The influence of climatic factors on residual stresses in nanomodified cyanate ester-based CFRP

Startsev V.O., Nikolaev E.V., Vardanyan A.M., Nechaev A.A.
Startsev V.O., Nikolaev E.V., Vardanyan A.M., Nechaev A.A. The influence of climatic factors on residual stresses in nanomodified cyanate ester-based CFRP // Proceedings of VIAM. 2021. No. 8. DOI: 10.18577/2307-6046-2021-0-8-104-112. URL: https://www.viam-works.ru/en/journal/2021/8/12
Keywords
CFRP, nanoscale additives, residual stresses, climatic testing, resign post-cure, mechanical properties, thermal expansion.
Abstract

The residual stresses in carbon fiber reinforced plastic (CFRP), based on VTkU-2.200 carbon fiber and VSC-14 cyanate ester resin, modified by nanoscale additives (astralen) were studied. Natural exposure was performed in a moderately cold climate. The influence of nanoadditives on mechanical and physical CFRP’s properties after 9 months of climatic testing was studied using the following properties: three-point bending strength, compression strength, coefficient of linear thermal expansion, glass transition temperature and residual stresses parameters. The increase of residual stresses after climatic testing was revealed.

Reference list
  1. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Prospects for the use of carbon-containing nanoparticles in binders for polymer composite materials. Rossiyskiye nanotekhnologii, 2012, no. 3-4. S. 20–42.
  2. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Development of FSUE "VIAM" in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  3. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  4. Startsev V.O., Golushko S.K., Valevin E.O., Gunyaeva A.G., Amelina E.V. Influence of a nanomodifier on the climatic resistance of carbon fiber reinforced plastic based on a cyanoester binder. Materials conf. "Climate 2020: modern approaches to assessing the impact of external factors on materials and complex technical systems". Moscow: VIAM, 2020, pp. 134–149. Available at: https://conf.viam.ru/conf/338/proceedings (accessed: July 18, 2021).
  5. Hahn H.T. Residual Stresses in Polymer Matrix Composite Laminates. Journal of Composite Materials, 1976, vol. 10, no. 4, pp. 266–278.
  6. Hancox N. Thermal effects on polymer matrix composites. Part 1. Thermal cycling. Materials & Design, 1998, vol. 19, no. 3, pp. 85–91.
  7. Dutta P.K. Structural fiber composite materials for cold regions. Journal of Cold Regions Engineering, 1988, vol. 2, no. 3, pp. 124–134.
  8. Awaja F., Zhang S., Tripathi M., Nikiforov A., Pugno N. Cracks, microcracks and fracture in polymer structures: Formation, detection, autonomic repair. Progress in Materials Science, 2016, vol. 83, pp. 536–573.
  9. Startsev O.V., Lebedev M.P., Kychkin A.K. Aging of polymer composite materials in extremely cold climates. Izvestiya Altayskogo gosudarstvennogo universiteta, 2020, no. 1 (111), pp. 41–51.
  10. Harper B.D., Weitsman Y. On the effects of environmental conditioning on residual stresses in composite laminates. International Journal of Solids and Structures, 1985, no. 8, pp. 907–926.
  11. Startsev O.V., Polyakov V.V., Salita D.S., Lebedev M.P. Acoustic Emission at the Crack Tip during Cooling of a Moisture-Saturated Composite. Doklady Physical Chemistry, 2020, vol. 493, no. 1, pp. 91–94.
  12. Startsev O.V., Vapirov Y.M., Lebedev M.P., Kychkin A.K. Comparison of Glass-Transition Temperatures for Epoxy Polymers Obtained by Methods of Thermal Analysis. Mechanics of Composite Materials, 2020, vol. 56, no. 2, pp. 227–240.
  13. Perov NS, Startsev V.O., Chutskova E.Yu., Gulyaev A.I., Abramov D.V. Properties of carbon fiber reinforced plastic based on polycyanurate binder after exposure to various natural and artificial environments. Materialovedenie, 2017, no. 2, pp. 3–9.
  14. Dolgova EV, Akhmadieva KR, Bokov VV et al. Cyanester binders. Getting, properties, application. Polymer composite materials for the aerospace industry: materials of All-Rus. Scientific and Technical Conf. Moscow: VIAM, 2019, pp. 42–52.
  15. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials: 1. Aging mechanisms. Russian Metallurgy (Metally), 2011, no. 10, pp. 993–1000.
  16. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. 1. Assessment of the influence of significant influencing factors. Deformatsiya i razrushenie materialov, 2019, no. 12, pp. 7–16.
  17. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. 2. Development of research methods for the early stages of aging. Deformatsiya i razrushenie materialov, 2020, no. 1, pp. 15–21.
  18. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  19. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  20. Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.