Destructive methods for determining residual stresses (review)
Monakhov A.D., Yakovlev N.O., Avtaev V.V., Kotova E.A. Destructive methods for determining residual stresses (review) // Proceedings of VIAM. 2021. No. 9. DOI: 10.18577/2307-6046-2021-0-9-95-104. URL: https://www.viam-works.ru/en/journal/2021/9/10
Keywords
residual stresses, tensometry, deformation, speckle interferometry, digital image correlation.
Abstract
The paper presents an overview of methods for determining residual stresses. Methods such as splitting and segmentation, layer-by-layer removal, slitting (cutting, pliability), profiling, drilling holes (including a «deep» hole) are considered. The description of the methods for mea-suring the deformation used in the determination of residual stresses is given. The most common contact method using strain gauges, as well as non-contact methods: polarization-optical (photo-elasticity), optical speckle interferometry, digital image correlation.
Reference list
- Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577 / 2071-9140-2020-0-1-3-11.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing – the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
- Ospennikova O.G., Naprienko S.A., Medvedev P.N., Krupnina O.A., Rogalev A.M. Features of the structure of Ti–6Al–4V alloy obtained by selective laser melting. Trudy VIAM, 2019, no. 10 (82), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 18, 2021). DOI: 10.18577/2307-6046-2019-0-10-14-24.
- Burkin S.P., Shimov G.V. Residual stresses in metal products. Ekaterinburg: Ural Federal University, 2015, 247 p.
- Birger I.A. Residual stresses. Moscow: Mashgiz, 1963, 233 p.
- Nochovnaya N.A., Panin P.V. Residual Macrostress Analysis in Welded Junctions of Different Titanium Alloys. Trudy VIAM, 2014, no. 05, paper no. 02. Available at: http://www.viam-works.ru. (accessed: June 20, 2021). DOI: 10.18577/2307-6046-2014-0-5-2-2.
- Lukin V.I., Ioda E.N. Improving the reliability of welded joints made of high-strength aluminum-lithium alloy V-1461. Svarochnoye proizvodstvo, 2010, no. 11, pp. 14–17.
- Arislanov A.А., Putyrskiy S.B., Yakovlev A.L., Gribkov M.S. Analysis of microstructure and mechanical properties of welded joint from VT6ch. alloy. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 74–79. DOI: 10.18577/2071-9140-2019-0-4-74-79.
- Zhongxu X., Changpeng C. Study of residual stress in selective laser melting of Ti6Al4V. Materials & Design, 2020, no. 193, art. 108846. DOI: 10.1016/j.matdes.2020.108846.
- Grinevich A.V., Laptev A.B., Skripachev S.Yu., Nuzhnyj G.A. Matrix strength characteristics for the assessment of limit states of structural metallic materials. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 67–74. DOI: 10.18577/2071-9140-2018-0-2-67-74.
- Rossini N.S., Dassisti M., Benyounis K.Y., Olabi A.G. Methods of measuring residual stresses in components (Review). Materials and Design, 2012, no. 35, pp. 572–588. DOI: 10.1016/j.matdes.2011.08.022.
- Schajer G.S. Residual Stresses: Measurement by Destructive Methods. Encyclopedia of Materials: Science and Technology. Oxford: Elsevier Science, 2001. Section 5a, pp. 8152–8158. DOI: 10.1016/B0-08-043152-6/01462-5.
- Walton H.W. Deflection Methods to Estimate Residual Stress. Handbook of Residual Stress and Deformation of Steel. ASM International, 2002, pp. 89–98.
- ASTM E1928. Standard Practice for Estimating the Approximate Residual Circumferential Stress in Straight Thin-walled Tubing, 2019. Available at: https://www.astm.org/Standards/E1928.htm (accessed: June 20, 2021).
- Cheng W., Finnie I. Residual Stress Measurement and the Slitting Method. New York: Springer, 2007. 164 p.
- Hill M.R. The Slitting Method. Practical Residual Stress Measurement Methods. Vancouver: University of British Columbia, 2013, pp. 89–108. DOI: 10.1002/9781118402832.ch4.
