Development of adhesive composite material based on UMT49S-12K-EP alternative carbon filler and VSK-14-3 adhesive binder

Starkov A.I., Kutsevich K.E., Tyumeneva T.Y.
Starkov A.I., Kutsevich K.E., Tyumeneva T.Y. Development of adhesive composite material based on UMT49S-12K-EP alternative carbon filler and VSK-14-3 adhesive binder // Proceedings of VIAM. 2020. No. 6-7. DOI: 10.18577/2307-6046-2020-0-67-62-71. URL: https://www.viam-works.ru/en/journal/2020/6-7/7
Keywords
adhesive binder, carbon filler, adhesive prepregs, carbon fiber, polymer composite materials, strength characteristics, automated lay-out, method of automated tare laying (prepregs).
Abstract

This article presents the results of the tests of basic physical and mechanical properties of adhesive polymer composite material (PCM) based on VSK-14-3 adhesive binder with heat resistance of 150 °C and a domestic alternative unidirectional high-strength carbon filler used for production of structural parts (including honeycomb structures) in one technological cycle of sheathing molding and gluing with honeycomb layer, designed for operation in the temperature range from minus 60 to plus 150 °C, with the aim of developing the domestic PCM market to maintain global competitiveness as well as increasing independence from western producers. The article contains information about the features of the technological production process of structural elements from polymer composite materials based on adhesive binders.

Reference list
  1. Kablov E.N. Based on effective materials. Inzhenernaya gazeta, 2012, no. 4, pp. 1.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Lukina N.F., Dementyeva L.A., Petrova A.P., Kirienko T.A., Chursova L.V. Adhesive binders for PCM honeycomb parts. Klei. Germetiki. Tekhnologii, 2016, no. 5, pp. 12–16.
  4. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  5. Gunyayeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  6. Kutsevich K.E., Dementeva L.A., Lukina N.F., Tyumeneva T.Yu. Adhesive prepregs as promising materials for parts and assemblies from polymeric composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 379–387. DOI: 10.18577/2071-9140-2017-0-S-379-387.
  7. Kablov E.N. New generation materials - the basis for innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  8. Kutsevich K.E. Adhesive prepregs and carbon composites based on them: thesis, Cand. Sc. (Tech.). Moscow, 2014. 101 p.
  9. Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Influence of fillers on properties of adhesive prepregs and PCM on their basis. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
  10. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  11. Valueva M.I., Gulyaev I.N., Sidorina A.I. Russian production of carbon fillers today (review). Materials Science News. Science and technology, 2016, no. 4 (22), paper no. 7. Available at: http://www.materialsnews.ru (accessed: March 2, 2020).
  12. Grashhenkov D.V., Chursova L.V. Strategy of development of composite and functional materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 231–242.
  13. Dementyeva L.A., Serezhenkov A.A., Bocharova L.I., Lukina N.F., Kutsevich K.E., Petrova A.P. Properties of composite materials based on adhesive prepregs. Klei. Germetiki. Tekhnologii, 2012, no. 6, pp. 19–24.
  14. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  15. Morozov BB The use of polymer composite materials in products developed by the Sukhoi Design Bureau. Collection of report Conf. «Adhesives for aviation purposes». Moscow: VIAM, 2013, pp. 31–36.
  16. State Standard 25.601–80. Calculations and strength tests. Methods for mechanical testing of composite materials with a polymer matrix (composites). Method of tensile testing of flat specimens at normal, elevated and low temperatures. Moscow: Standartinform, 2005, 9 p.
  17. State Standard 25.602–80. Calculations and strength tests. Methods for mechanical testing of composite materials with a polymer matrix (composites). Compression test method at normal, high and low temperatures. Moscow: Standartinform, 2005, 13 p.
  18. State Standard 25.604–82. Calculations and strength tests. Methods for mechanical testing of composite materials with a polymer matrix (composites). Bending test method at normal, high and low temperatures. Moscow: Standartinform, 2007, 7 p.
  19. State Standard 15139–69. Plastics. Method for determining density (bulk density). Moscow: Publishing house of standards, 1990. 80 p.
  20. State Standard 9.707–81. Unified system of protection against corrosion and aging. Moscow: Publishing house of standards, 1988.
  21. Guidance Document 50-675-88. Methodical instructions. Calculations and tests for strength in mechanical engineering. Composite materials. Interlaminar shear test methods. Moscow: Publishing house of standards, 1989, 9 p.
  22. Lukina N.F., Dementeva L.A., Kutsevich K.E. Adhesive prepregs based on tissue Porsher – perspective materials for parts and units out of polymeric composite materials. Trudy VIAM, 2014, no. 6, paper no. 10. Available at: http://www.viam-works.ru (accessed: March 4, 2020). DOI: 10.18577/2307-6046-2014-0-6-10-10.
  23. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Development of FSUE «VIAM» in the field of melt binders for polymer composite materials. Polimernyye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  24. Kutsevich K.E., Dementeva L.A., Lukina N.F. Properties and application of polymer composite materials based on glue prepregs. Trudy VIAM, 2016, no. 8, paper no. 7. Available at: http://www.viam-works.ru (accessed: March 4, 2020). DOI: 10.18577/2307-6046-2016-0-8-7-7.
  25. Petrova A.P., Donskoy A.A., Chalykh A.E., Shcherbina A.A. Adhesive materials. Sealants: a reference book. Saint Petersburg: Professional, 2008, 589 p.
  26. Dementyeva L.A., Lukina N.F., Serezhenkov A.A., Kutsevich K.E. Basic properties and purpose of PCM based on adhesive prepregs. Abstacts of reports of XIX Int. scientific and technical conf. «Designs and technology for producing products from non-metallic materials». Obninsk: ONPP «Tekhnologiya», 2010, pp. 11–12.
  27. Gusev Yu.A., Borshhev A.V., Khrulkov A.V. Features of prepregs intended for automated laying by ATL and AFP technologies. Trudy VIAM, 2015, no. 3, paper no. 6. Available at: http://www.viam-works.ru (accessed: March 4, 2020). DOI: 10.18577/2307-6046-2015-0-3-6-6.
  28. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Study of moisture transport rules and development of a standard on measurement of the diffusion coefficient and moisture content limit to evaluate mechanical properties of carbon fiber reinforced plastics. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 44–48.