Corrosion resistance of the brazed joints of the GTE fuel manifolds, made with various brazing alloys

Sviridov A.V., Afanasiev-Khodykin A.N., Galushka I.A.
Sviridov A.V., Afanasiev-Khodykin A.N., Galushka I.A. Corrosion resistance of the brazed joints of the GTE fuel manifolds, made with various brazing alloys // Proceedings of VIAM. 2021. No. 1. DOI: 10.18577/2307-6046-2021-0-1-23-33. URL: https://www.viam-works.ru/en/journal/2021/1/3
Keywords
fuel manifold, gas turbine engine, corrosion-resistant steel, brazed joint, brazing alloy, corrosion resistance.
Abstract

Presents the results of work on assessing the corrosion resistance of brazed joints of corrosion-resistant steels used in the manufacture of fuel manifolds for gas turbine engines in a salt spray chamber. The main types of corrosion damage of brazed joints made with brazing alloys of various types (based on copper and nickel) have been identified. The influence of the type of brazing alloy and the grade of the brazed materials on the nature of corrosion damage to brazed joints is determined. Based on the research results, assumptions have been made about the mechanism of occurrence and development of corrosion damage in brazed joints of various materials.

Reference list
  1. Kablov E.N., Startsev O.V., Medvedev I.M., Panin S.V. Corrosive aggressiveness of the seaside atmosphere. Part 1. Factors of influence (review). Korroziya: materialy, zashchita, 2013, no. 12, pp. 6–18.
  2. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  3. Kablov E.N., Startsev O.V., Medvedev I.M. Corrosive aggressiveness of the seaside atmosphere. Part 2. New approaches to assessing the corrosiveness of coastal atmospheres. Korroziya: materialy, zashchita, 2016, no. 1, pp. 1–15.
  4. Vetrova E.Yu., Shchekin V.K., Kurs M.G. Comparative evaluation of methods for the determination of corrosion aggressivity of the atmosphere. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 74–81. DOI: 10.18577/2071-9140-2019-0-1-74-81.
  5. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  6. Ospennikova O.G. Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings Aviacionnye materialy i tehnologii, 2012, no. S, pp. 19–36.
  7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Rylnikov V.S., Lukin V.I. Solders used for soldering materials aviation applications. Trudy VIAM, 2013, no. 8, paper no. 02. Available at: http://viam-works.ru (accessed: October 21, 2020).
  9. Aminazad A. M., Hadian A., Ghasimakbari F. Investigation on Corrosion Behavior of Copper Brazed Joints. Prosedia Materials Science, 2015, vol. 11, pp. 672–678. DOI: 10.1016/j.mspro.2015.11.024.
  10. Rylnikov V.S., Afanasev-Hodykin A.N., Krasikov M.I. Research of repair technology of defects correction of soldered joints of fuel collector. Trudy VIAM, no. 12, paper no. 02. Available at: http://www.viam-works.ru (accessed: October 21, 2020).
  11. Klapper H.S., Zadorozne N.S., Rebak R.B Localiazed Corrosion Characteristica of Nickel Alloys. Acta Metallurgica et Materialia, 2017, vol. 30, pp. 296–305. DOI: 10.1007/s40195-017-0553-z.
  12. Lukin V.I., Rilnikov V.S., Starova L.L., Ioda E.N., Kovalchuk V.G., Golev E.V. Welding and soldering in aircraft construction. Aviation materials. 75 years old. Selected Works. Moscow: VIAM, 2007, pp. 132–141.
  13. Ospennikova O.G., Lukin V.I., Afanasyev-Khodykin A.N., Galushka I.A., Shevchenko O.V. Advanced developments in the field of the high-temperature soldering of heat resisting alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 144–158. DOI: 10.18577/2071-9140-2017-0-S-144-158.
  14. Zhilikov V.P., Rilnikov V.S. Corrosion features of soldered joints. Korroziya: materialy, zashchita, 2012, no. 7, pp. 7–9.
  15. Lukin V.I., Rilnikov V.S., Afanasyev-Khodykin A.N. Nickel-based brazing alloys for brazing heat-resistant alloys and steels. Svarochnoye proizvodstvo, 2014, no. 7, pp. 36–42.
  16. Chulkov E.I., Ivanov M.A., Belova E.A., Afanasyev-Khodykin A.N., Rilnikov V.S. High-temperature brazing of pipelines from steel 12X18H10T in a protective atmosphere using local induction heating. Novosti materialovedeniya. Nauka i tekhnika, 2014, no. 5, paper no. 10. Available at: http://www.materialsnews.ru (accessed: October 21, 2020).
  17. Rilnikov V.S., Lukin V.I. New developments of solders for brazing nickel alloys and steels. Soldering in mechanical engineering: abstracts. Togliatti: TPI, 1991, pp. 51–52.
  18. Kurs M.G., Kutyrev A.E., Kirichok P.F., Fomina M.A. Accelerated and cyclic corrosion tests of aviation materials. Trudy VIAM, 2019, no. 10 (82), paper no. 06. Available at: http://www.viam-works.ru (accessed: October 21, 2020). DOI: 10.18577/2307-6046-2019-0-10-61-75.
  19. Varchenko E.A., Kurs M.G. Natural tests of metal materials in sea water: key approaches to estimation of resistance to corrosion and biodeterioration. Trudy VIAM, 2017, no. 11 (59), paper no. 12. Available at: http://www.viam-works.ru (accessed: October 21, 2020). DOI: 10.18577/2307-6046-2017-0-11-12-12.
  20. Kurs M.G., Nikolayev E.V., Abramov D.V. Full-scale and accelerated tests of metallic and nonmetallic materials: key factors and specialized stands. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 66–73. DOI: 10.18577/2071-9140-2019-0-1-66-73.