Influence of additional sizing of carbon fiber in producing volume-reinforced preforms on the properties of high-temperature carbon fiber

Nacharkina A.V., Zelenina I.V., Valueva M.I., Voronina O.G.
Nacharkina A.V., Zelenina I.V., Valueva M.I., Voronina O.G. Influence of additional sizing of carbon fiber in producing volume-reinforced preforms on the properties of high-temperature carbon fiber // Proceedings of VIAM. 2021. No. 1. DOI: 10.18577/2307-6046-2021-0-1-54-65. URL: https://www.viam-works.ru/en/journal/2021/1/6
Keywords
carbon fiber, bulk-reinforced perform, sizing, removal of sizing, high-temperature carbon plastic, physic-mechanical properties.
Abstract

Presents the results of experimental studies of the effect of additional apparet on the properties of high-temperature carbon plastic based on a heat-resistant thermosetting phthalonitrile binder and a volume-reinforced woven preform. Comparative data are given on physical and mechanical properties of carbon plastics based on preforms with and without an apparet, including after exposure to operational factors (thermal aging, water and moisture absorption), results of thermal analysis and microstructure research.

Reference list
  1. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  2. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  3. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  4. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  5. Boychuk A.S., Generalov A.S., Dikov I.A. FRP parts and structures testing by phased array technique. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 45–50. DOI: 10.18577/2071-9140-2017-0-1-45-50.
  6. Oreshko E.I., Erasov V.S., Lutsenko A.N. Mathematical modeling of deformation constructional carbon fiber at a bend. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 50–59. DOI: 10.18577/2071-9140-2016-2-50-59.
  7. Antyufeeva N.V., Aleksashin V.M., Pavlov M.R., Stolyankov Yu.V. Research of possibility of use carbon fiber reinforced polymers in the conditions of the Arctic climate. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 86–94. DOI: 10.18577/2071-9140-2016-0-4-86-94.
  8. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  9. Kablov E.N., Skibin V.A., Abuzin Yu.A., Kochetov V.N., Shavnev A.A., Karimbaev T.D., Luppov A.A. Wide-chord fan blades for turbofan engines of 5–6 generations. Konversiya v mashinostroyenii, 2006, no. 5, pp. 5–16.
  10. Karimbaev T.D., Luppov A.A., Afanasiev D.V. Fan blades for advanced engines. Dvigatel, 2011, no. 6, pp. 2–10.
  11. Mekham M. Snecma and her partner AEC create a new technology for the manufacture of composite blades. Aviatransportnoe obozreniye, 2012, no. 131. Available at: http://www.ato.ru/content/snecma-i-ee-partner-aec-sozdayut-novuyu-tehnologiyu-izgotovleniya-kompozitnyh-lopatok (accessed: November 06, 2020).
  12. Novikov A.S., Karimbaev T.D., Luppov A.A. and other Innovations in the use of composite materials in aircraft engines. Dvigatel, 2015, no. 2 (98), pp. 6–9.
  13. Novikov A.S., Karimbaev T.D. Rotor blades of large bypass fans for advanced turbojet engines. Dvigatel, 2015, no. 5 (101), pp. 6–11.
  14. Zelenina I.V., Gulyayev I.N., Kucherovskiy A.I., Mukhametov R.R. Heat-resistant CFRP for the impulse wheel of the centrifugal compressor. Trudy VIAM, 2016, no. 2 (38), paper no. 08. Available at: http://www.viam-works.ru (accessed: November 06, 2020). DOI: 10.18577/2307-6046-2016-0-2-8-8.
  15. Evdokimov A.A., Gulyaev I.N., Zelenina I.V. Investigation of the physicomechanical properties and microstructure of volume-reinforced carbon fiber reinforced plastic. Trudy VIAM, 2019, no. 4 (76), paper no. 05. Available at: http://viam-works.ru (accessed: November 06, 2020). DOI: 10.18577/2307-6046-2019-0-4-38-47.
  16. Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577 / 2071-9140-2019-0-4-18-26.
  17. Woven preforms having a given shape with multidirectional reinforcement for composite structures: pat. 2504478 Rus. Federation, no. 2010134758/05; filed 09.02.09; publ. 20.01.14.
