Mastering chromium-based ligatures in smelting heat-resistant nickel alloys and steels

Krylov S.А., Egorov E.V., Makarov А.А., Druzhnov M.A.
Krylov S.А., Egorov E.V., Makarov А.А., Druzhnov M.A. Mastering chromium-based ligatures in smelting heat-resistant nickel alloys and steels // Proceedings of VIAM. 2021. No. 1. DOI: 10.18577/2307-6046-2021-0-1-13-22. URL: https://www.viam-works.ru/en/journal/2021/1/2
Keywords
metallurgy, chromium, alumothermy, ligatures, degassing, vacuum induction smelting, open arc smelting, vacuum arc remelting, mechanical properties, metallography.
Abstract

The rapid rise in prices for charge materials used for smelting heat-resistant nickel alloy and steels leads to a significant rise in the cost of the final product. In order to curb the rise in prices for semi-finished products FSUE «VIAM» together with metallurgical plants of the industry, is carrying out work on testing and introducing new types of charge materials that can replace the currently used high-frequency materials.

The article discussed the materials tested instead of those currently used in the smelting of steels and alloys containing chromium, tungsten and molybdenum, produced at domestic enterprises from domestic raw materials.

Reference list
  1. Kablov E.N. Innovative development is the most important priority of the state. Metally Evrazii, 2010, no. 2, pp. 6–11.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N., Lomberg B.S., Ospennikova O.G. Creation of modern heat-resistant materials and technologies for their production for aircraft engine building. Krylya Rodiny, 2012, no. 3–4, pp. 34–38.
  4. Sidorov V.V., Rigin V.E., Goryunov A.V., Kablov D.Ye. Highly efficient technologies and modern equipment for the production of charge blanks from cast heat-resistant alloys. Metallurg, 2012, no. 5, pp. 26–30.
  5. Zachery C.L. A computational investigation of the effect of alloying elements on the thermodyna- mic and diffusion properties of FCC Ni alloys with application on the creep rate of delute Ni-X alloys: PhD Degree. Pennsylvania University, 2012, pp. 163–165.
  6. Volkov A.M., Karashaev M.M., Bakradze M.M., Pustynnikov T.O. Alternative technologies of the incresing of mechanical properties of p/m Ni-based superalloys for jet-engine disk application (review). Trudy VIAM, 2019, No. 8 (80), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 22, 2020). DOI: 10.18577/2307-6046-2019-0-8-3-8.
  7. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Development trends of nickel-based intermetallic alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  8. Krylov S.A., Shcherbakov A.I., Makarov A.A., Tonysheva O.A. Reduction of non-metallic inclusions in the nitrogen-containing corrosion-resistant steels. Trudy VIAM, 2017, no. 5 (53), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 24, 2020). DOI: 10.18577/2307-6046-2017-0-5-1-1.
  9. Lutsenko A.N., Slavin A.V., Erasov V.S., Khvackij K.K. Strength tests and researches of aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 527–546. DOI: 10.18577/2071-9140-2017-0-S-527-546.
  10. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nickel foundry heat resisting alloys of new generation. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 36–52.
  11. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. High-temperature heat resisting nickel alloys for details of gas turbine engines. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 52–57.
  12. Jeandin M., Bienvenu Y., Kounty J.L. Liquid phase sintering of nickel base superalloys. Superalloys, 1984, no. 87, pp. 467–476.
  13. Oryshchenko A.S. Heat-resistant high-temperature alloys. Saint Petersburg: Nauka, 2011.189 p.
  14. Novik F.S. Mathematical methods for planning experiments in metal science: textbook in 2 parts. Moscow: MISIS, 1979, part 2, 67 p.
  15. Choren J.A., Heinrich S.M., Silver-Thorn M.B. Young’s modulus and volume porosity relationships for additive manufacturing applications. Journal of Materials Scienсe, 2013, vol. 48, pp. 5103–5112.