The use of composite materials is carried out more on the widest scale. More and more relatively small, but structurally complex and critical parts of machines and mechanisms began to be made of polymers, and at the same time, polymers began to be used more and more often in the manufacture of large-sized body parts that carry significant loads. Polymer composite materials have firmly won a place among structural materials. Composite materials can no doubt be attributed to the most promising products of both modern and future industrial production.

Reference list
  1. Kablov E.N. In the history of VIAM, Petr Dementyev occupies a special place. Wings of the Motherland, 2017, no. 1, pp. 1–2.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  4. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt & Tekhnologii, 2016, no. 4, pp. 41–46.
  5. Kablov E.N. VIAM Materials and Technologies for Aviadvigatel. Permskiye aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
  6. 6. Kablov E.N. On the present and future of VIAM and Russian materials science: interviews. Rossiyskaya akademiya nauk: 2015. 19 January. Available at: https://www.ras.ru/news/shownews.aspx?id=824e2453-383e-4d9e-b78d-87v9f7bf16ee (accessed: June 27, 2020).
  7. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  8. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: June 27, 2020). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  9. Carbon fiber drive shaft: pat. US4089190A; filed 14.04.76; publ. 16.05.78.
  10. Biaxial mesh structure made of composite material: pat. RU183461 Rus. Federation; filed 25.06.18; publ. 24.09.18.
  11. Gusev Yu.A., Borshhev A.V., Khrulkov A.V. Features of prepregs intended for automated laying by ATL and AFP technologies. Trudy VIAM, 2015, no. 3, paper no. 06. Available at: http://www.viam-works.ru (accessed: September 19, 2019). DOI: 10.18577/2307-6046-2015-0-3-6-6.
  12. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Melt binding for perspective methods of production of PCM of new generation. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 260–265.
  13. Timoshkov P.N., Platonov A.A., Hrulkov A.V. Film resin infusion as an advanced method for out-of-autoclave processing of polymer composites. Trudy VIAM, 2015, no. 5, paper no. 09. Available at: http://www.viam-works.ru (accessed: November 11, 2019). DOI: 10.18577/2307-6046-2015-0-5-9-9.
  14. Donetskij K.I., Kogan D.I., Hrulkov A.V. The use of thecnology of braiding in production of structural elements of polymer composites materials. Trudy VIAM, 2013, no. 10, paper no. 04. Available at: http://www.viam-works.ru (accessed: September 19, 2019).
  15. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  16. Perov B.V., Gunyaev G.M., Rumyantsev A.F., Stroganov G.B. Application of high-modulus polymer composite materials in aircraft products. Available at: https://viam.ru/public/files/1982/1982-198546.pdf (accessed: July 27, 2020).
  17. Drive shaft made of composite materials: pat. 2601971 Rus. Federation; filed 08.09.15; publ. 10.11.16.
  18. Wagner B. Cutting Weight: Why You Should Use A Carbon Fiber Driveshaft. Available at: www.streetmusclemag.com/news/cutting-weight-why-you-should-use-a-carbon-fiber-driveshaft (accessed: April 05, 2020).
  19. Carbon fiber driveshaft Driveshaft Shop. Available at: https://www.drive2.ru/l/3888355/ (accessed: June 22, 2020).
  20. Carbon Shaft, All C63. Available at: http://weistec.com.ua/product/carbon-fiber-drive-shaft-c63-all (accessed: June 22, 2020).
  21. Shaft made of plastic. Carbon fiber. Hollow. Azimuth. Available at: https://www.directindustry.com.ru/prod/centa/product-9279-717567.html (accessed: April 05, 2020).
  22. Carbon, carbon and carbon fiber. Available at: https://carbocarbo.ru/shop/carbon_fabric (accessed: July 27, 2020).
  23. Manufacturing and repair of carbon fiber cooling tower shafts and drive shafts of sea and river vessels Centa. Available at: http://safit.info/carbon-fiber-shaft.html (accessed: April 05, 2020).