Porous ceramic for filtration of metal melts and hot gases (review)

Babashov V.G., Varrik N.M., Karaseva T.A.
Babashov V.G., Varrik N.M., Karaseva T.A. Porous ceramic for filtration of metal melts and hot gases (review) // Proceedings of VIAM. 2020. No. 8. DOI: 10.18577/2307-6046-2020-0-8-54-63. URL: https://www.viam-works.ru/en/journal/2020/8/6
Keywords
porous ceramics, ceramic filters, metal melts filtration, refractory oxides, duplication of polymer matrix, alumina.
Abstract

Provides an overview of the highly porous ceramic materials currently used for filtration of metal melts and hot gases, filter manufacturers and methods for their production. Gas permeability and high specific surface area in combination with refractory properties allow using of highly porous oxides in processes carried out at high temperatures in chemical media when other materials are not applicable. Ways of improving the operational properties of porous ceramic filters, such as operating temperature, strength, oxidative resistance, bimodal porosity, as well as possibilities of improving the technological process of their production: reduced cost, increased environmental safety of production, reduced time of the technological cycle wereconsidered.

Reference list
  1. Kablov E.N. The key problem is materials. Trends and guidelines for innovative development in Russia. Moscow: VIAM, 2015, p. 458–464.
  2. Antsiferov V.N., Beklemyshev A.M., Gilev V.G. et al. Problems of powder materials science. Part II. Highly porous permeable materials. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2002, 262 p.
  3. Ivanchenkova L.G. Classification of filters for metal refining. Ogneupory, 1991, no. 2, pp. 28–29.
  4. Catalog of products of LLC «SpheroLit». Available at: https://sferolit.ru (accessed: July 20, 2020).
  5. Method of manufacturing a ceramic foam filter from titanium carbide: pat. 2280536 Rus. Federation; filed 27.12.04; publ. 27.07.06.
  6. Ceramic mass and method of making porous products from it: pat. 2047582 Rus. Federation; filed 17.07.92; publ. 10.11.95.
  7. FineWay Ceramics (Canada). Available at: http://finewayceramics.com (accessed: July 20, 2020).
  8. Ceramic mass for the manufacture of filter products: certificate of authorship 1323551 USSR; filed 19.11.85; publ. 15.07.87.
  9. A method of manufacturing a ceramic composite material: pat. 2355665 Rus. Federation; filed 25.07.07; publ. 20.05.08.
  10. Mukanova A.Zh., Kanygina ON. The problem of creating a pore space in siliceous ceramics for environmentally friendly filters. Vektor nauki TGU, 2013, no. 3, pp. 77–79.
  11. A method of manufacturing highly porous cellular ceramic products: pat. 2377224 Rus. Federation; filed 14.04.08; publ. 27.12.09.
  12. Method of manufacturing highly porous cellular ceramic materials: pat. 2580959 Rus. Federation; filed 08.04.15; publ. 10.04.16.
  13. Method for producing porous ceramics with bimodal distribution of porosity: pat. 2691207 Rus. Federation; filed 26.12.17; publ. 11.06.19.
  14. Talsicukur Z., Balaban C., Kuskonmaz N. Production of ceramic foam filters for molten metal filtration using expanded polystyrene. Journal of the European Ceramic Society, 2007, vol. 27, p. 637–640.
  15. Method of manufacturing lightweight ceramic products: certificate of authorship 1323554 USSR; filed 119.11.85; publ. 15.07.87.
  16. Gonzenback U.T., Studart A.R., Steinlin D., Tervoot E., Gauckler J.L. Processing of particle-stabilized wet foams into porous ceramics. Journal of the American Ceramic Society. 2007, vol. 90, no. 11, pp. 3407–3414.
  17. Salomao R., Villas Boas M.O.C., Pandolfelli V.C. Porous alumina-spinel ceramics for high temperature applications. Ceramics International, 2011, vol. 37, pp. 1393–1399.
  18. A method of obtaining a porous structure of a ceramic material: pat. 2483043 Rus. Federation; filed 12.05.11; publ. 20.11.12.
  19. Zo E Mo U. Porous and highly porous ceramics from aluminum oxide and silicon carbide: thesis, Dr. Sc. (Tech.). Moscow: D. Mendeleev University of Chemical Technology of Russia, 2019, 35 p.
