Trends in the development of cast magnesium alloys with an increased ignition temperature (review)
UDC
669.018.28:669.721.5
DOI
10.18577/2307-6046-2021-0-2-3-9
Article PDF (Russian)
(687.76 KB)
How to cite
Leonov A.A., Trofimov N.V., Duyunova V.A., Uridiya Z.P. Trends in the development of cast magnesium alloys with an increased ignition temperature (review) // Proceedings of VIAM. 2021. No. 2. DOI: 10.18577/2307-6046-2021-0-2-3-9. URL: https://www.viam-works.ru/en/journal/2021/2/1
Keywords
overview, ignition temperature, fire resistance, thermal stability, magnesium alloys, alloying elements.
Abstract
Trends in the development of cast magnesium alloys with increased temperature, ignition and fire resistance are presented. The main world companies and institutions - developers of casting magnesium alloys are presented. The developed alloys are considered, indicating their chemical characteristics, mechanical characteristics at high and high temperatures and corrosion resistance, as well as the use of materials and design aspects of industry. The presented magnesium alloys with an increased ignition temperature allow expanding the scope of their use.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare earth elements – materials of modern and future high technologies. Trudy VIAM, 2013, no. 2, paper no. 01. Available at: http://www.viam-works.ru (accessed: September 30, 2020).
- Kablov E.N., Morozov G.A., Krutikov V.N., Muravskaya N.P. Certification of standard samples of structure of complex-alloyed alloys using standard. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 9–11.
- Kablov E.N. Aviation and Space Materials Science. Vse materialy. Enciklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
- Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metaliy Evrazii, 2012, no. 3, pp. 10–15.
- Trofimov N.V., Leonov A.A. Investigation of the influence of alloying elements (Nb and Ti) on the content of impurities and mechanical properties of a high-strength magnesium alloy of the Mg–Zn–Zr system. Metally, 2020, no. 3, pp. 14–18.
- Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
- Volkova E.F., Mostyaev I.V., Akinina M.V. Comparative analysis of mechanical properties anisotropy and microstructure of semi-finished products from high-strength magnesium alloys with REE. Trudy VIAM, 2018, no. 5 (65), paper no. 04. Available at: http://www.viam-works.ru (date of access: October 10, 2020). DOI: 10.18577/2307-6046-2018-0-5-24-33.
- Duyunova V.A., Leonov A.A., Trofimov N.V. Investigation of the influence of rare-earth elements and heat treatment on the structure and properties of heat-resistant casting magnesium alloy of the Mg–REM–Zr system. Metally, 2020, no. 5, pp. 58–63.
- Duyunova V.A., Leonov A.A., Molodtsov S.V. VIAM's contribution to the development of light alloys and the corrosion control of rocket and space technology products. Trudy VIAM, 2020, no. 2 (86), paper no. 03. Available at: http://www.viam-works.ru (date of access: October 30, 2020). DOI: 10.18577/2307-6046-2020-0-2-22-30.
- Casting magnesium alloy with rare earth metals: pat. RU 2617072 C2; filed 06.10.15; publ. 19.04.17.
- Alloy based on magnesium and method of its production: pat. RU 2218438 C2; filed 26.12.01; publ. 10.02.03.
- Alloy based on magnesium and method of its production: pat. RU 2215056 C2; filed 26.12.01; publ. 20.08.03.
- Casting magnesium alloy: pat. RU 2687359 C1; filed 23.11.18; publ. 13.05.19.
- Magnesium alloy containing heavy rare earths: pat. WO 2011117630 A1; filed 23.03.11; publ. 29.09.11.
- Castable magnesium alloys: pat. WO 2005035811 A8; filed 08.10.04; publ. 21.04.05.
- High temperature resistant magnesium alloys: pat. US 6767506; filed 14.03.02; publ. 27.06.04.
- Creep resistant magnesium alloy with improved ductility and fracture toughness for gravity casting applications: pat. US 20060020596 A1; filed 29.09.06; publ. 01.11.09.
- Mg–Gd–Y–Zr magnesium alloy and heat treatment method of large-scale complex casting prepared from the Mg–Gd–Y–Zr magnesium alloy: pat. CN103388095; filed 18.07.13; publ. 26.10.16.
- High-toughness heat-resistant Mg–Gd–Y alloy and preparation method thereof suitable for gravitational casting: pat. CN 201910251471; filed 29.03.19; publ. 25.06.19.
- High-toughness heat-resistant Mg–Er alloy and preparation method thereof suitable for low pressure casting: pat. CN 201910250338; filed 29.03.19; publ. 07.06.19.
- Aluminum-containing rare earth magnesium alloy and preparation method thereof: pat. CN 201910271180; filed 04.04.19; publ. 28.05.19.
- Wu X., Pan F.S., Cheng R.J., Luo S.Q. Mater Effect of morphology of long period stacking ordered phase on mechanical properties of Mg–10Gd–1Zn–0,5Zr magnesium alloy. Materials Science and Engineering, 2018, no. 5. Р. 64–68
- Wang D., Fu P.H., Peng L.M. et al. Development of high strength sand cast Mg–Gd–Zn alloy by co-precipitation of the prismatic β′ and β1 phases. Materials Characterization, 2019, vol. 153, no. 7, pp. 157–168.
- Wang J., Zhou H., Wang L. et al. Microstructure, mechanical properties and deformation mechanisms of an as-cast Mg–Zn–Y–Nd–Zr alloy for stent applications. Journal of Materials Science & Technology, 2019, vol. 35, is. 7, pp. 1211–1217.