Method of increasing tightness and hardening of cast corrosion-resistant welded magnalias

Duyunova V.A., Leonov A.A., Trapeznikov A.V.
Duyunova V.A., Leonov A.A., Trapeznikov A.V. Method of increasing tightness and hardening of cast corrosion-resistant welded magnalias // Proceedings of VIAM. 2020. No. 6-7. DOI: 10.18577/2307-6046-2020-0-67-11-18. URL: https://www.viam-works.ru/en/journal/2020/6-7/2
Keywords
foundry magnalias, tightness, abrasive treatment, hot isostatic pressing, density, gas-shrink porosity, through defects.
Abstract

Based on the studies, it was found that abrasive treatment of castings surface made from Al–Mg alloys in combination with hot isostatic pressing is a very promising stage of the technological process of manufacturing responsible cast parts and welded structural elements with high strength, corrosion resistance and tightness. Practice of proposed physical and mechanical complex treatment of VAL19 magnalia castings received in cold-box mold allows getting solid structure(I–II point) and high tightness castings, and also guarantee high level of mechanical properties.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58..
  3. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  4. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  5. Lukin V.I., Kovalchuk V.G., Ioda E.N. Fusion welding is a core of welding manufacturing. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 130–143. DOI: 10.18577/2071-9140-2017-0-S-130-143.
  6. Fridlander I.N. Creation, research and application of aluminum alloys. Selected works. Ed. E.N. Kablov. Moscow: Nauka, 2013, 291 p.
  7. Hafenstein S., Werner E. Pressure dependence of age-hardenability of aluminum cast alloys and coarsening of precipitates during hot isostatic pressing. Materials Science & Engineering: A, 2019, vol. 757, pp. 62–69.
  8. Napalkov V.I., Makhov S.V., Bobryshev B.L., Moiseev V.S. Physico-mechanical processes of aluminum refining and its alloys. Moscow: Teplotekhnik, 2011, 496 p.
  9. Belov N.A., Savchenko S.V., Belov V.D. Atlas of microstructures of industrial silumins. Moscow: Publishing house MISIS, 2009, 204 p.
  10. Belov E.V., Duyunova V.A., Leonov A.V., Trapeznikov A.V. Features of the formation of the structure and properties of casting magnals during thermal stabilizing annealing. Tekhnologiya mashinostroeniya, 2019, no. 12, pp. 5–12.
  11. Zolotorevsky V.S., Belov N.A. Metallurgy of foundry aluminum alloys. Moscow: MISiS, 2005, 376 p.
  12. Engler O., Marioara C.D., Aruga Y. et al. Effect of natural aging or pre aging on the evolution of precipitate structure and strength during age hardening of Al – Mg – Si alloy AA 6016. Materials Science & Engineering: A, 2019, vol. 759, pp. 520–529.
  13. Kuznetsov A.O., Oglodkov M.S., Klimkina A.A. The influence of chemical composition on structure and properties of Al–Mg–Si alloy. Trudy VIAM, 2018, no. 7 (67), paper no. 01. Available at: http://www.viam-works.ru (accessed: February 25, 2020). DOI: 10.18577/2307-6046-2018-0-7-3-9.
  14. Belov E.V., Duyunova V.A., Leonov A.V., Trapeznikov A.V. Management of structure formation and properties of welded joints of aluminum lithodeformed alloys with low specific gravity. Svarochnoye proizvodstvo, 2019, no. 7, pp. 3–11.
  15. Postnikov N.S. Hardening of aluminum alloys and castings. Moscow: Metallurgiya, 1983, 119 p.