Study of the tribotechnical characteristics of corrosion-resistant steels with different mechanisms of volumetric hardening

Sevalnev G.S., Sevalneva T.G., Kolmakov A.G., Dulnev K.V., Krylov S.А.
Sevalnev G.S., Sevalneva T.G., Kolmakov A.G., Dulnev K.V., Krylov S.А. Study of the tribotechnical characteristics of corrosion-resistant steels with different mechanisms of volumetric hardening // Proceedings of VIAM. 2021. No. 10. DOI: 10.18577/2307-6046-2021-0-10-3-11. URL: https://www.viam-works.ru/en/journal/2021/10/1
Keywords
friction, wear, tribology, martensite, hardness, frictional interaction.
Abstract

The structure, phase composition and hardness of corrosion-resistant steels with different mechanisms of volumetric hardening was studied. It was found that after hardening treatment of steel VNS9-Sh, VNS30-Sh, VNS72-Sh have approximately the same hardness with a volumetric martensite content of 50, 90 and 75 %, respectively. According to the results of tribological tests for wear under dry friction conditions, it was found that VNS9-Sh steel with the TRIP effect has the best wear resistance. VNS30-Sh steel with precipitation hardening and VNS72-Sh steel with martensite hardening have approximately the same wear resistance.

Reference list
  1. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  2. Tonysheva O.A., Voznesenskaya N.M., Shestakov I.I., Eliseyev E.A. Influence of modes of high-temperature thermomechanical processing on structure and properties of high-strength corrosion-resistant steel of austenitic-martensitic class 17Х13Н4К6САМ3ч. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 11–16. DOI: 10.18577/2307-6046-2017-0-1-11-16.
  3. Shi F., Tian P.C., Jia N. et al. Improving intergranular corrosion resistance in a nickel-free and manganese-bearing high-nitrogen austenitic stainless steel through grain boundary character distribution optimization. Corrosion Science, 2016, Vol. 107, PP. 49–59.
  4. Voznesenskaya N.M., Tonusheva O.A., Leonov A.V., Dulnev K.V. Hydrogen influence on high-strength corrosion-resistant steel VNS65-Sh properties and ways of elimination of hydrogen embrittlement. Trudy VIAM, 2018, no. 10 (70), paper no. 01. Available at: http://www.viam-works.ru (accessed: June 1, 2019). DOI: 10.18577/2307-6046-2018-0-10-3-9.
  5. Bannykh O., Blinov V., Lukin E. High-strength economically alloyed corrosion-resistant steels with the structure of nitrogen martensite. IOP Conference Series: Materials Science and Engineering, 2016, vol. 130, no. 1, pp. 012001.
  6. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  7. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellect and technology, 2016, no. 2 (14), pp. 16–21.
  8. Romanenko D.N., Sevalnev G.S., Leonov A.A., Udod K.A., Stepanenko E.V. Improving the tribological characteristics of 18KHGT steel after cementation and hardening heat treatment. Aviation materials and technology, 2021. no. 1 (62). paper no. 02. Available at: https://journal.viam.ru (accessed: May 20, 2021). DOI: 10.18577/2713-0193-2021-0-1-13-21.
  9. Sevalnev G.S., Tsukanov D.V., Zubkov N.N. et al. Improvement of Austenitic Steel Tribological Properties by Deformational Cutting. Metallurgist, 2021, vol. 65, pp. 169–176. DOI: 10.1007/s11015-021-01145-6.
  10. Kolmykov V.I., Romanenko D.N., Abyshev K.I., Bedin V.V. Efficiency of surface hardening by carburizing steel objects operating under abrasive wear conditions. Chemical and Petroleum Engineering, 2015, vol. 51, no. 1–2, pp. 58–61.
  11. Gerasimov S.A., Kuksenova L.I., Lapteva V.G., Ospennikova O.G., Alekseeva M.S., Gromov V.I. Surface engineering and operational properties of nitrided structural steels: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2019, 600 p.
  12. Terent’ev V.F., Ashmarin A.A., Blinova E.N. et al. Mechanical properties and structure of a VNS9-Sh steel as functions of the tempering temperature. Russian metallurgy (Metally), 2019, vol. 2019, no. 4, pp. 403–408.
  13. Betzofen S.Ya., Ashmarin A.A., Terentyev V.F. et al. Phase composition and residual stresses in surface layers of trip-steel VNS9-Sh. Deformatsiya i razrushenie materialov, 2020, no. 6, pp. 12–20.
  14. Zhegina I.P., Lutsenko A.N., Muboyadzhyan S.A., Belous V.Ya., Kotelnikova L.V. The nature of destruction of steel EP866-Sh with coatings. Voprosy materialovedeniya, 2009, no. 4, pp. 150–156.
  15. Tonysheva O.A. Features of the formation of structure and properties during smelting, heat treatment and plastic deformation of corrosion-resistant welded chromium-nickel steels alloyed with nitrogen: thesis, Cand. Sc. (Tech.). Moscow, 2014, 138 p.
  16. Materials science: textbook. Ed. B.N. Arzamasov, G.G. Mukhina. Moscow, 2001, 648 p.