  18. Soutis C. Fiber reinforced composites in aircraft construction. Progress in Aerospace Sciences, 2005, no. 41 (2), pp. 143–151.
  19. Hufenbach W., Bohm R., Thieme M. et al. Polypropylene/glass fiber 3D-textile reinforced composites for automotive applications. Materials and Design, 2011, no. 32 (3), pp. 1468–1476.
  20. Bogomolov P.I., Kozlov I.A., Birulya M.A. Review of modern technologies for the manufacture of volume-reinforcing preforms for advanced composite materials. Tekhniko-tekhnologicheskiye problemy servisa, 2017, no. 1, pp. 22–27.
  21. Behera B.K., Mishra R. 3-Dimensional weaving. Indian Journal of Fiber and Textile Research, 2008, no. 33 (3), pp. 274–287.
  22. Sergeev V.T. Development of the structure and manufacturing technology of a multilayer combined fabric from carbon and quartz threads: thesis abstract, Cand. Sc. (Tech.). Moscow: Moscow State University of Design and Technology, 2014, 16 p.
  23. Donetskij K.I., Hrulkov A.V., Kogan D.I., Belinis P.G., Lukyanenko Yu.V. Use of three-dimensional reinforcing preforms during the production of polymer composite products. Aviacionnye materialy i tehnologii, 2013, no. 1, pp. 35–39.
  24. Baklanova N.I. Interface coatings on reinforcing carbon and silicon carbide fibers for composites with a ceramic matrix: thesis, Dr. Sc. (Chem.). Novosibirsk: Institute of Solid State Chemistry and Mechanochemistry SB RAS, 2010, 380 p.
  25. Baklanova N.I., Zima T.M., Titov A.T., Isaeva N.V., Grashchenkov D.V., Solntsev S.S. Protective coatings for carbon fibers. Neorganicheskiye materialy, 2006, vol. 42, no. 7, pp. 823–829.
  26. Urvanov S.A. Modification of carbon fiber with carbon nanostructures: thesis, Cand. Sc. (Chem.). Moscow: TISNUM, 2016, 155 p.
  27. Valueva M.I., Zelenina I.V., Khaskov M.A., Gulyaev A.I. Preparation of carbon fibers to interphase coating deposition for ceramic matrix composites. Trudy VIAM, 2017, no. 10 (58), paper no. 09. Available at: http://www.viam-works.ru (accessed: November 06, 2020). DOI: 10.185577/2307-6046-2017-0-10-9-9.
  28. Petrova G.N., Bejder E.Ya. Development and research of finishing compositions for thermoplastic carbon plastics. Trudy VIAM, 2016, no. 12 (46), paper no. 09. Available at: http://www.viam-works.ru (accessed: November 06, 2020). DOI: 10.18577/2307-6046-2016-0-12-9-9.
  29. Beev A.A., Khashirova S.Yu., Slonov A.L. et al. Activation of the surface of carbon and glass fibers. New polymer composite materials: collection of articles. scientific. tr. XV Int. scientific-practical conf. (Nalchik, July 3–7, 2019). Nalchik, 2019, pp. 71–75.
  30. A method of obtaining finished carbon fibers and composite materials based on them: pat. 2712612 Rus. Federation, no. 2019115024; filed 16.05.19; publ. 29.01.20.
  31. Kondrashova I.A., Cheblakova E.G., Evteeva E.E. Carbon fiber processing for further operation in technological processes. Evraziyskiy soyuz uchenykh, 2015, no. 3 (12), pp. 36–38.
  32. Khaskov M.A., Zelenina I.V., Sorokin O.Yu., Gulyaev A.I. Ceramic interphase coating on carbon fibers based on polycarbosilane and oligovinylsilazane. Fizika i khimiya stekla, 2019, vol. 44, no. 2, pp. 1–9.
  33. Evdokimov A.A., Gulyaev I.N., Nacharkina A.V. Investigation of the physicomechanical properties of volume-reinforced carbon fiber reinforced plastic. Trudy VIAM, 2020, no. 3 (87), paper no. 07. Available at: http://www.viam-works.ru (accessed: November 06, 2020). DOI: 10.18577/2307-6046-2020-0-3-66-73.
  34. Perepelkin K.E. Reinforcing fibers and fibrous polymer composites. Saint Petesburg: Scientific bases and technologies, 2009, 380 p.
  35. Rashkovan I.A. The influence of surface modification on the properties of carbon fibers and the realization of their strength in unidirectional polymer composites: thesis abstract, Cand. Sc. (Tech.). Mytishchi: All-Russian Research Institute of Polymer Fibers, 1993, 14 p.
  36. Gulyaev I.N., Zelenina I.V., Valevin E.O., Shvedkova A.K. Investigation of the influence of increased temperature and humidity on the properties of heat-resistant carbon plastics. Konstruktsii iz kompozitsionnykh materialov, 2015, no. 3, pp. 55–60.