Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. Features of technology and polymer composite materials for the manufacture of wings of advanced aircraft (review) // Proceedings of VIAM. 2022. No. 1. DOI: 10.18577/2307-6046-2022-0-1-66-75. URL: https://www.viam-works.ru/en/journal/2022/1/7
Keywords
polymer composite materials, vacuum infusion, automated laying out, prepregs, autoclave molding, cycle time
Abstract

Today, the wings of Boeing 787, Airbus A350 aircraft are made by automated laying out of prepregs with subsequent autoclave molding. Boeing and Airbus plan to replace the 737 and A320 aircraft in the coming years, and new materials and technologies need to be developed to ensure the production of these aircraft in the amount of 100 pieces per month. To introduce new processes and materials, research is being carried out on the selection of a binder, reinforcing fillers, development of the vacuum impregnation process, curing and automation in order to increase reliability, speed up the process and reduce cycle time.

Reference list
  1. Corner of the sky. Su-47 "Berkut". Available at: http://www.airwar.ru/enc/fighter/s37.html (accessed: September 10, 2021).
  2. Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Kablov E.N. Formation of domestic space materials science. Vestnik RFBR, 2017, no. 3, pp. 97–105.
  4. Kablov E.N. VIAM: New generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8. pp. 54–58.
  5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Kara-vaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021. no. 1 (62). paper no. 03. Available at: https://journal.viam.ru (accessed: February 19, 2021). DOI: 10.18577/2713-0193-2021-0-1-22-23.
  7. Doneckij K.I., Karavaev R.Yu., Raskutin A.E., Panina N.N. Properties of carbon fiber and fiberglass on the basis of braiding preforms. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 54–59. DOI: 10.18577/2071-9140-2016-0-4-54-59.
  8. Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577/2071-9140-2019-0-4-18-26.
  9. Timoshkov P.N. Equipment and materials for the technology of automated calculations prepregs. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  10. Veshkin E.A., Postnov V.I., Postnova M.V., Barannikov A.A. Experience in the use of vacuum infusion technologies in the production of PCM structures. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2018, vol. 20, no. 4 (3). pp. 344–350.
  11. How superlight parts for aircraft and missiles are made in Russia. Available at: https://ria.ru/20190522/1553632826.html (accessed: September 8, 2021).
  12. A wing made of Russian composite materials was installed on the MS-21-300 aircraft. Composite World, 2021, no. 3, pp. 7.
  13. "Wing of Tomorrow": FACC and Airbus develop wings of the future. Available at: https://newsroom.aviator.aero/wing-of-tomorrow-facc-and-airbus-develop-wings-of-the-future (acces-sed: September 10, 2021).
  14. GKN Aerospace Manufactures First Parts for Wing of Tomorrow Program. Available at: https://www.compositesworld.com/news/gkn-aerospace-manufactures-first-demonstrator-parts-for-wing-of-tomorrow-program (accessed: September 10, 2021).
  15. Update: Lower wing skin, Wing of Tomorrow. Available at: https://www.compositesworld.com/ articles/update-lower-wing-skin-wing-of-tomorrow (accessed: September 13, 2021).
  16. Large, high-volume, infused composite structures on the aerospace horizon. Available at: https://www.compositesworld.com/articles/large-high-volume-infused-composite-structures-on-the-aerospace-horizon (accessed: September 7, 2021).
  17. Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: September 13, 2021). DOI: 10.18577/2713-0193-2021-0-3-105-106.
  18. Timoshkov P.N., Goncharov V.A., Grigoreva L.N., Usacheva M.N., Hrulkov A.V. Robotic laying out of prepregs as an alternative to technology to ATL and AFP (review). Trudy VIAM, 2021, no. 3 (97), paper no. 08. Available at: http://www.viam-works.ru (accessed: September 13, 2021). DOI: 10.18577/2307-6046-2021-0-3-87-98.