Investigation of the influence of the thermal regime of FDM printing on the structuring and warping of polyethylene samples

Kablov E.N., Kondrashov S.V., Melnikov A.A., Pavlenko S.A., Guseva M.A., Pykhtin A.A., Larionov S.A.
Kablov E.N., Kondrashov S.V., Melnikov A.A., Pavlenko S.A., Guseva M.A., Pykhtin A.A., Larionov S.A. Investigation of the influence of the thermal regime of FDM printing on the structuring and warping of polyethylene samples // Proceedings of VIAM. 2021. No. 7. DOI: 10.18577/2307-6046-2021-0-7-48-58. URL: https://www.viam-works.ru/en/journal/2021/7/6
Keywords
FDM printing, polyolefins, warpage, physical and mechanical properties, rheological properties, microstructure.
Abstract

The study of the influence of the temperature of polyethylene printing on the dimensional stability of samples obtained by the method of FDM printing has been carried out. It is shown that a change in the temperature of the nozzle from 200 to 260 °C leads to a decrease in the deviation from the plane by a factor of eight. In this case, the tensile strength remains practically unchanged, and the elongation increases by 30 %. It has been established by the methods of rheological and microstructural studies that the observed effect is associated with a change in the structure of polyethylene, which is initiated by an increased temperature of the printer's extruder head. It has been suggested that the likely reason for the change in the structure of polyethylene is a change in the course of the crystallization process due to partial thermal oxidative destruction of the polymer matrix in the extruder head of a 3D printer.

