Adhesives as part of PCM based on organic fillers
Lukina N.F., Petrova A.P., Isaev A.Yu., Smirnov O.I. Adhesives as part of PCM based on organic fillers // Proceedings of VIAM. 2021. No. 12. DOI: 10.18577/2307-6046-2021-0-12-31-38. URL: https://www.viam-works.ru/en/journal/2021/12/4
Keywords
adhesives, adhesive binder, organoplastic, protective screen, aramid fibers, damping characteristics.
Abstract
The use of various adhesives and adhesive binders in the composition of organoplastics is shown, as well as the use of adhesives for gluing structural elements made of organoplastics in the composition of products. Examples of the use of VK-3 film adhesive as part of VKO-20 and VKO-2TB organoplastics, VK-36RT adhesive as part of VKO-19, VKO-19L organoplastics, VSK-14-2m adhesive binder as part of VKO-24 organoplastics are given. The results of the use of VK-41M adhesive in the composition of the Alor D16/41 aluminum organoplastic and the use of this material in the An-124 aircraft are presented.
Reference list
- Mashinskaya G.P. Organoplasty – results and problems. Aviation materials at the turn of the XX – XXI centuries. Moscow: VIAM, 1994, pp. 219–228.
- Mashinskaya G.P., Perov B.V., Shalin R.E. Multipurpose organoplastics for aviation technology. Aviation materials. Selected works of "VIAM" 1932-2002. Ed. E.N. Kablov. Moscow: VIAM, 2002, pp. 247–270.
- Zhelezina G.F. Features of the destruction of organoplastics under shock impacts. Aviation materials and technologies. Ed. E.N. Kablov. Moscow: VIAM, 2012, pp. 272–277.
- Gunyaev G.M., Zhelezina G.F., Zelenina I.V. et al. Corporate nano- and CALS-technologies in science-intensive industries. Proceedings of the 4th International. conf. "Theory and practice of technologies for the production of products from composite materials and new metal alloys". Moscow: Lomonosov Moscow State University, 2005, pp. 739–743.
- Mukhametov R.R., Akhmadieva K.R., Chursova L.V., Kogan D.I. New polymer binders for promising methods for the manufacture of structural fibrous PCM. Aviacionnye materialy i tehnologii, 2011, no. 2, pp. 38–42.
- Petrova A.P., Donskoy A.A., Chalykh A.E., Shcherbina A.A. Adhesive materials. Sealants. Saint Petersburg: Professional, 2008. 589 p.
- Petrova A.P., Malysheva G.V. Adhesives, adhesive binders and adhesive prepregs: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2017, 472 p.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. New generation materials. Zashchita i bezopasnost, 2014, no. 4, pp. 28–29.
- Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Kulagina G.S., Zhelezina G.F. Structural and ballistic resistant organoplastics based on film adhesives. All-Rus. scientific and technical conf. "Fundamental and applied research in the field of creating adhesives, adhesive binders and adhesive prepregs". Moscow: VIAM, 2018, pp. 31–42.
- Zhelezina G.F., Shuldeshova P.M. Structural organoplastics based on film adhesives. Klei. Germetiki. Tekhnologii, 2014, no. 2, pp. 9–14.
- Zhelezina G.F., Kulagina G.S., Shuldeshova P.M., Chernykh Т.E. Organoplastics based on heat-resistant polymer fibers and matrices. Trudy VIAM, 2021, no. 5 (99), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 16, 2021). DOI: 10.18577/2307-6046-2021-0-5-78-86.
- Zhelezina G.F., Tikhonov I.V., Chernykh T.E. and other Aramid fibers of the third generation Rusar-NT for the reinforcement of organotexolites for aviation purposes. Plasticheskie massy, 2019, no. 3-4, pp. 43–47.
- Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
- Zhelezina G.F., Voinov S.I., Solovyova N.A., Kulagina G.S. Aramid organotexolites for shock-resistant aircraft structures. Journal of Applied Chemistry, 2019, vol. 92. 3, pp. 358–364. DOI: 10.1134/S0044461819030101.
- Shuldeshova P.M., Deev I.S., Zhelezina G.F. Features of destruction of SVM aramide fibers and structural organoplastics on their basis. Trudy VIAM, 2016, no. 2 (38), paper no. 11. Available at: http://www.viam-works.ru (accessed: March 29, 2021). DOI 10.18577/2307-6046-2016-0-2-11-11.
- Zheleznyak V.G., Muhametov R.R., Chursova L.V. Study of possibility of thermoset binder creation for operating temperature up to 400°C. Aviacionnye materialy i tehnologii, 2013, no. S2, pp. 58–61.
- Zhelezina G.F., Gulyaev I.N., Soloveva N.A. Aramide organic plastics of new generation for aviation designs. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 368–378. DOI: 10.18577/2071-9140-2017-0-S-368-378.
- Kulagina G.S., Zhelezina G.F., Shuldeshova P.M. Organoplastics for aviation purposes, properties and applications. All-Rus. scientific and technical conf. "New generation polymer composite materials for civilian industries". Moscow: VIAM, 2020, pp. 55–62.
- Antipov V.V., Kotova E.V., Serebrennikova N.Yu., Petrova A.P. Glue binders and glue prepregs for alumopolymeric composite materials. Trudy VIAM, 2018, no. 5 (65), paper no. 06. Available at: http://www.viam-works.ru (accessed: July 22, 2021). DOI: 10.18577/2307-6046-2018-0-5-44-54.