Heat resistance and technological plasticity of an alloy of the Fe–Cr–Al–Y system for honeycomb seals in the flow path of gas turbine engines
Skugorev A.V., Melnikova D.A., Stolyankov Yu.V., Yaroshenko A.S. Heat resistance and technological plasticity of an alloy of the Fe–Cr–Al–Y system for honeycomb seals in the flow path of gas turbine engines // Proceedings of VIAM. 2022. No. 10. DOI: 10.18577/2307-6046-2022-0-10-3-12. URL: https://www.viam-works.ru/en/journal/2022/10/1
Keywords
heat-resistant alloy, fechral, yttrium alloying, honeycomb seals
Abstract
The work is devoted to the study of heat resistance and technological plasticity of a new heat-resistant alloy of the Fe–Cr–Al–Y system. The alloy of the Fe–Cr–Al–Y system being developed is intended for the manufacture of honeycomb seals for the flow path of gas turbine engines with an operating temperature of up to 1100 °С. This alloy is intended to replace heat-resistant alloys ЭИ435 and ЭИ868, which are currently used for the manufacture of honeycomb seals. In terms of heat resistance at 1100 °С, the alloy of the Fe–Cr–Al–Y system is 1.5–2 times superior to alloys analogs ЭИ435 and ЭИ868.
Reference list
- Farafonov D.P., Leshchev N.E., Afanasiev-Khodykin A.N., Artemenko N.I. Abrasive wear-resistant seal materials of the gas turbine engine flow section. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 67–74. DOI: 10.18577/2071-9140-2019-0-3-67-74.
- Salakhova R.K., Tikhoobrazov A.B., Farafonov D.P., Smirnova T.B. Features of electrolytic deposition of abrasive-wear-resistant nickel-based coatings. Trudy VIAM, 2022, no. 2 (108), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 16, 2022). DOI: 10.18577/2307-6046-2022-0-2-99-110.
- Farafonov D.P., Migunov V.P., Sarayev A.A., Leshchev N.E. Abradability and erosion resistance of seals in turbine engine air-gas channel. Trudy VIAM, 2018, no. 8 (68), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 16, 2022). DOI: 10.18577/2307-6046-2018-0-8-70-80.
- Bakradze M.M., Peskova A.V., Kaplansky Yu.Yu. Influence of thermal post-treatment on the texture and anisotropy of mechanical properties in the Cu–Cr construction alloy manufactured by laser powder bed fusion. Aviation materials and technologies, 2022, no. 1 (66), paper no. 01. Available at: http://www.journal.viam.ru (accessed: August 16, 2022). DOI: 10.18577/2071-9140-2022-0-1-3-16.
- Kablov E.N. The role of fundamental research in the creation of new generation materials. Abstracts of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, pp. 24.
- Ospennikova O.G. Implementation results of the strategic directions on creation of new generation of heat-resisting cast and wrought alloys and steels for 2012–2016. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 17–23. DOI: 10.18577/2071-9140-2017-0-S-17-23.
- Ivanov V.V., Tagiltsev S.V. Comparative analysis of manufacturing technologies for honeycomb seals. Gasoturbinnye tekhnologii, 2019, no. 6, pp. 26–29.
- Farafonov D.P., Degovets M.L., Aleshina R.Sh. The metal fibers of heat-resistant alloys alloyed by platinum group metals. Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 44–52. DOI: 10.18577/2071-9140-2016-0-1-44-52.
- Abraimov N.V. High-temperature materials and coatings for gas turbines. Moscow: Mashinostroenie, 1993, 336 p.
- Nychka J.A., Clarke D.R. Quantification of Aluminum Outward Diffusion During Oxidation of FeCrAl Alloys. Oxidation of Metals, 2005, vol. 63, no. 5/6, pp. 324–352.
- Clemendot F., Gras J.M., Van Duysen J.C. Influence of yttrium on high temperature behavior of Fe–Cr–Al–Y alloys. Journal de Physique IV France, 1993, no. 3, pp. 291–299.
- Mennicke C., Schumann E., Ruhle M. et al. The Effect of Yttrium on the Growth Process and Microstructure of α-Al2O3 on FeCrAl. Oxidation of Metals, 1998, vol. 49, no. 5/6, pp. 455–466.
- Amano T. High-temperature oxidation of FeCrAl (Y, Pt) alloys in oxygen-water vapour. Materials at high temperatures, 2011, vol. 28, is. 4, p. 342–348.
- Simms N.J., Norton J.F., McColvin G. Performance of candidate gas turbine abradeable seal materials in high temperature combustion Atmospheres. Materials and Corrosion, 2005, no. 11, pp. 765–777.
- Smarsly W., Zheng N., Buchheim C.S. et al. Advanced High Temperature Turbine Seals Materials and Designs. Material Science Forum, 2005, vol. 492–493, pp. 21–26.
- Zhukov L.L., Plemyannikova I.M., Mironova M.N. et al. Alloys for heaters. Moscow: Metallurgiya, 1985, 146 p.
- Ponomarenko D.A., Letnikov M.N., Skugorev A.V., Sidorov S.A. The use of specialized isothermal presses for forging blanks of turbine disks from hard-to-deform heat-resistant alloys. Kuznechno-shtampovochnoe proizvodstvo. Obrabotka materialov davleniyem, 2018, no. 3, pp. 19–25.
- Kapitanenko D.V., Nekrasov B.R., Izakov I.A., Chebotareva E.S. Deforming equipment for isothermal stamping (part 1). Kuznechno-shtampovochnoe proizvodstvo. Obrabotka materialov davleniyem, 2021, no. 10, pp. 12–20.
- Akhmedzyanov M.V., Skugorev A.V., Ovsepyan S.V., Mazalov I.S. Development of a resource-saving technology for producing cold-rolled sheet from a high-temperature weldable alloy VZh171. Proizvodstvo prokata, 2015, no. 1, pp. 14–17.