Technological aspects of obtaining frit of heat-resistant enamel for the protection of corrosion-resistant steels

Zakalashnyy A.V., Denisova V.S., Vlasova O.V., Solntsev St.S.
Zakalashnyy A.V., Denisova V.S., Vlasova O.V., Solntsev St.S. Technological aspects of obtaining frit of heat-resistant enamel for the protection of corrosion-resistant steels // Proceedings of VIAM. 2021. No. 8. DOI: 10.18577/2307-6046-2021-0-8-43-49. URL: https://www.viam-works.ru/en/journal/2021/8/5
Keywords
heat-resistant enamel coating, corrosion-resistant steels, heat-resistant alloys, glass, frit, production technology.
Abstract

The technological aspects of producing frit based are studied for heat-resistant enamel EV-300-60M in experimental industrial conditions. It was found that in the temperature range of 1200–1250 °C, intensive foaming of the charge occurs due to the active release of oxygen by manganese oxide. Due to the combination of technological operations, it is possible to ensure a sufficient reduction, but not complete exclusion of foaming when cooking frit. In this regard, the further direction of work on improving heat-resistant enamels for the protection of corrosion-resistant steels determines the need to develop a technological composition of frit.

Reference list
  1. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  2. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577 / 2071-9140-2020-0-1-3-11.
  3. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  4. Solncev S.S., Denisova V.S., Rozenenkova V.A. Reaction cure – the new direction in technology ofhigh-temperature composite coatings and materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 329–343. DOI: 10.18577/2071-9140-2017-0-S-329-343.
  5. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovations. Wings of the Motherland, 2016, no. 5, pp. 8–18.
  6. Denisova V.S., Soloveva G.A. Heat-resistant glass-ceramic coating for protection of gas turbines’ combustion chambers parts. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 18–22. DOI: 10.18577/2071-9140-2016-0-4-18-22.
  7. Vargin V.V. Enamel and metal enamel technology. Moscow: Stroyizdat, 1965, 316 p.
  8. Kablov E.N. Aviation materials: reference book in 12 vols. 7th ed. Moscow: VIAM, 2011, 176 p.
  9. Gromov V.I., Voznesenskaya N.M., Pokrovskaya N.G., Tonysheva O.A. High-strength constructional and corrosion-resistant steels developed by VIAM for aviation engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 159–174. DOI: 10.18577/2071-9140-2017-0-S-159-174.
  10. Petzold A., Peshman G. Enamel and enameling. Trans. from German. Moscow: Metallurgiya, 1990, 576 p.
  11. Niu X., Zhang H., Hu X., Han W. Synthesis of well-adhered SiO2–Al2O3 glass-ceramic coating on NiCrFe alloy supports. Applied Surface Science, 2013, vol. 268, p. 265–269.
  12. Bachar A., Mabrouk A., De Sousa Meneses D. et al. Study of the firing type on the microstructure and color aspect of ceramic enamels. Journal of Alloys and Compounds, 2018, vol. 735, pp. 2479–2485. DOI: 10.1016/j.jallcom.2017.11.364.
  13. Guldal O., Apak C. A study on Cr3+/Cr6+ equilibria in industrial emerald green glasses. Journal of Non-Crystallibe Solids, 1986, vol. 38–39, pp. 251–256.
  14. Shultz M.M., Mazurin O.V. Modern ideas about the structure of glasses and their properties. Leningrad: Nauka, 1988, 198 p.
  15. Chen M., Li W., Shen M. et al. Glass coatings on stainless steels for high-temperature oxidation protection: Mechanisms. Corrosion Science, 2014, vol. 82, pp. 316–327.