FRP structures radius zones ultrasonic testing (review)

Boychuk A.S., Dikov I.A., Generalov A.S., Slavin A.V.
Boychuk A.S., Dikov I.A., Generalov A.S., Slavin A.V. FRP structures radius zones ultrasonic testing (review) // Proceedings of VIAM. 2021. No. 8. DOI: 10.18577/2307-6046-2021-0-8-92-103. URL: https://www.viam-works.ru/en/journal/2021/8/11
Keywords
fiber reinforced plastics (FRP), radius testing, non-destructive testing, ultrasonic testing, phased array, pulse-echo method.
Abstract

The review of FRP structures radius zones ultrasonic non-destructive testing techniques is given in the paper. It is shown that both single-element piezoelectric transducers and phased arrays can currently be used to solve this problem. It is necessary to use special tools for positioning and creating an acoustic contact with both types of transducers. Ultrasonic testing using the described tools allows detecting defects in radius zones up to 6 mm in size.

Reference list
  1. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  2. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  3. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  4. Zhelezina G.F., Solovyeva N.A., Makrushin K.V., Rysin L.S. Polymer composite materials for manufacturing engine air particle separation of advanced helicopter engine. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 58–63. DOI: 10.18577/2071-9140-2018-0-1-58-63.
  5. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  6. Timoshkov P.N. Equipment and materials for the technology of automated calculations prepregs. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  7. Ivanov N.V., Gurevich Ya.M., Khaskov M.A., Akmeev A.R. Mode studying curing binding VSE-34 and its influences on mechanical properties. Aviacionnyye materialy i tehnologii, 2017, no. 2, pp. 50–55. DOI: 10.18577 / 2071-9140-2017-0-2-50-55.
  8. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  9. González S., Herrera Á., Fernández R. etc. Ad-hoc solutions for ultrasonic inspection of radii in closed composite Structures. 11th International Symposium «NDT in Aerospace». Paris, 2019. Available at: https://https://www.ndt.net/article/aero2019/papers/fp_fri2b3_s_gonzalez.pdf (accessed: May 6, 2021).
  10. We developed a unique solution for real-time detection of defects in composite plates using acousto-ultrasonic tomography (AUT). Creo Dynamics. 2021. Available at: https://creodynamics.com/portfolio-posts/acousto-ultrasonic-tomography (accessed: May 7, 2021).
  11. Kite A.H. Nondestructive evaluation of a carbon fiber wing spar using air-coupled ultrasound. Retrospective Theses and Dissertations. 2007. Available at: https://https://lib.dr.iastate.edu/cgi/viewcontent.cgi?article=16040&context=rtd (accessed: May 6, 2021).
  12. Rau E., Grauvogl E., Manzke H. etc. Ultrasonic Phased Array Testing of Complex Aircraft Structures. ECNDT. 2006. Tu. 1.1.2. Available at: https://www.ndt.net/article/ecndt2006/doc/Tu.1.1.2.pdf (accessed: May 7, 2021).
  13. Boychuk A.S., Generalov A.S., Dalin M.A., Stepanov A.V. Non-destructive testing of technological violations of the continuity of the T-shaped zone of an integral structure made of PCM using ultrasonic phased arrays. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 10, pp. 38–44.
  14. Boychuk A.S. Development of technologies for non-destructive testing of monolithic structures made of carbon fiber using ultrasonic antenna arrays: thesis, Cand. Sc. (Tech.). Moscow, 2016, 203 p.
  15. Lamarre A. Ultrasonic phased-array and eddy current array as approved methods for aircraft maintenance. Aerospace Testing Conference. Hamburg, 2006. Available at: https://https://ndt.aero/images/docs/UTPAfor%20maintenance.pdf (accessed: May 7, 2021).
  16. Boychuk A.S., Generalov A.S., Dalin M.A., Dikov I.A. Inspection of monolithic parts and structures of aviation equipment made of PCM by ultrasonic non-destructive testing using phased arrays. TestMat. The main trends, directions and prospects for the development of non-destructive testing methods in the aerospace industry: collection of articles. materials of the X All-Russia. conf. (Moscow, February 9, 2018). Moscow: VIAM, 2018, pp. 18–31. Available at: https://https://conf.viam.ru/sites/default/files/uploads/proceedings/1063.pdf (accessed: May 7, 2021).
  17. Flexible Phassed Array Scanning Tool. Phoenix ISL. 2021. Available at: https://www.phoenixisl.com/ product/wrapit (accessed: May 7, 2021).
  18. Flexible Ultrasonic Phased-Array Probe for Complex Shape Inspection. Olympus Corporation. 2021. Available at: https://www.olympus-ims.com/en/applications/flexible-ultrasonic-phased-array-probe-for-complex-shape-inspection (accessed: May 7, 2021).