Manufacturing technologies of polymer composite materials on thermoplastics (review)

Sorokin A.E., Sagomonova V.A., Petrova A.P., Solovyanchik L.V.
Sorokin A.E., Sagomonova V.A., Petrova A.P., Solovyanchik L.V. Manufacturing technologies of polymer composite materials on thermoplastics (review) // Proceedings of VIAM. 2021. No. 3. DOI: 10.18577/2307-6046-2021-0-3-78-86. URL: https://www.viam-works.ru/en/journal/2021/3/7
Keywords
thermoplastics, composite materials, thermoplastic matrix, technology, prepreg, pultrusion, melt technology, film technology, fiber technology.
Abstract

Various technologies for the production of prepregs based on a thermoplastic matrix and composite materials based on them are considered. Their advantages over the technologies of manufacturing polymer composite materials based on a thermosetting matrix are presented. It is shown that the use of melt technology allows the production of fiberglass with the highest level of strength characteristics. An algorithm for estimating residual stresses in a thermoplastic composite to optimize the technological process of producing complex products is described.

Reference list
  1. Donetskiy K.I., Bystrikova D.V., Karavaev R.Yu., Timoshkov P.N. Application of polymeric composite materials for creation of elements of transmissions of aviation engineering (review). Trudy VIAM, 2020, no. 3 (87), paper no. 09. Available at: http://www.viam-works.ru (accessed: February 28, 2021). DOI: 10.18577/2307-6046-2020-0-3-82-93.
  2. Petrova G.N., Bader E.Ya. Structural materials based on reinforced thermoplastics. Rossiyskiy khimicheskiy zhurnal, 2010, vol. 54, no. 1, pp. 30–40.
  3. Petrova G.N., Bader E.Ya. Injection molded thermoplastic materials for aerospace purposes. Rossiyskiy khimicheskiy zhurnal, 2010, vol. 54, no. 1, pp. 41–45.
  4. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  5. Sorokin A.E., Bejder E.Ya., Izotova T.F., Nikolaev E.V., Shvedkova A.K. Investigation of carbon fiber reinforced plastic on polyphenylenesulfide resin after accelerated and natural climatic test. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 66–72. DOI: 10.18577/2071-9140-2016-0-3-66-72.
  6. Bondaletova L.I., Bondaletov V.G. Polymer composite materials: textbook. Tomsk: Publishing house of Tomsk Polytechnic University, 2013, 118 p.
  7. Johnson R.O., Teutsch E.O. Thermoplastic aromatic polymer composites. Polymer composites, 1983, vol. 4, no. 3, pp. 162–166.
  8. Johnston N.J., Clair T.L.St., Baucom R.M., Towell T.W. Polyimide Matrix Composites: Polyimidesulfone/LARC-TPI (1: 1) Blend. Tomorrow's Materials, 1989, vol. 34, pp. 976–987.
  9. Kotomin S.V., Barankova T.I., Plotnikova E.L., Filippova T.N. Obtaining and properties of microplastics with polysulfone and montmorilonite. Vse materialy. Entsiklopedicheskiy spravochnik, 2016, no. 2, pp. 2–9.
  10. Kotomin S.V., Ivanova R.S., Konkin A.A., Molchanov B.I. Kinetics of carbon fiber impregnation with thermoplastic melts. Khimicheskiye volokna, 1981, no. 6, pp. 29–31.
  11. Kotomin S.V., Avdeev N.N. Wetting of chemical fibers with thermoplastic melts. Kolloidnyy zhurnal, 1999, vol. 61, no. 3, pp. 336–343.
  12. Barantseva T.E., Gorbatkina Yu.A., Kravchenko T.P., Kerber M.L. Adhesive strength during the interaction of polyamides with aramid fibers. Khimicheskiye volokna, 1997, no. 5, pp. 51–55.
  13. Bolotina L.M., Gorbatkina Yu.A., Ivanova-Mumzhieva V.G., Korneeva N.V. Influence of the molecular weight of polysulfones on their adhesion to fibers. Vysokomolekulyarnye soyedinenia, series B, 2002, vol. 44, no. 8, pp. 433–444.
  14. Korneeva N.V., Gorbatkina Yu.A., Ivanova-Mumzhieva V.G. et al. Adhesion of thermoplastic matrices with different molecular weights to fibers. Mekhanika kompozitnykh materialov, 2002, vol. 38, no. 4, pp. 433–444.
  15. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  16. Kablov E.N. Aviation and Space Materials Science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  17. Kablov E.N. Chemistry in Aviation Materials Science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. 54, no. 1, pp. 3–4.
  18. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy, ser.: Chemistry and Chemical Technology, 2016, vol. 59, no. 10, pp. 61–71.
  19. Petrova G.N., Beider E.Ya., Izotova T.F., Malyshenok S.V. Composite thermoplastic materials – methods of production and processing. Vse materialy. Entsiklopedicheskiy spravochnik, 2013, no. 10, pp. 10–17.