- Prime M.B. Cross-sectional Mapping of Residual Stresses by Measuring the Surface Contour After a Cut. Journal of Engineering Materials and Technology, 2001, no. 123 (2), pp. 162–168.
- Pagliaro P., Prime M.B., Swenson H., Zuccarello B. Measuring Multiple Residual-Stress Components Using the Contour Method and Multiple Cuts. Experimental Mechanics, 2010, no. 50 (2), pp. 187–194. DOI: 10.1007/s11340-009-9280-3.
- ASTM E837. Standard Test Method for Determining Residual Stresses by the Hole-Drilling Strain-Gage Method, 2020. Available at: https://www.astm.org/Standards/E837.htm (accessed: June 20, 2021).
- Schajer G.S., Yang L. Residual-stress Measurement in Orthotropic Materials Using the Hole-drilling Method. Experimental Mechanics, 1994, no. 34, pp. 324–333.
- Ghasemi A.R., Shokrieh M.M. Measuring residual stresses in composite materials using the simulated hole-drilling method. Residual Stresses in Composite Materials. Woodhead Publishing, 2014, pp. 76–120. DOI: 10.1533/9780857098597.1.76.
- Mathar J. Determination of Initial Stresses by Measuring the Deformation Around Drilled Holes. Transactions ASME, 1934, no. 56 (4), pp. 249–254.
- Schajer G.S., Philip S.W. Hole-Drilling Method for Measuring Residual Stresses. Synthesis SEM Lectures on Experimental Mechanics, 2018, no. 1, pp. 1–186. DOI: 10.2200/S00818ED1V01Y201712SEM001.
- Leggatt R.H., Smith D.J., Smith S.D., Faure F. Development and Experimental Validation of the Deep Hole Method for Residual Stress Measurement. Journal of Strain Analysis, 1996, no. 31 (3), pp. 177–186. DOI: 10.1243/03093247V313177.
- Aleksandrov A.Ya., Akhmetzyanov M.X. Polarization-optical methods of solid mechanics. Moscow: Nauka, 1973, 572 p.
- Razumovsky I.A. Method of photoelastic coatings in studies in areas of high stress gradients. Mashinovedenie, 1984, no. 2, pp. 84–87.
- Thomas W.C., Wayne E.N. Residual strain Measurement using Photoelastic Coating. Optics and Lasers in Engineering, 1997, vol. 27, is. 1, pp. 111–123. DOI: 10.1016/S0143-8166(95)00012-7.
- Rickert T. Residual Stress Measurement by ESPI Hole-Drilling. Procedia CIRP, 2016, vol. 45, pp. 203–206. DOI: 10.1016/j.procir.2016.02.256.
- Razumovsky I.A. Interference-optical methods of solid mechanics. Moscow: Publ. house of MSTU, 2007, 240 p.
- Apalkov A.A., Odintsev I.N., Razumovsky I.A. Application of electronic speckle interferometry for measuring residual stresses. Zavodskaya laboratoriya. Diagnostika materialov, 2002, vol. 68, no. 4, pp. 48–51.
- Nelson D.V., McCrickerd J.T. Residual-stress Determination Through Combined Use of Holographic Interferometry and Blind-Hole Drilling. Experimental Mechanics, 1986, no. 26 (4), pp. 371–378.
- Sutton M.A., Orteu J., Schreier H.W. Image correlation for shape, motion and deformation measurements: basic concepts, theory and applications. Springer, 2009, 321 p.
- Nelson D.V., Makino A., Schmidt T. Residual Stress Determination Using Hole Drilling and 3D Image Correlation. Experimental Mechanics, 2006, no. 46 (1)p pp. 31–38. DOI: 10.1007/s11340-006-5859-0.
- Gao J., Shang H. Deformation-Pattern-Based Digital Image Correlation Method and its Application to Residual Stress Measurement. Applied Optics, 2009, vol. 48, pp. 1371–1381. DOI: 10.1364/AO.48.001371.