Features of the formation of the structural-phase state of the EP648 alloy during selective lase manufacture

Ospennikova O.G., Naprienko S.A., Medvedev P.N., Zaysev D.V., Rogalev A.M.
Ospennikova O.G., Naprienko S.A., Medvedev P.N., Zaysev D.V., Rogalev A.M. Features of the formation of the structural-phase state of the EP648 alloy during selective lase manufacture // Proceedings of VIAM. 2021. No. 8. DOI: 10.18577/2307-6046-2021-0-8-3-11. URL: https://www.viam-works.ru/en/journal/2021/8/1
Keywords
alloy EP648, SLM, additive technologies, structural-phase state, texture, SEM, TEM.
Abstract

The paper shows the features of the formation of the structural-phase and textural state of the EP648 alloy obtained by the SLM method in the initial state, after hot isostatic pressing and heat treatment. It was found that in the process of synthesis, a limited crystallographic texture of the γ-phase is formed, which does not undergo significant changes in the process of subsequent treatments. The uniform distribution of fine particles of the hardening phases, apparently, leads to an increase in both the strength and plastic properties of the material obtained by the SLM method in comparison with the material obtained by the traditional technology.

Reference list
  1. Sims Ch., Hagel V. Heat-resistant alloys. Trans. from Engl. Moscow: Metallurgiya, 1976, 568 p.
  2. Kishkin S.T., Kablov E.N. Casting heat-resistant alloys for turbine blades. Aviation materials. Selected works of "VIAM" 1932–2002. Moscow: VIAM, 2002. S. 48–58.
  3. Kablov E.N., Golubovsky E.R. Heat resistance of nickel alloys. Moscow: Mashinostroenie, 1998, 464 p.
  4. Kablov E.N., Evgenov A.G., Ospennikova O.G., Semenov B.I., Semenov A.B., Korolev V.A. Metal-powder compositions of EP648 heat-resistant alloy produced by FSUE "VIAM" State Scientific Center of the Russian Federation in technologies of selective laser fusion, laser gas-powder surfacing and high-precision casting of polymers filled with metal powders. Izvestiya vysshikh uchebnykh zavedeniy, Mashinostroene. 2016, no. 9 (678), pp. 62–80.
  5. Kablov E.N., Evgenov A.G., Mazalov I.S., Shurtakov S.V., Zaitsev D.V., Prager S.M. Structure and properties of EP648 and VZh159 alloys synthesized by selective laser alloying after imitation annealing. Materialovedenie, 2020, no. 6, pp. 3–10.
  6. Evgenov A.G., Gorbovec M.A., Prager S.M. Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  7. Ospennikova O.G., Naprienko S.A., Medvedev P.N., Krupnina O.A., Rogalev A.M. Fea-tures of the structure of Ti–6Al–4V alloy obtained by selective laser melting. Trudy VIAM, 2019, no. 10 (82), paper no. 02. Available at: http://www.viam-works.ru (accessed: May 18, 2021). DOI: 10.18577/2307-6046-2019-0-10-14-24.
  8. Carter L., Martin C., Withers P., Attallah M. The influence of the laser scan strategy on grain structure and cracking behavior in SLM powder-bed fabricated nickel superalloy. Journal of Alloys and Compounds, 2014, vol. 615, pp. 338–347.
  9. Zhu Y., Liu D., Tian X. et al. Characterization of microstructure and mechanical properties of laser melting deposited Ti – 6.5Al – 3.5Mo – 1.5Zr – 0.3Si titanium alloy. Materials and Design, 2014, vol. 56, p. 445-453.
  10. Gaiduk S.V., Kononov V.V., Nalesny N.B. Investigation of dendritic liquation and phase inhomogeneity in heat-resistant corrosion-resistant nickel alloys. Vestnik dvigatelestroyeniya, 2006, no. 1, pp. 150–154.
  11. 11 Bazyleva O.A., Unchikova M.V., Turenko E.Yu., Bagetov V.V., Shestakov A.V. Study of heat treatment effect on structure, dendritic liquation parameters and time to failure of Ni3Al-based alloy containing Re). Trudy VIAM, 2016, no. 10, paper no. 4. Available at: http://www.viam.ru (accessed: May 20, 2021) DOI: 10.18577/2307-6046-2016-0-10-4-4.
  12. Lukina E.A., Filonova E.V., Treninkov I.A. The microstructure and preferential crystallographic orientation of nickel superalloy, synthesized by SLM method, depending of the energy impact and heat treatment. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 38–44. DOI: 10.18577/2071-9140-2017-0-1-38-44.
  13. Shalin R.E., Svetlov I.L., Kachanov E.B., Toloraia V.N., Gavrilin O.S. Single crystals of nickel heat-resistant alloys. Moscow: Mashinostroenie, 1997, 336 p.