Aspects of structure formation dispersion-strengthened metal composite material obtained on the basis of shavings and powder of aluminum corrosion-resistant alloy

Gololobov A.V., Nyafkin A.N., Zhabin A.N.
Gololobov A.V., Nyafkin A.N., Zhabin A.N. Aspects of structure formation dispersion-strengthened metal composite material obtained on the basis of shavings and powder of aluminum corrosion-resistant alloy // Proceedings of VIAM. 2021. No. 12. DOI: 10.18577/2307-6046-2021-0-12-39-46. URL: https://www.viam-works.ru/en/journal/2021/12/5
Keywords
metal composite material, aluminum alloy, silicon carbide, shavings, powder, mechanical alloying, extrusion, structure.
Abstract

A metal composite material (MCM) based on an aluminum corrosion-resistant alloy of the AMg6 brand, containing 22.5 % (vol.) Silicon carbide, obtained by mechanical alloying, has been investigated. Aspects of the formation of the MCM structure based on chips and powder from this alloy are considered. The influence of the initial components on the structure of the dispersion-strengthened MCM was investigated, and samples were made from this composite material.

Reference list
  1. Kablov E.N. Composites: today and tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. New generation materials and digital technologies of their processing. Vestnik Rossijskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  4. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  5. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  6. Alaneme K.K., Bodunrin M.O. Corrosion behavior of alumina reinforced aluminium (6063) metal matrix composites. Journal of Minerals and Materials Characterization and Engineering, 2011, vol. 10, no.12, pp.1153–1165.
  7. Singh J., Chauhan A. Characterization of hybrid aluminum matrix composites for advanced applications – a review. Journal of Materials Research and Technology, 2016, vol. 5, no.2, pp.159–169.
  8. Kosolapov D.V., Shavnev A.A., Nyafkin A.N., Grishina O.I. Research of forming of structure of composition granules of Al–SiC. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 49–52. DOI: 10.18577 / 2071-9140-2016-0-3-49-52.
  9. Kosolapov D.V., A.A. Shavnev, E.I. Kurbatki-na, A.N. Nyafkin, A.V. Gololobov. Study on structure and properties of dispersion hardened MMC based on aluminium alloy of Al–Mg–Si system. Trudy VIAM, 2020, no. 1, paper no. 06. Available at: http://www.viam-works.ru (accessed: June 14, 2021). DOI: 10.18577/2307-6046-2020-0-1-58-67.
  10. Miller W.S., Humphreys F.J. Strengthening mechanisms in particulate metal matrix composite. Scripta Metallurgica et Materialia, 1991, vol. 25, pp.33–38.
  11. Velidandla B., Radhakrishna B., Anjilivelil K. et al. P/M processing of Al–SiC composites. Journal of Powder Metallurgy, 1991, vol. 27, pp.227–235.
  12. Deaquino-Lara R., Gutierrez-Castaneda E., Estrada-Guel I. et al. Structural characterization of aluminium alloy 7075-graphite composites fabricated by mechanical alloying and hot extrusion. Materials and Design, 2014, vol. 53, pp. 1104–1111.
  13. Yuan W., Zhang J., Zhang C., Chen Z. Processing of ultrahigh strength SiCp/Al–Zn–Mg–Cu composites. Journal of Materials Processing Technology, 2009, vol. 209, pp.3251–3255.
  14. Verma R.K., Mahesh N.S., Anwar M.I. Numerical Analysis of Powder Compaction to Obtain High Relative Density in ʹ601ABʹ Aluminum Powder. SasTech journal, 2012, vol. 11, is. 1, pp.79–84.
  15. Veeresh Kumar G.B., Rao C.S.P., Selvaraj N., Bhagyashekar M.S. Studies on Al6061–SiC and Al7075–Al2O3 Metal Matrix Composites. Journal of Minerals & Materials Characterization & Engineering, 2010, vol. 9, no.1, pp. 43–55.