Technological ways to create composite materials based on heat-resistant refractory compounds (review)

Shestakov A.V., Karashaev M.M., Dmitriev N.S.
Shestakov A.V., Karashaev M.M., Dmitriev N.S. Technological ways to create composite materials based on heat-resistant refractory compounds (review) // Proceedings of VIAM. 2021. No. 8. DOI: 10.18577/2307-6046-2021-0-8-12-20. URL: https://www.viam-works.ru/en/journal/2021/8/2
Keywords
intermetallide, Ni–Al system, metallurgy granules, spark plasma sintering, hot isostatic pressing, thermomechanical processing, mechanical activation.
Abstract

The article discusses the main technological approaches to obtain heat-resistant and heat-resistant materials based on compounds in the Ni–Al system in order to use them in promising products of aviation and rocket technology. It is shown that when receiving materials based on compounds in the Ni-Al system, a phase of eutectic origin is formed based on the Ni3Al compound, which reduces the technological plasticity of the alloys of this system. The use of powder metallurgy methods eliminates such phases in the structure of alloys obtained using granule metallurgy technology, as well as with the use of special methods of powder metallurgy.

Technological approaches are presented to obtain similar materials using powder metallurgy methods combined with thermomechanical processing.

Reference list
  1. Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  4. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  5. Bazyleva O.A., Turenko E.Yu., Rassokhina L.I., Bityutskaya O.N., Shitikov A.V., Lapeev B.S. Cast blocks of the nozzle apparatus of the 2nd stage of the HPT from the VKNA-4-VI intermetallic alloy. Liteinoe proizvodstvo, 2014, no. 10, pp. 7–10.
  6. Bazyleva O.A., Unchikova M.V., Turenko E.Yu., Bagetov V.V., Shestakov A.VStudy of heat treatment effect on structure, dendritic liquation parameters and time to failure of Ni3Al-based alloy containing Re). Trudy VIAM, 2016, no. 10, paper no. 4. Available at: http://www.viam.ru (accessed: May 31, 2021). DOI: 10.18577/2307-6046-2016-0-10-4-4.
  7. Evgenov A.G., Bazyleva O.A., Korolev V.A., Arginbaeva E.G. Prospects of Ni3Al-based intermetallic alloy VKNA-4UR application in additive technologies. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 31–35. DOI: 10.18577/2071-9140-2016-0-S1-31-35.
  8. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Development trends of nickel-based intermetallic alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  9. Garibov G.S. Theory of crystallization and technology of granulated heat-resistant nickel alloys. Tekhnologiya legkikh splavov, 2016, no. 1, pp. 107–118.
  10. Garibov G.S., Grits N.M. V.I. Dobatkin and metallurgy of high-temperature nickel alloy granules. Tekhnologiya legkikh splavov, 2015, no. 2, pp. 34–39.
  11. Eskin G.I. On the conditions for the formation of a non-dendritic structure in ingots and granules from heat-resistant nickel alloys. Tekhnologiya legkim splavov, 2013, no. 4, pp. 147–159.
  12. Gessinger G.Kh. Powder metallurgy of heat-resistant alloys. Trans. from English Chelyabinsk: Metallurgy, 1988, 320 p.
  13. Bazyleva O.A., Efimochkin I.Y., Arginbaeva E.G., Kuptsov R.S., Karashaev M.M. Composite Material Based оn Intermetallic Alloy оf VKNA Type Reinforced With Oxide Particles. Inorganic Materials: Applied Research, 2021, vol. 12, no. 2, pp. 307–312.
  14. Abuzin Yu.A., Karashaev M.M., Roslyakov S.I. High-temperature composite material based on Nb reinforced with Al2O3. Uspekhi sovremennoy nauki, 2016, vol. 3, no. 6, pp. 6–12.
  15. Abuzin Yu.A., Karashaev M.M., Sokolov R.A. Evaluation of Energy Efficiency of the Aluminothermic Process of Producing Metal Composite Materials by the Criteria of the Maximum Self-Heating Temperature and the Aggregate State of Oxygen Exchange Reaction Products // International Journal of Nanomechanics Science and Technology, 2015, vol. 6, no. 4, pp. 299–304.
  16. Abuzin Yu.A., Karashaev M.M., Roslyakov S.I. Development of the fundamentals of the production technology and methods for controlling the structure of a high-temperature composite material of the Nb–Al2O3 system. Tekhnologiya legkikh splavov, 2017, no. 1, pp. 60–68.
  17. Garibov G.S. Scientific and technical groundwork in the field of granular metallurgy for the creation of advanced aircraft engines. Tekhnologiya legkikh splavov, 2018, no. 2, pp. 63–71.
  18. Reed R.C. The Superalloys: Fundamentals and Applications. Cambridge: Cambridge University Press, 2006, 370 p.
  19. Povarova K.B., Lomberg B.S., Filin S.A., Kazanskaya N.K., Shkolnikov D.Yu., Bespalova M.D. Structure and properties of (β + γ)-alloys of the Ni–Al–Co system. Metally, 1994, no. 3, pp. 77–81.
  20. Zhitnyuk S.V., Sorokin O.Yu., Zhuravleva P.L. Silicon carbide ceramics obtained by sintering granular powder. Trudy VIAM, 2020, no. 2 (86), paper no. 06. Available at: http://www.viam-works.ru (accessed: May 31, 2021). DOI: 10.18577/2307-6046-2020-0-2-50-59.
  21. Sevostyanov N.V., Efimochkin I.Yu., Basargin O.V., Burkovskaya N.P. Stages of the process of synthesis of titanium carbosilicide from simple elements by the method of spark plasma sintering (SPS). Metallovedenie i termicheskaya obrabotka metallov, 2020, no. 3 (777), pp. 55–59.