Modeling of the curing process of a polymer resin and changes in microhardness in its volume

Postnov V.I., Kachura S.M., Veshkin E.A
Postnov V.I., Kachura S.M., Veshkin E.A Modeling of the curing process of a polymer resin and changes in microhardness in its volume // Proceedings of VIAM. 2021. No. 4. DOI: 10.18577/2307-6046-2021-0-4-92-99. URL: https://www.viam-works.ru/en/journal/2021/4/7
Keywords
polymer composite materials, binder EDT-69N, thermophysical modeling, finite element method, microhardness, degree of conversion.
Abstract

Curing parameters have the greatest impact on the physical and mechanical properties of FRP, therefore their optimum value is of particular importance for obtaining quality products. During curing temperature of the inner layers of the FRP can increase unevenly, which can lead to the formation of a gradient in the degree of conversion and heterogeneity of physical and mechanical properties. The article is devoted to the development of a mathematical model of the curing process of the EDT-69N resin, taking into account the kinetic parameters of curing and implementation thermophysical modeling using the finite element method.The correspondence of the family of curves for the degree of conversion along the sample cross-section and the family of microhardness curves is also shown.

Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  3. Marakhovsky P.S. Modeling of heat transfer in multilayer epoxy fiberglass and determination of the temperature-time regime of their molding by direct pressing: thesis, Cand. Sc. (Tech.). Moscow, 2019, 124 p.
  4. Veshkin E.A., Postnov V.I., Semenychev V.V. Methodology for assessing changes in matrix properties in the volume of polymer composites. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 7, pp. 25–32.
  5. Veshkin E.A., Postnov V.I., Semenychev V.V., Krasheninnikova E.V. Research of microhardness and sclero-metric characteristics of the binding UP-2227N, cured by different regimes. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 39–45. DOI: 10.18577/2071-9140-2018-0-1-39-45.
  6. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  7. Kablov E.N. The sixth technological order. Nauka i zhizn, 2010, no. 4, pp. 2–7.
  8. Zhelezina G.F., Solovyeva N.A., Makrushin K.V., Rysin L.S. Polymer composite materials for manufacturing engine air particle separation of advanced helicopter engine. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 58–63. DOI: 10.18577/2071-9140-2018-0-1-58-63.
  9. Barinov D.Ya., Marakhovsky P.S., Kutsevich K.E., Chutskova E.Yu. Mathematical modeling of temperature fields taking into account the kinetics of solidification of a thick-walled fiberglass plate. Perspektivnyye materialy, 2017, no. 5, pp. 19–28.
  10. Bulgakov B.A., Kalugin D.I., Babkin A.V. Mathematical modeling of the curing process of composite materials based on propargyl-modified phenol-formaldehyde resins. Khimiya i khimicheskaya tekhnologiya, 2015, vol. 58, no. 12, pp. 73–76.
  11. Dimitrienko Yu.I., Zakharova Yu.V., Sbornikov S.V. Modeling of the curing process of thick-walled structures made of polymer composite materials. Innovatsionnaya nauka. 2016, no. 12-4. C. 31–36.
  12. Chutskova E.Yu., Aleksashin V.M., Barinov D.Ya., Dementyeva L.A. The differential scanning calorimetry application for kinetic regularities investigation of the epoxy adhesive VK-36R curing process. Trudy VIAM, 2015, no. 1, paper no. 12. Available at: http://www.viam-works.ru (accessed: December 24, 2020). DOI: 10.18577/2307-6046-2015-0-1-12-12.
  13. Postnova M.V., Postnov V.I. Modern thermoanalytical methods for studying the properties of prepregs and materials based on them. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk, 2014, vol. 16, no. 1–5, pp. 1577–1582.
  14. Veshkin E.A., Postnov V.I., Semenichev V.V., Krasheninnikova E.V. Microhardness and sclerometry as criteria for the degree of curing of the EDT-69N binder. Materialovedenie, 2018, no. 10, pp. 3–7.
  15. Chen Yanyan, Marakhovskij P.S., Malysheva G.V. Determination of thermophysical properties of epoxy materials during their curing. Trudy VIAM, 2018, no. 9 (69), paper no. 12. Available at: http://www.viam-works.ru (accessed: December 12, 2020). DOI: 10.18577/2307-6046-2018-0-9-119-123.
  16. Barinov D.Ya., Marahovskiy P.S., Maltceva E.Yu., Besprozvanniy E.D., Aliasova E.E. Research of thermal conductivity of printed circuit boards based on aluminum substrate and alumina dielectric. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 43–48. DOI: 10.18577/2071-9140-2019-0-1-43-48.
  17. Khaskov M.A., Safronov E.V. The optimization of thermosetting matrixes curing schedule on the example of complex shape sample. Trudy VIAM, 2019, no. 12 (84), paper no. 06. Available at: http://www.viam-works.ru (accessed: December 24, 2020). DOI: 10.18577/2307-6046-2019-0-12-46-54.
  18. Heinze S., Echtermeyer A. A Practical Approach for Data Gathering for Polymer Cure Simulations. Applied Sciences, 2018, vol. 8, no. 11, p. 2227.
  19. Behzad T., Sain M. Cure Simulation of Hemp Fiber Acrylic Based Composites during Sheet Molding Process. Polymers and Polymer Composites, 2005, vol. 13, no. 3, pp. 235–244.
  20. Behzad T., Sain M. Finite element modeling of polymer curing in natural fiber reinforced composites. Composites Science and Technology, 2007, vol. 67, no. 7-8, pp. 1666–1673.