Features of destruction of nitrided samples of 38H2MYuA and 30H3MA steels

Slavin A.V., Lyakhov A.A., Vishtalyuk A.A., Kuzmina O.V., Gulina I.V., Yakovlev N.O., Grinevich A.V.
Slavin A.V., Lyakhov A.A., Vishtalyuk A.A., Kuzmina O.V., Gulina I.V., Yakovlev N.O., Grinevich A.V. Features of destruction of nitrided samples of 38H2MYuA and 30H3MA steels // Proceedings of VIAM. 2021. No. 9. DOI: 10.18577/2307-6046-2021-0-9-76-84. URL: https://www.viam-works.ru/en/journal/2021/9/8
Keywords
chemical-thermal treatment, nitriding, brittle layer, load-bearing capacity, destruction of heterogeneous material, complex stress state.
Abstract

The article deals with the features of deformation and destruction of samples that have undergone chemical-thermal treatment, using the example of testing nitrided samples of steels 38H2MYuA and 30H3MA. It is established that the mechanical properties determined during the tensile testing of samples with a highly rigid brittle layer cannot serve as design characteristics when evaluating the bearing capacity of parts that have undergone chemical-thermal treatment. Testing of nitrided samples of 38H2MYuA and 30H3MA steels demonstrated a complex process of their deformation and destruction, and the test result showed that this steel treated to the «hardened + high tempering» mode sensitivity to the most dangerous concentration the crack is absent.

Reference list
  1. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577 / 2071-9140-2020-0-1-3-11.
  2. Kostetskiy B.I. Friction, lubrication and wear in machines. Kiev: Technika, 1970, 396 p.
  3. Berliner E.M., Brown E.D., Chichinadze A.V. Friction, wear and lubrication (tribology and tribotechnics). Moscow: Mashinostroenie, 2003, 576 p.
  4. Iakovlev N.O., Selivanov A.A., Gulina I.V., Grinevich A.V. Revisiting the durability of hinged-bolt connections. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 79–85. DOI: 10.18577/2071-9140-2020-0-4-79-85.
  5. Romanenko D.N., Sevalnev G.S., Leonov A.A., Udod K.A., Stepanenko E.V. Improving the tribo-logical characteristics of 18KHGT steel after ce-mentation and hardening heat treatment. Aviation materials and technology, 2021. no. 1 (62). paper no. 02. Available at: https://journal.viam.ru (accessed: May 31, 2021). DOI: 10.18577/2713-0193-2021-0-1-13-21.
  6. Lakhtin Yu.M., Arzamasov B.N. Chemical heat treatment of metals. Moscow: Metallurgiya, 1985, 256 p.
  7. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  8. Kablov E.N., Podzhivotov N.Yu., Lutsenko A.N. On the need to create a unified information and analytical center for aviation materials of the Russian Federation. Problemy mashinostroyeniya i avtomatizatsii, 2019, no. 3, pp. 28–34.
  9. Carrying capacity and strength calculation of machine parts: handbook. Ed. S.V. Serensen. Ed. 3rd, rev. and add. Moscow: Mashinostroenie, 1975, 488 p.
  10. Lakhtin Yu.M., Kogan Ya.D. Steel nitriding. Moscow: Mashinostroenie, 1976, 256 p.
  11. Fetisov G.P. Materials science and technology of metals. Moscow: Vysshaya shkola, 2001, 640 p.
  12. Brand of steels and alloys. Ed. Yu.G. Dragunov, A.S. Zubchenko. 4th ed., rev. and add. Mosocow: Mashinostroenie, 2015, 1216 p.
  13. Mitrakov O.V., Yakovlev N.O., Yakusheva N.A., Grinevich A.V. Destruction features of steel 20ХГСН2МФА-ВД during the fracture toughness test. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 49–56. DOI: 10.18577/2071-9140-2019-0-1-49-56.
  14. Popov L.E., Koneva N.A., Tereshko I.V. Strain hardening of ordered alloys. Moscow: Metallurgiya, 1976, 256 p.
  15. Pisarenko G.S., Lebedev A.A. Deformation and strength of materials under complex stress conditions. Kiev: Naukova Dumka, 1976, 416 p.
  16. Grinevich A.V., Laptev A.B., Skripachev S.Yu., Nuzhnyj G.A. Matrix strength characteristics for the assessment of limit states of structural metallic materials. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 67–74. DOI: 10.18577/2071-9140-2018-0-2-67-74.