  20. Guo X., Nakanishi K., Kanamori K. et al. Preparation of macroporous cordierite monoliths via the sol–gel process accompanied by phase separation. Journal of the European Ceramic Society, 2014, vol. 34, pp. 817–823.
  21. Ceramic Foam Filter: pat. 3947363 US; filed 28.03.75; publ. 30.03.76.
  22. Method of Preparation of Ceramic Foam: pat. 4075303 US; filed 22.02.77; publ. 21.02.78.
  23. Molten Metal Filter: pat. 4265659 US; filed 09.10.79; publ.05.05.81.
  24. Molten Metal Filter: pat. 4342664 US; filed 23.05.80; publ. 03.08.82.
  25. Process of Preparing a Ceramic Foam: pat. 4610832 US; filed 26.09.84; publ. 09.09.86.
  26. Porous Ceramic Filter Body and Manufacturing Method Thereof: pat. 4678758 US; filed 27.01.84; publ. 07.07.87.
  27. Ceramic Foam: pat. 4803025 US; filed 23.04.84; publ. 07.02.89.
  28. Method and Apparatus for Removing Liquid Salts From Liquid Metal: pat. 6036743 USA; filed 27.10.97; publ. 14.03.00.
  29. Dual Stage Ceramic Foam Filtration System and Method: pat. EP863217; filed 03.03.97; publ. 09.09.98.
  30. Ceramic Foam Filter Having a Protective Sleeve: pat. 5456833 US; filed 02.05.94; publ. 10.10.95.
  31. Die folgenden Angaben sind den vom Anmelder eingereichten Unterlagen entnommen: pat. 20318773U1 DE; filed 01.12.03; publ. 12.05.05.
  32. Ceramic Material Permitting the Passage of Fluids and Based on Silicon Powder Reaction-banded in the Presence of Carbon: pat. 5093289 US; filed 14.02.89; publ. 03.03.92.
  33. Ceramic Foam Filters: pat. 5190897 US; filed 20.09.91; publ. 02.03.93.
  34. Low Expansion Corrosion Resistant Ceramic Foam Filters for Molten Aluminum Filtration: pat. 8518528 US; filed 02.04.07; publ. 27.08.13.
  35. Process for the Production of Porous Ceramic Molded Articles: pat. 4472331 US; filed 22.02.83; publ. 18.09.84.
  36. Manufacturing Method of a Ceramics Body Having Through Holes: pat. 4664858 US; filed 13.08.85; publ. 12.05.87.
  37. High-Temperature Ceramic Filter: pat. 5676833 US; filed 08.02.96; publ. 14.10.97.
  38. Silicon carbide foam ceramic filter: pat. 100536985 China; filed 24.08.07; publ. 09.09.09.
  39. Preparation method of magnesian foamed ceramic filter for casting: pat. 101138691 China; filed 10.07.07; publ. 12.03.08.
  40. Method for preparing ceramic filter with composite pore diameter: pat. 101165003 China; filed 06.09.07; publ. 23.04.08.
  41. Shengguan Group «SQ Group» company (China) (official representative in Russia LLC «Scientific and technical center of industrial technologies»). Available at: www.sq-spb.ru (accessed: July 21, 2020).
  42. The company OOO Kit-Stroy SPb. Available at: http://t-tiss.com (accessed: July 20, 2020).
  43. Tarasovsky V.P., Krasny B.L., Koshkin V.I. et al. Quantitative analysis of the structure of permeable ceramics made of narrowly fractionated electrocorundum powder and hollow corundum microspheres. Novye ogneupory, 2016, no. 6, pp. 49–52.
  44. Buchilin N.V., Prager E.P. Reologicheskie harakteristiki shlikernyh suspenzij na osnove oksida alyuminiya. Trudy VIAM, 2015, no. 5, paper no. 06. Available at: http://www.viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2015-0-5-6-6.
  45. Buchilin N.V., Prager E.P. On rheological characteristics of alumina-based slip suspensions. Trudy VIAM, 2015, no. 8, paper no. 06. Available at: http://viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2015-0-8-6-6.
  46. Buchilin N.V., Lyulyukina G.Yu. Characteristics of sintering of highly porous alumina-based ceramic materials. Aviacionnye materialy i tehnologii, 2016, No. 4 (45), pp. 40–46. DOI: 10.18577/2071-9140-2016-0-4-40-46.
  47. Buchilin N.V., Prager E.P., Ivahnenko Yu.A. The influence of plasticizating additives on rheology of slip for porous ceramic materials based on aluminum oxide. Trudy VIAM, 2016, no. 8, paper no. 6. Available at: http://www.viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2016-0-8-6-6.
  48. Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and pro-perties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (57), pp. 54–63. DOI: 10.8577/2071-9140-2020-0-1-54-63.
  49. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.