhyan S.A., Kablov E.N., Budinovsky S.A. Vacuum-plasma technology for obtaining protective coatings from complex alloyed alloys. Metallovedenie i termicheskaya obrabotka metallov, 1995, no. 2, pp. 15–18.
  9. Budinovsky S.A., Muboyadzhyan S.A. Efficiency of a two-stage ion-plasma technology for obtaining alloyed diffusion aluminide coatings on heat-resistant nickel alloys. Metallovedeniye i termicheskaya obrabotka metallov, 2003, no. 5, pp. 27–32.
  10. Matveev P.V., Budinovskij S.A. Research of the properties of protective heat-resistant coating for intermetallic nickel alloys operating at temperatures up to 1300 °C. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 22–26.
  11. Azarovskiy E.N., Doronin O.N., Muboyadzhyan S.A. Formation of porosity on the border «of heat-resistant alloy–heat-resistant condensation-diffusion coating». Trudy VIAM, 2019, no. 2 (74), paper no. 12. Available at: http://www.viam-works.ru (accessed: July 4, 2022). DOI: 10.18577/2307-6046-2019-0-2-113-120.
  12. Simonov V.N., Abraimov N.V., Shkretov Yu.P., Lukina V.V., Terekhin A.M. Chromium aluminizing of cooled gas turbine blades by the circulation method. Metallovedenie i termicheskaya obrabotka metallov, 2007, no. 7 (625), pp. 36–39.
  13. The method of one-stage diffusion chromium-altering of parts from heat-resistant alloys: pat. EN 2572690C2; filed 05.05.14; publ. 01.20.16.
  14. Method for obtaining a combined heat-resistant coating: pat. 1658652 Rus. Federation; filed 08.04.88; publ. 20.12.00.
  15. Kablov E.N., Muboyadzhyan S.A., Budinovsky S.A., Galoyan A.G. Protective and hardening coatings for gas turbine turbine blades. Proceedings of Intern. sci.-tech. conf. “Scientific ideas of S.T. Kishkin and modern materials science” (Moscow, April 25–26, 2006). Moscow: VIAM, pp. 55–65.
  16. Muboyadzhyan S.A., Galoyan A.G. Thermodiffusion processes of saturation of the surface of heat-resistant alloys with refractory elements and carbon. Tekhnologiya legkikh splavov, 2007, no. 2, pp. 114–120.
  17. Galoyan A.G., Muboyadzhyan S.A., Kashin D.S. Termodiffusion barrier formation under vacuum cementation process on rhenium and rhenium-ruthenium comprising nickel based superalloys. Aviacionnye materialy i tehnologii, 2015, no. 3 (36), pp. 38–43. DOI: 10.18577/2071-9140-2015-0-3-27-37.
  18. Kablov E.N. Materials of the new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.