Development of the production of standard samples of the composition of alloys at the national research center «Kurchatov Institute» – VIAM

Karachevtsev F.N., Eroshkin S.G., Gorbovets M.A.
Karachevtsev F.N., Eroshkin S.G., Gorbovets M.A. Development of the production of standard samples of the composition of alloys at the national research center «Kurchatov Institute» – VIAM // Proceedings of VIAM. 2022. No. 10. DOI: 10.18577/2307-6046-2022-0-10-140-148. URL: https://www.viam-works.ru/en/journal/2022/10/12
Keywords
reference material, aluminum alloy, nickel alloy, titanium alloy, magnesium alloy, spectroscopy, manufacturing technology, type approval, uncertainty
Abstract

The results of the production of standard samples of the composition of alloys on various bases for spectral analysis are given, as well as a list of standard samples developed over the past 10 years. The technologies for manufacturing standard samples homogeneous in chemical composition are shown, which provide the requirements for the material of standard samples. The capabilities of the National Research Center "Kurchatov Institute" - VIAM for the development and production of reference materials are presented, directions for the development of the production of reference materials are indicated.

Reference list
  1. State Standard 8.315–2019. Standard samples of the composition and properties of substances and materials. Basic provisions. Moscow: Standartinform, 2019, 33 p.
  2. Karpov Yu.A., Baranovskaya V.B. Analytical control is an integral part of material diagnostics. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1-I, pp. 5–12.
  3. Karpov Yu.A. Analytical control of metallurgical production. Moscow: Metallurgiya, 1995, pp. 97–107.
  4. Otto M. Modern methods of analytical chemistry: in 2 vols. Moscow: Technosfera, 2003, vol. I, 416 p.
  5. On ensuring the uniformity of measurements: Feder. Law No. 102-FZ of June 26, 2008. Rossiyskaya Gazeta, 2010, no. 112 (5191), May 26.
  6. Karachevtsev F.N., Letov A.F., Protsenko O.M., Yakimova M.S. Development and application of certified reference materials of airborne advanced alloys. Trudy VIAM, 2016, no. 10, paper no. 8. Available at: http://www.viam-works.ru (accessed: December 21, 2021). DOI: 10.18577/2307-6046-2016-0-10-8-8.
  7. Osintseva E.V. Tasks and functions of the Scientific Methodological Center of the State Service of Reference Materials of the Composition and Properties of Substances and Materials. Standartnye obraztsy, 2012, no. 3, pp. 15–40.
  8. Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: July 12, 2022). DOI: 10.18577/2071-9140-2022-0-1-30-40.
  9. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  10. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  11. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
  12. Min P.G., Vadeev V.E., Kramer V.V. The development of the new VZhM200 superalloy and the technology of its production for casting of the advanced engines’ blades by the directional crystallization. Aviation materials and technologies, 2021, no. 3 (64), paper no. 02. Available at: http://www.journal.viam.ru (accessed: July 11, 2022). DOI: 10.18577/2071-9140-2021-0-3-11-18.
  13. Alishin M.I., Knyazev A.E. Production of metal-powder high-purity titanium alloy compositions by induction gas atomization for application in additive manufacturing. Trudy VIAM, 2017, no. 11 (59), paper no. 05. Available at: http://www.viam-works.ru (accessed: December 21, 2021). DOI: 10.18577/2307-6046-2017-0-11-5-5.
  14. Kuznetsov B.Yu., Sorokin O.Yu., Vaganova M.L., Osin I.V. Synthesis of model high-temperature ceramic matrices by the method of spark plasma sintering and the study of their properties for the production of composite materials. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 37–44. DOI: 10.18577/2071-9140-2018-0-4-37-44.
  15. Karachevtsev F.N., Eroshkin S.G., Mosolov A.N. Standard sample for spectral analysis of aluminum alloy VSDP 16 // Etalony. Standartnyye obraztsy, 2022, vol. 18, no. 1, pp. 39–58. DOI: 10.20915/2077-1177-2022-18-1-39-58.
  16. Yakimovich P.V., Alekseev A.V. Determination of impurities in magnesium alloys by inductively coupled plasma mass spectrometry. Izmeritelnaya tekhnika, 2019, no. 8, pp. 68–72.
  17. Alekseev A.V., Yakimovich P.V., Proskurnina E.V. Determination of Si, B, Ca, Mg, Ba, and Zr in complex nickel alloys by ICP-MS. Vestnik Moskovskogo universiteta. Ser. 2: Chemistry, 2020, vol. 61, no. 1, pp. 27–33.
  18. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level RM and MI. Kompetentnost, 2017, no. 2, pp. 40–46.