Low-cycle fatigue at elevated temperatures of heat-resistant nickel-based alloy manufactured by selective laser melting

Khodinev I.A., Gorbovets M.A., Monin S.A., Ryzhkov P.V.
Khodinev I.A., Gorbovets M.A., Monin S.A., Ryzhkov P.V. Low-cycle fatigue at elevated temperatures of heat-resistant nickel-based alloy manufactured by selective laser melting // Proceedings of VIAM. 2022. No. 1. DOI: 10.18577/2307-6046-2022-0-1-97-110. URL: https://www.viam-works.ru/en/journal/2022/1/10
Keywords
low-cycle fatigue (LCF), high-temperature alloy, wrought alloy, nickel alloy, Basquin–Manson–Coffin equation, prediction of fatigue resistance characteristics, asymmetry coefficient
Abstract

Low-cycle fatigue has been investigated under a «hard» loading cycle and under a «soft» loading cycle of a heat-resistant deformable VZh175 alloy at room and two operating temperatures at three asymmetry coefficients. The tests were carried out at a sinusoidal loading cycle with a frequency of 1 Hz. Comparison of stresses at «soft» and «hard» loading cycles is carried out. A comparison of the fatigue curve and a priori curves obtained using the characteristics of short-term strength is carried out.

Reference list
  1. Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Single-crystal nickel-based superalloy of a new generation with low-density. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
  2. Kablov E.N., Ospennikova O.G., Petrushin N.V. New single crystal heat-resistant intermetallic γʹ-based alloy for GTE blades. Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 34–40. DOI: 10.18577/2071-9140-2015-0-1-34-40.
  3. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  4. Ospennikova O.G. Tendencies of development of heat-resistant nickel alloys of low density with polycrystalline and single-crystal structures (review). Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 3–19. DOI: 10.18577/2071-9140-2016-0-1-3-19.
  5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Priority directions of development of technologies for the production of heat-resistant materials for aircraft engine building. Problemy chernoy metallurgii i materialovedeniya, 2013, no. 3, pp. 47–54.
  7. Golubovsky E.R., Svetlov I.L., Petrushin N.V., Cherkasova S.A., Volkov M.E. Low-cycle fatigue of single crystals of heat-resistant nickel alloys at elevated temperatures. Deformatsiya i razrushenie materialov, 2009, no. 8, pp. 41–48.
  8. Gorbovets M.A., Bazyleva O.A., Belyaev M.S., Khodinev I.A. Low-cycle fatigue of a single-crystal intermetallic alloy of the VKNA type under conditions of "hard" loading. Metallurg, 2014, no. 8, pp. 111–114.
  9. Hodinev I.A., Monin S.A. Anisotropy of low cycle fatigue characteristics of single-crystal heat-resistant nickel alloys. Trudy VIAM, 2020, no. 10 (92), paper no. 11. Available at: http://www.viam-works.ru (accessed: May 1, 2021). DOI: 10.18577/2307-6046-2020-0-10-97-105.
  10. Zhong Z., Gu Y., Yuan Y. et al. On the low cycle fatigue behaviour of a Ni-based superalloy containing high Co and Ti contents. Materials Science and Engineering, 2012, vol. A552, pp. 434–443.
  11. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. High-temperature heat resisting nickel alloys for details of gas turbine engines. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 52–57.
  12. Belyayev M.S., Gorbovets M.A., Bakradze M.M. Change of parameters of elasto-plastic deformation for LCF testing Ni-base superalloy VZh175. Trudy VIAM, 2015, no. 12, paper no. 04. Available at: http://www.viam-works.ru (accessed: May 1, 2021). DOI: 10.18577/2307-6046-2015-0-12-4-4.
  13. Lomberg B.S., Shestakova A.A., Letnikov M.N., Bakradze M.M. The influence of temperature and stresses on nature of nanosize γʹ-phase in Ni-base superalloy VZh175-ID. Trudy VIAM, 2019, no. 12 (84), paper no. 01. Available at: http://www.viam-works.ru (accessed: May 1, 2021). DOI: 10.18577/2307-6046-2019-0-12-3-10.
  14. State Standart 25.502–79. Calculations and tests for strength in mechanical engineering. Methods for mechanical testing of metals. Fatigue test methods. Moscow: Publishing house of Standards, 1986, 34 p.
  15. ASTM E606/ E606M-19. Standard Test Method for Strain-Controlled Fatigue Testing. American Society for Testing and Materials, 2018, 16 p.
  16. Gorbovets M.A., Khodinev I.A., Ryzhkov P.V. Equipment for testing carrying out the strain-controlled low-cycle fatigue. Trudy VIAM, 2018, no. 9 (69), paper no. 06. Available at: http://www.viam-works.ru (accessed: July 01, 2021). DOI: 10.18577/2307-6046-2018-0-9-51-60.
  17. Recommended circular RC-AP-33.15-1. Guidelines for determining the design values of the characteristics of the structural strength of metallic materials. Moscow: Aviaizdat, 2013. S. 32–33.
  18. Troshchenko V.T., Khamaza L.A. Deformation curves of fatigue of steels and methods for determining their parameters. Communication 1. Traditional methods. Problemy prochnosti, 2010, no. 6, pp. 26–43.
  19. Erasov V.S., Oreshko E.I. Tests for fatigue of metal materials (review). Part 2. Analysis of the Basquin–Manson–Coffin equation. Methods of testing and processing of results. Aviation materials and technology, 2021. no. 1 (62). paper no. 08. Available at: http://www.journal.viam.ru (accessed: May 15, 2021). DOI: 10.18577/2071-9140-2021-0-1-80-94.
  20. Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DO1: 10.18577/2071-9140-2020-0-4-59-70.
  21. Radhakrishnan V.M. On bilinearity of the Coffin–Manson low-cycle fatigue relationship. International Journal of Fatigue, 1992, vol. 14, no. 5, pp. 305–311.
  22. Norman E. Dowling. Mean Stress Effects in Stress-Life and Strain-Life Fatigue. Fatigue & Fracture of Engineering, 2009, no. 32 (3), pp. 163–179.
  23. Manson S.S. Fatigue: a Complex Subject – Some Simple Approximations. Experimental Mechanics – Journal of the Society for Experimental Stress Analysis, 1965, no. 5 (7), pp. 193–226.
  24. Muralidharan U., Manson S.S. Modified Universal Slopes Equation for Estimation of Fatigue сharacteristics. Journal of Engineering Materials and Technology – Transactions of the American Society of Mechanical Engineers, 1988, no. 110, pp. 55‒58.