Application of optical deformation sensors for estimating the deformability of CFRP samples near the stress concentrators
Shershak P.V., Yakovlev N.O., Oreshko E.I. Application of optical deformation sensors for estimating the deformability of CFRP samples near the stress concentrators // Proceedings of VIAM. 2022. No. 1. DOI: 10.18577/2307-6046-2022-0-1-111-122. URL: https://www.viam-works.ru/en/journal/2022/1/11
Keywords
CFRP, optical strain gauge, non-contact strain gauge, video extensometer, strain, gauge base, mark
Abstract
The results of the calculations and the obtained experimental data show the need to take into account the distribution of strain fields on samples with stress concentrators for the selection of the correct gage of optical strain gauges. The ability to install certain gage of optical sensors with specific geometric parameters of the sample allows one to obtain the values of the stiffness and deformation characteristics on the sample with holes close to the values of the material characteristics, which can be used, for example, when carrying out research work in conditions of limited materials.
Reference list
- Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
- Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Podzhivotov N.Yu., Lutsenko A.N. On the need to create a unified information and analytical center for aviation materials of the Russian Federation. Problemy mashinostroyeniya i avtomatizatsii, 2019, no. 3, pp. 28–34.
- Afanasyev A.V., Rabinsky L.N., Shershak P.V. Experimental determination of deformation and strength characteristics of polymer composite materials. Mekhanika kompozitsionnykh materialov i konstruktsiy, 2010, vol. 16, no. 2, pp. 214–222.
- Erasov V.S. Modern methods for assessing the physical and mechanical properties of materials. Collection of reports of the All-Russian conference on testing and research of properties of materials "TestMat-2012". Moscow: VIAM, 2012, p. 13.
- Lutsenko A.N., Odintsev I.N., Grinevich A.V. i dr. Study of material deformation by optical-correlation methods. Aviacionnye materialy i tehnologii, 2014, no. S4, pp. 70–86. DOI: 10.18577/2071-9140-2014-0-s4-70-86.
- Nikitin A.V., Krylov V.D., Khanzhin V.G. Equipment and technique for real-time observation of deformation instability during stretching of thin aluminum foil. Vestnik Tambovskogo universiteta, 2013, vol. 18, no. 4-2, pp. 1871–1872.
- Panin S.V., Burkov M.V., Lyubutin P.S., Altukhov Yu.A., Eremin A.V., Khizhnyak S.A. Application of an integral-type strain gauge in cyclic testing of a composite material based on carbon fibers. Izvestiya vysshikh uchebnykh zavedeniy. Fizika, 2013, vol. 56, no. 12-2. S. 186-191.
- Oreshko E.I., Erasov V.S., Grinevich D.V., Sershak P.V. Review of criteria of durability of materials. Trudy VIAM, 2019, no. 9 (81), paper no. 12. Available at: http://www.viam-works.ru (accessed: May 11, 2021). DOI: 10.18577/2307-6046-2019-0-9-108-126.
- Grinevich D.V., Yakovlev N.O., Slavin A.V. The criteria of the failure of polymer matrix composites (review). Trudy VIAM, 2019, no. 7 (79), paper no. 11. Available at: http://viam-works.ru (accessed: May 11, 2021). DOI: 10.18577/2307-6046-2019-0-7-92-111.
- Kosarev V.A., Azikov N.S., Alipov A.E. Technique for solving physically nonlinear problems of structural strength with stress concentrators. Aviatsionnaya promyshlennost, 2014, no. 2, pp. 26–31.
- Tretyakova T.V., Spaskova E.M. Experimental study of the limiting stress-strain states of a quasi-brittle material using the digital image correlation method. Vestnik Permskogo natsionalnogo issledovatelskogo politekhnicheskogo universiteta, ser.: Mekhanika, 2013, no. 2, pp. 186–198.
- Ilichev A.V., Raskutin A.E. Research of stress concentrator influence on stress-strain state of carbon by digital images correlation method. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 62–66. DOI: 10.18577/2071-9140-2014-0-3-61-62.
- Ilichev A.V., Gubin A.M., Akmeev A.R., Ivanov N.V. Definition of area of the maxi-mum shear deformations for CFRP samples on Iosipescu method, with use of optical system of measurements. Trudy VIAM, 2018, no. 6 (66), paper no. 10. Available at: http://www.viam-works.ru (accessed: May 11, 2021). DOI: 10.18577/2307-6046-2018-0-6-99-109.