Reference list
  1. Kablov E.N. Present and future of additive technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  2. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  3. Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  4. Petrova G.N., Larionov S.A., Platonov M.M., Perfilova D.N. Thermoplastic materials of new generation for aviation. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 420–436. DOI: 10.18577/2071-9140-2017-0-S-420-436.
  5. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  6. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  7. Kondrashov S.V., Pykhtin A.A., Larionov S.A., Sorokin A.E. Influence of the technological FDM-modes of the press and structure of used materials on physic-mechanical cha-racteristics of FDM-models (review). Trudy VIAM, 2019, no. 10 (82), paper no. 04. Available at: http://www.viam-works.ru (accessed: June 1, 2021). DOI: 10.18577/2307-6046-2019-0-10-34-49.
  8. Zhao F., Li D., Jin Z. Preliminary investigation of poly-ether-ether-ketone based on fused deposition modeling for medical applications. Materials, 2018, vol. 11, no. 2, pp. 288–299.
  9. Rinaldi M., Ghidini T., Cecchini F. et al. Additive layer manufacturing of poly (ether ether ketone) via FDM. Composites Part B: Engineering, 2018, vol. 145, pp. 162–172.
  10. Zhang X., Fan W., Liu T. Fused deposition modeling 3D printing of polyamide-based composites and its applications. Composites Communications, 2020, vol. 21, pp. 100413.
  11. Peng X., Zhang M., Guo Z. et al. Investigation of processing parameters on tensile performance for FDM-printed carbon fiber reinforced polyamide 6 composites. Composites Communications, 2020, vol. 22, pp. 100478.
  12. Geng P., Zhao J., Gao Z. et al. Effects of Printing Parameters on the Mechanical Properties of High-Performance Polyphenylene Sulfide Three-Dimensional Printing. 3D Printing and Additive Manufacturing, 2021, vol. 8, no. 1, pp. 33–41.
  13. El Magri A., Vaudreuil S., El Mabrouk K. et al. Printing temperature effects on the structural and mechanical performances of 3D printed Poly-(phenylene sulfide) material. Materials Science and Engineering: IOP Conference Series, 2020, vol. 783, no. 1, pp. 012001.
  14. Mohamed O.A., Masood S.H., Bhowmik J.L. Optimization of fused deposition modeling process parameters: a review of current research and future prospects. Advances in Manufacturing, 2015, vol. 3, no. 1, pp. 42–53.
  15. Kochesfahani S.H. Improving PLA-based material for FDM 3D-printers using minerals (principles and method development). Proceedings of the Society of Plastics Engineers Annual Technical Conference, 2016, pp. 1958–1614.
  16. Turner B.N., Gold S.A. A review of melt extrusion additive manufacturing processes: II. Materials, dimensional accuracy, and surface roughness. Rapid Prototyping Journal, 2015, vol. 21, no. 3, pp. 250–261.
  17. Duty C., Ajinjeru C., Kishore V. et al. What makes a material printable? A viscoelastic model for extrusion-based 3D printing of polymers. Journal of Manufacturing Processes, 2018, vol. 35, no. 10, pp. 526–537.
  18. Mark J.E. Physical properties of polymers handbook. New York: Springer, 2007, p. 825.
  19. Tager A.A. Physicochemistry of polymers. Moscow: Nauchnyy mir, 2007, 573 p.
  20. Spoerk M., Holzer C., Gonzalez‐Gutierrez J. Material extrusion‐based additive manufacturing of polypropylene: A review on how to improve dimensional inaccuracy and warpage. Journal of Applied Polymer Science, 2020, vol. 137, no. 12, pp. 48545.
  21. Rosli A.A., Shuib R.K., Ishak K.M. et al. Influence of bed temperature on warpage, shrinkage and density of various acrylonitrile butadiene styrene (ABS) parts from fused deposition modelling (FDM). AIP Conference Proceedings, 2020, vol. 2267, no. 1, pp. 020072.
  22. Alsoufi M.S., Elsayed A.E. Warping deformation of desktop 3D printed parts manufactured by open source fused deposition modeling (FDM) system. International Journal of Mechanical and Mechatronics Engineering, 2017, vol. 17, pp. 7–16.
  23. Peng A.H. Research on the interlayer stress and warpage deformation in FDM. Advanced Materials Research, 2012, vol. 538, pp. 1564–1567.
  24. Noriega A., Blanco D., Alvarez B.J. et al. Dimensional accuracy improvement of FDM square cross-section parts using artificial neural networks and an optimization algorithm. The International Journal of Advanced Manufacturing Technology, 2013, vol. 69, no. 9–12, pp. 2301–2313.
  25. Dilberoglu U.M., Simsek S., Yaman U. Shrinkage compensation approach proposed for ABS material in FDM process. Materials and Manufacturing Processes, 2019, vol. 34, no. 9, pp. 993–998.
  26. Pickering K., Stoof D. Sustainable composite fused deposition modeling filament using post-consumer recycled polypropylene. Journal of Composites Science, 2017, vol. 1, no. 2, pp. 17.
  27. Dong M., Zhang S., Gao D. et al. The study on polypropylene applied in fused deposition modeling. AIP Conference Proceedings, 2019, vol. 2065, no. 1, pp. 030059.
  28. Spoerk M., Sapkota J., Weingrill G. et al. Shrinkage and Warpage Optimization of Expanded-Perlite-Filled Polypropylene Composites in Extrusion-Based Additive Manufacturing. Macromolecular Materials and Engineering, 2017, vol. 302, no. 10, pp. 1700143.
  29. Chatham C.A., Zawaski C.E., Bobbitt D.C. et al. Semi‐Crystalline Polymer Blends for Material Extrusion Additive Manufacturing Printability: A Case Study with Poly (ethylene terephthalate) and Polypropylene. Macromolecular Materials and Engineering, 2019, vol. 304, no. 5, pp. 1800764.
  30. Das A., Marnot A.E.С., Fallon J.J. et al. Material extrusion-based additive manufacturing with blends of polypropylene and hydrocarbon resins. ACS Applied Polymer Materials, 2019, vol. 2, no. 2, pp. 911–921.
  31. Spiegel G., Paulik C. Polypropylene Copolymers Designed for Fused Filament Fabrication 3D‐Printing. Macromolecular Reaction Engineering, 2020, vol. 14, no. 1, pp. 1900044.
  32. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  33. Kim B.K., Kim K.J. Cross‐Linking of polypropylene by peroxide and multifunctional monomer during reactive extrusion. Advances in Polymer Technology: Journal of the Polymer Processing Institute, 1993, vol. 12, no. 3, pp. 263–269.
  34. Chodak I., Zimanyova E. The effect of temperature on peroxide initiated crosslinking of polypropylene. European Polymer Journal, 1984, vol. 20, no. 1, pp. 81–84.
  35. Krajenta J., Safandowska M., Pawlak A. The re-entangling of macromolecules in polypropylene. Polymer, 2019, vol. 175, pp. 215–226.
  36. Tuskaev V.A., Gagieva S.C., Kurmaev D.A. et al. Novel titanium (IV) diolate complexes with additional O‐donor as precatalyst for the synthesis of ultrahigh molecular weight polyethylene with reduced entanglement density: Influence of polymerization conditions and its implications on mechanical properties. Applied Organometallic Chemistry, 2021, pp. e6256.
  37. Measurement of viscosity and activation energy of liquid molecules. Available at: http://genphys.phys.msu.ru/rus/lab/mol/Lab208(2018).pdf (accessed: May 30, 2021).
  38. Bertolino M., Battegazzore D., Arrigo R. et al. Designing 3D printable polypropylene: Material and process optimization through reology. Additive Manufacturing, 2021, vol. 40, pp. 101944.