Prospects for the use of radio-absorbing materials to ensure electromagnetic compatibility of avionics

Devin K.L., Agafonova A.S., Sokolov I.I.
Devin K.L., Agafonova A.S., Sokolov I.I. Prospects for the use of radio-absorbing materials to ensure electromagnetic compatibility of avionics // Proceedings of VIAM. 2020. No. 8. DOI: 10.18577/2307-6046-2020-0-8-94-100. URL: https://www.viam-works.ru/en/journal/2020/8/9
Keywords
radar absorbing material, avionics, electromagnetic compatibility, fiberglass, polymer composite material, radar absorbing coating.
Abstract

The article is devoted to issues in the field of creation of radar absorbing materials (RAM) in order to solve the problem of electromagnetic compatibility (EMC) in modern aircrafts. The characteristics of a number of RAM developed at FSUE «VIAM» are provided that are designed to ensure coordination and operability of aircraft antenna systems and to provide EMC for on-board radio-electronic equipment in the microwave range. The materials presented in the work differ in their overall dimensions, operating frequency range, method of attachment (application/installation) and have different purposes for use on aircrafts.

Reference list
  1. Paramonov P.P., Zharinov I.O. Integrated on-board computing systems: an overview of the current state and analysis of development prospects in aviation instrumentation. Nauchno-tekhnicheskiy vestnik informatsionnykh tekhnologiy, mekhaniki i optiki, 2013, no. 2 (84), pp. 1–17.
  2. Klyagin V.A., Petrova I.A., Shkurin M.V. Analysis of the placement of airborne radio-electronic equipment units on airplanes of various types. Trudy MAI, 2017, no. 95. Available at: http://www.trudymai.ru/published.php?ID=84442 (accessed: November 01, 2019).
  3. Koptev A.N. Aviation and radio-electronic equipment of civil aviation aircraft. Samara: SSAU Publishing House, 2011, 196 p.
  4. Bespalova E.E., Belyaev A.A., Shirokov V.V. Radar-absorbing materials for protection against high power microwave radiation. Trudy VIAM, 2015, no. 3, paper no. 07. Available at: http://www.viam-works.ru (accessed: November 1, 2019). DOI: 10.18577/2307-6046-2015-0-3-7-7.
  5. Romanov A.M., Belyaev A.A., Shirokov V.V. Peculiar features of optimization of resonant radar-absorbing materials of nonmagnetic type. Trudy VIAM, 2014, no. 11, paper no. 05. Available at: http://www.viam-works.ru (accessed: November 1, 2019). DOI: 10.18577/2307-6046-2014-0-11-5-5.
  6. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy, ser.: Chemistry and Chemical Technology, 2016, vol. 59, no. 10, pp. 61–71.
  7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovation. Krylya rodiny, 2016, no. 5, pp. 8-18.
  9. Bogush V.A., Borbotko T.V., Gusinsky A.V. et al. Electromagnetic radiation. Methods and means of protection. Minsk: Bestprint, 2003.401 p.
  10. Mikhailin Yu.A. Special polymer materials. Saint Petersburg: Nauchnye osnovy i tekhnologii, 2008, 660 p.
  11. Alekseev A.G., Shtager E.A., Kozyrev S.V. Physical foundations of stealth technology. Saint Petersburg: VVM, 2007, 284 p.
  12. Kovneristy Yu.K., Lazarev I.Yu., Ravaeva A.A. Materials that absorb microwave radiation. Moscow: Nauka, 1982, 162 p.
  13. Kazantseva N.E., Ryvkina N.G., Chmutin I.A. Promising materials for absorbers of microwave electromagnetic waves. Radiotekhnika i elektronika, 2003, vol. 48, no. 2, pp. 196–209.
  14. Simamura S., Shindo A., Kotsuka K. et al. Carbon fibers. Moscow: Mir, 1987, 304 p.
  15. Fitzer E. Carbon fibers and carbon composites. Moscow: Mir, 1988, 336 p.
  16. Devin K.L., Bortsov A.N., Devin E.A. Gradient absorber of electromagnetic waves. Perspektivnyye materialy, 2018, no. 9, pp. 79–84.
  17. Bespalova E.E., Belyaev A.A., Romanov A.M., Shirokov V.V. Investigation of the dielectric characteristics of designed for anechoic chambers laminated radar absorbing material layers based with carbonized fiber filled foam asbestos. Trudy VIAM, 201, no. 8, paper no. 12. Available at: http://www.viam-works.ru (accessed: November 1, 2019). DOI: 10.18577/2307-6046-2014-0-8-12-12.
  18. Agafonova A.S., Belyaev A.A., Kondrashov E.K., Romanov A.M. Features of the formation of monolithic structural radio absorbing materials based on composites filled with resistive fibers. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 56–59.
  19. Berkhovskikh L.M. Waves in layered media. Moscow: Nauka, 1973, 343 p.