Metal composite materials based on titanium alloys, reinforced with refractory particles (review)
Krasnov E.I., Serpova V.M., Khodykin L.G., Gololobov A.V. Metal composite materials based on titanium alloys, reinforced with refractory particles (review) // Proceedings of VIAM. 2021. No. 6. DOI: 10.18577/2307-6046-2021-0-6-36-45. URL: https://www.viam-works.ru/en/journal/2021/6/4
Keywords
metal composite material, titanium, refractory particles, strength, heat treatment, physical and mechanical properties.
Abstract
Presents a literature review in the field of methods for strengthening titanium and its alloys by introducing various refractory particles into the matrix. The main problematic issues related to the chemical nature of refractory particles and titanium alloys that arise during hardening are briefly described. The main structural, physical and mechanical properties and morphology of such metal composite materials are described. The dependence of the influence of various refractory particles and their amount, as well as the effect of heat treatment on the physical and mechanical properties of microns based on titanium alloys, is presented.
Reference list
- Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
- Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
- Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 7. Available at: http://www.viam-works.ru (accessed: June 2, 2021). DOI: 10.18577/2307-6046-2020-0-1-68-77.
- Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
- Krasnov E.I., Kurbatkina E.I., Shavnev A.A., Serpova V.M., Zhabin A.N. Application of the active brazing method for connecting fiber materials with ceramic materials (review). Trudy VIAM, 2020, no. 10 (92), paper no. 7. Available at: http://www.viam-works.ru (accessed: June 2, 2021). DOI: 10.18577/2307-6046-2020-0-10-63-72.
- Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
- Tian Y.S., Chen C.Z., Chen L.B., Liu J.H. Wear properties of alloyed layers produced by laser surface alloying of pure titanium with B4C and Ti mixed powders. Journal of Materials Science, 2005, no. 40, pp. 4387–4390. DOI: 10.1007/s10853-005-0736-2.
- Fouvry S., Paulin C., Deyber S. Impact of contact size and complex gross-partial slip conditions on Ti–6Al–4V/Ti–6Al–4V fretting wear. Tribology International, 2009, vol. 42, is. 3, pp. 461–474. DOI: 10.1016/j.triboint.2008.08.005.
- Qin Y.L., Geng L. Dry sliding wear behavior of titanium matrix composites hybrid-reinforced by in situ TiB whisker and TiC particle. Journal of Materials Science, 2011, no. 46 (14), pp. 4980–4985. DOI: 10.1007/s10853-011-5415-x.
- Peng W.W., Zeng W.D., Wang Q.J., Yu H.Q. Comparative study on constitutive relationship of as-cast Ti60 titanium alloy during hot deformation based on Arrhenius-type and artificial neural network models. Materials and Design, 2013, vol. 51, pp. 95–104. DOI: 10.1016/j.matdes.2013.04.009.
- Popov A., Rossina N., Popova M. The effect of alloying on the ordering processes in near-alpha titanium alloys. Materials Science and Engineering A, 2013, vol. 564, pp. 284–287. DOI: 10.1016/j.msea.2012.11.043.
- Fu B.G., Wang H.W., Zou C., Wei Z. The effects of Nb content on microstructure and fracture behavior of near α titanium alloys. Materials and Design, 2015, vol. 66, part A, pp. 267–273. DOI: 10.1016/j.matdes.2014.10.069.
- Jia W.J., Zeng W.D., Liu J.R. Influence of thermal exposure on the tensile properties and microstructures of Ti60 titanium alloy. Materials Science and Engineering A, 2011, vol. 530, pp. 511–518. DOI: 10.1016/j.msea.2011.10.011.
- Soorya Prakash K., Gopal P.M., Anburose D., Kavimani V. Mechanical, corrosion and wear characteristics of powder metallurgy processed Ti–6Al–4V/B4C metal matrix composites. Ain Shams Engineering Journal, 2018, vol. 9, is. 4, pp. 1489–1496. DOI: 10.1016/j.asej.2016.11.003.
- Balaji V.S., Kumaran S. Dry sliding wear behavior of titanium (TiB + TiC) in situ composite developed by spark plasma sintering. Tribology Transactions, 2015, vol. 58, is. 4, pp. 698–703. DOI: 10.1080/10402004.2014.993780.
- Zheng B., Dong F., Yuan X. et al. Microstructure and tribological behavior of in situ synthesized (TiB + TiC)/Ti6Al4V (TiB/TiC = 1/1) composites. Tribology International, 2020, vol. 145. Reference 106177. DOI: 10.1016/j.triboint.2020.106177.
- Mohanavel V., Vijayakumar M.D. Mechanical properties of titanium matrix composites fabricated via powder metallurgy method. Materials Today: Proceedings, 2020, pp. 5–10. DOI: 10.1016/j.matpr.2020.04.569.
- Fereiduni E., Ghasemi A., Elbestawi M. Selective laser melting of hybrid ex-situ/in-situ reinforced titanium matrix composites: Laser/powder interaction, reinforcement formation mechanism, and non-equilibrium microstructural evolutions. Materials & Design, 2019, vol. 184. Reference 108185. DOI: 10.1016/j.matdes.2019.108185.
- Loretto M.H., Konitzer D.G. The effect of matrix reinforcement reaction on fracture in Ti–6Ai–4V-base composites. Metallurgical Transactions A, 1990, vol. 21А, pp. 1579–1587. DOI: 10.1007/BF02672573.
- Reeves A.J., Dunlop H., Clyne T.W. The effect of interfacial reaction layer thickness on fracture of titanium-SiC particulate composites. Metallurgical Transactions A, 1992, vol. 23, is. 3, pp. 977–988. DOI: 10.1007/BF02675572.
- Tong W., Ravichandran G., Christman T., Vreeland T. Processing SiC-particulate reinforced titanium-based metal matrix composites by shock wave consolidation. Acta Metallurgica et Materialia, 1995, vol. 43, is. 1, pp. 235–250. DOI: 10.1016/0956-7151(95)90279-1.
- Wang B., Huang L.J., Geng L. Effects of heat treatments on the microstructure and mechanical properties of as-extruded TiBw/Ti6Al4V composites. Materials Science & Engineering A, 2012, vol. 558, pp. 663–667. DOI: 10.1016/j.msea.2012.08.071.
- Huang L.J., Geng L., Li A.B. et al. In situ TiBw/Ti–6Al–4V composites with novel reinforcement architecture fabricated by reaction hot pressing. Scripta Materialia, 2009, vol. 60, is. 11, pp. 996–999. DOI: 10.1016/j.scriptamat.2009.02.032.
- Wang B., Huang L.J., Geng L. et al. Effects of heat treatments on microstructure and tensile properties of as-extruded TiBw/near-α Ti composites. Materials and Design, 2015, vol. 85, pp. 679–686. DOI: 10.1016/j.matdes.2015.07.058.
- Badini C., Ubertalli G., Puppo D., Fino P. High temperature behaviour of a Ti–6Al–4V/TiCp composite processed by BE-CIP-HIP method. Journal of Materials Science, 2000, vol. 35, pp. 3903–3912. DOI: 10.1023/A:1004893700762.