  20. Tkachuk A.I., Grebeneva T.A., Chursova L.V., Panina N.N. Thermoplastic binders. The present and the future. Trudy VIAM, 2013, no. 11, paper no. 07. Available at: http://www.viam-works.ru (accessed: January 14, 2021).
  21. Agafonova A.S., Kondrashov S.V. Features of a technology to manufacture monolithic glass-fiber plastics intended for radio engineering. Aviacionnye materialy i tehnologii, 2014, no. 1, pp. 30–33. DOI: 10.18577 / 2071-9140-2014-0-1-30-33.
  22. Beider E.Ya., Petrova G.N., Izotova T.F. An influence of coupling agent on properties of thermoplastic glass reinforced plastics. Trudy VIAM, 2014, no. 9, paper no. 07. Available at: http://viam-works.ru (accessed: January 14, 2021). DOI: 10.18577/2307-6046-2014-0-9-7-7.
  23. Beider E.Ya., Petrova G.N., Dykun M.I. Dressing of carbon fibers – fillers of thermoplastic carbon reinforced plastics. Trudy VIAM, 2014, no. 10, paper no. 03. Available at: http://www.viam-works.ru (accessed: January 14, 2021). DOI: 10.18577/2307-6046-2014-0-10-3-3.
  24. Zaborskaya L.V., Yurkevich O.R., Dovgyalo V.A., Pisanova E.V. Investigation of the regularities of combining dispersed polysulfone with reinforcing fibers in the preparation of composite materials. Mekhanika kompozitnykh materialov, 1991, no. 3, pp. 403–407.
  25. Ustinov V.A., Bader E.Ya. The use of composite materials with a thermoplastic matrix. Konstruktsii iz kompozitsionnykh materialov, 1991, no. 1, pp. 21–28.
  26. Petrova G.N., Perfilova D.N., Gryaznov V.I., Bejder E.Ya. Thermoflexible elastomer for replacement of rubbers. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 302–308.
  27. Petrova G.N., Rumyantseva T.V., Perfilova D.N., Bader E.Ya., Gryaznov V.I. Thermoplastic elastomers – a new class of polymer materials. Aviacionnye materialy i tehnologii, 2010, no. 4, pp. 20–25.
  28. Kryzhanovsky V.K., Burlov V.V., Panimatchenko A.D., Kryzhanovskaya Yu.V. Technical properties of polymeric materials: allowance. Saint Petersburg: Professiya, 2007, 240 p.
  29. Thermoplastic compositions: pat. US 3785916; filed 11.12.70; publ. 15.01.74.
  30. Treatment of carbon fiber: pat. US 4269876; filed 10.04.77; publ. 26.05.81.
  31. Zaixia F., Zhangyu, Yanmo Ch., Hairu L. Tensile Properties of Glass Fiber Knitted Fabric Reinforced Polypropylene Composite Made from GF/PP Commingled Yarn Affected by Prestretching. Journal of reinforced plastics and composites, 2006, vol. 25. P. 553–560.
  32. Shalin R.E., Zinoviev S.N., Pomerantseva K.P. and other Heat-resistant carbon-fiber reinforced plastic KMU-8. Aviatsionnaya promyshlennost, 1987, no. 5, pp. 10–19.
  33. Nelyub V.A. Technologies for preparing prepregs. Vse materialy, 2013, no. 3, pp. 12–17.
  34. Narkevich A.L., Stavrov V.P. Optimization of the modes of obtaining profiles from reinforced thermoplastics. Materialy. Tekhnologii. Instrumenty, 2003, vol. 8, no. 4, pp. 75–79.
  35. Yakovlev Yu.Yu., Khasyanov R.Sh., Galiguzov A.A. et al. Peculiarities of melt flow characteristics of PERT-polyethylene filled with basalt and glass fibers. Plastichnyye massy, 2018, no. 9-10, pp. 49–51.
  36. Gaitukieva Z.Kh., Akhriev A.S., Kunizhev B.I., Tkhakakhov R.B. Dielectric constant and density of polymer composites based on synthetic isoprene rubber and polyethylene containing soot and aluminum nanoparticles. Plasticheskiye massy, 2018, no. 9-10, pp. 47–49.
  37. Zimin D.E. Reinforced with basalt fibers polymer composite material with increased heat and chemical resistance: thesis abstract, Cand. Sc. (Tech.). Biysk: IPKhTSO RAN, 2009, 24 p.
  38. Eurasian chemical market. New polymers: polyphenylene sulfide. International business journal, 2008, vol. 39, no. 3, pp. 14–21.
  39. Borodulin A.S., Kalinnikova A.N., Music S.S., Tereshkov A.G. Polyetherimides for the creation of heat-resistant polymer composite materials with high physical and mechanical properties. Vestnik Belgorodskogo gosudarstvennogo tekhnologicheskogo universiteta im. V.G. Shukhova, 2019, no. 11, pp. 94–100.
  40. Ryabev A.N., Donetskiy K.I., Shaposhnikova V.V. et al. Homo- and copolyarylene ether ketones with side hydroxyl groups. Vysokomolekulyarnye soyedineniya, series B, 2009, vol. 51, no. 2, pp. 315–321.
  41. Fedulov B.N., Safronov A.A., Kantor M.M., Lomov S.V. Modeling of curing of thermoplastic composites and estimation of residual stresses. Kompozity i nanostruktury, 2017, vol. 9, no. 2 (34), pp. 102–122.