Determination of sulfur, carbon, nitrogen and oxygen in copper based alloys
UDC
669.018.44:669.35
DOI
10.18577/2307-6046-2021-0-11-112-119
Article PDF (Russian)
(669.35 KB)
How to cite
Alekseev A.V., Pahomkina T.N., Lapshina Yu.V. Determination of sulfur, carbon, nitrogen and oxygen in copper based alloys // Proceedings of VIAM. 2021. No. 11. DOI: 10.18577/2307-6046-2021-0-11-112-119. URL: https://www.viam-works.ru/en/journal/2021/11/11
Keywords
superalloys, copper alloys, sulfur determination, carbon determination, nitrogen determination, oxygen determination, infrared absorption spectroscopy method.
Abstract
The determination of gas-forming impurities in samples of low-alloyed copper alloys of the Cu–Cr and Cu–Cr–Zr systems is carried out. The content of sulfur and carbon was determined by the method of combustion in an induction furnace of a gas analyzer with subsequent detection in the infrared cell of the spectrometer, and to determine oxygen and nitrogen, the method of reducing melting in a flow of an inert carrier gas was used, followed by the detection of oxygen in the infrared cell and nitrogen in the conductometric cell of the gas analyzer.
Reference list
- Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
- Trofimenko N.N., Efimochkin I.Yu., Bolshakova A.N. Problems of creation and prospects for the use of heat-resistant high-entropy alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 3–8. DOI: 10.18577/2071-9140-2018-0-2-3-8.
- Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
- Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. The application of new wrought nickel alloys for advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
- Ten E.B., Badmazhapov I.B. Fundamentals of development of multifunctional heat-resistant copper alloys. Metallurgiya mashinostroyeniya, 2009, no. 6, pp. 21–24.
- Lovshenko F.G., Lovshenko G.F., Lozikov I.A. Cast chromium-containing bronzes obtained with the use of mechanically alloyed ligatures. Litye i metallurgiya, 2012, no. 3, pp. 131–135.
- Busygin S.L., Dovzhenko N.N., Mozhaev A.V., Demchenko A.I., Bezrukikh A.A. Electrodes from copper alloy low-alloyed with nanostructured chromium particles for resistance spot welding. Innovatsii i investitsii, 2020, no. 5, pp. 174–178.
- Tebyakin A.V., Fokanov A.N., Podurazhnaya V.F. Multipurpose copper alloys. Trudy VIAM, 2016, no. 12, paper no. 05. Available at: http://www.viam-works.ru (accessed: June 8, 2021). DOI: 10.18557/2307-6046-2016-0-12-5-5.
- Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRM and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
- State Standard 13938.2–78. Copper. Methods for the determination of sulfur. Moscow: Publishing house of standards, 1978, pp. 2–5.
- State Standard 12344–2003. Alloyed and high-alloyed steels. Methods for the determination of carbon. Moscow: Publishing house of standards, 2003, pp. 4–5.
- State Standard 13938.13–93. Copper. Methods for the determination of oxygen. Moscow: Publishing house of standards, 1993, pp. 7–20.
- State Standard 12359–99. Carbon steels, alloyed and high-alloyed. Methods for the determination of nitrogen. Minsk: Publishing house of standards, 1999, p. 3.
- ASTME E1019-11. Standard Test Methods for Determination of Carbon, Sulfur, Nitrogen, and Oxygen in Steel, Iron, Nickel, and Cobalt Alloys by Various Combustion and Fusion Techniques. ASTM International. United States, 2011, p. 24.
- Alekseev A.V., Rastegaeva G.Yu., Pakhomkina T.N., Razmakhov M.G. Determination sulfur, carbon, nitrogen and oxygen in alloys of system Co–Fe–Co–B and Gd–Fe–Co–B. Trudy VIAM, 2019, No. 8 (80), paper no. 10. Available at: http://www.viam-works.ru (accessed: July 12, 2021). DOI: 10.18557/2307-6046-2019-0-8-90-97.