Analysis of the US federal aviation administration proposals for the reform of aviation standards regarding the fire safety of used materials (review)

Barbotko S.L., Volnyj O.S., Bochenkov M.M.
Barbotko S.L., Volnyj O.S., Bochenkov M.M. Analysis of the US federal aviation administration proposals for the reform of aviation standards regarding the fire safety of used materials (review) // Proceedings of VIAM. 2020. No. 6-7. DOI: 10.18577/2307-6046-2020-0-67-101-117. URL: https://www.viam-works.ru/en/journal/2020/6-7/11
Keywords
airworthiness regulations, fire safety, test methods, Federal Aviation Administration, proposed rulemaking.
Abstract

A draft of the US Federal Aviation Administration on amendments to the text of aviation standards regarding fire safety requirements is considered. In the proposed set of documents, a significant change in the requirements and the test methods used is planned. After the adoption of this amendment, in order to certify new brands of domestic aviation equipment for compliance with foreign aviation standards, as well as to create competitive materials, it is necessary to develop a domestic testing base for conducting fire tests.

Reference list
  1. Review and Assessment of Transport Category Airplane Ditching Standards and Requirements. Available at: http://www.fire.tc.faa.gov/pdf/TC-14-8.pdf (accessed: July 10, 2020).
  2. Structural Factors influencing the Survivability of Occupants in Airplane Accidents. Available at: http://www.fire.tc.faa.gov/2016Conference/files/Crash_Dynamics_I/CherrySurvivability/CherrySurvivabilityPres.pdf (accessed: July 10, 2020).
  3. Analysis of the state of flight safety in civil aviation of the Russian Federation in 2017. Available at: http://szfavt.ru/wp-content/uploads/2018/06/ analyz_po_bp_2017.pdf (accessed: March 02, 2020).
  4. Mouritz A.P., Gibson A.G. Fire Properties of Polymer Composite Materials. Dordrecht: Springer, 2006, 398 p.
  5. RRJ-95B RA-89098 Aircraft Accident Investigation Preliminary Repor. Available at: http://mak-iac.org/upload/iblock/4e4/ report_ra-89098_pr.pdf (accessed: July 10, 2020).
  6. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Assessment of the fire safety of polymer materials for aviation purposes: analysis of the state, test methods, development prospects, methodological features. Ed. E.N. Kablov. Moscow: VIAM, 2018, 424 p.
  7. 1/4 Scale Fire Penetration Testing of Composite Fuselage. Sixth Triennial International Fire & Cabin Safety Research Conference. Atlantic City, 2010. 22 p. Available at: http://www.fire.tc.faa.gov/ 2010Conference/files/Materials_Safety_Development_I/LopezFirePenetration/LopezFirepenetrationPres.pdf (accessed: March 02, 2020).
  8. Lyon R.E. Nongalogen Fire-Resistant Plastics for Aircraft Interiors. Available at: http://www.fire.tc.faa.gov/pdf/TN08-5.pdf (accessed: July 10, 2020).
  9. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  10. Kurnosov A.O., Sokolov I.I., Melnikov D.A., Topunova T.E. Fireproof fiberglass for interior of passenger aircraft (review). Trudy VIAM, 2015, no. 11, paper no. 07. Available at: http://www.viam-works.ru (accessed: October 10, 2019). DOI: 10.18577/2307-6046-2015-0-11-7-7.
  11. Kutsevich K.E., Dementeva L.A., Lukina N.F., Tyumeneva T.Yu. Adhesive prepregs as promising materials for parts and assemblies from polymeric composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 379–387. DOI: 10.18577/2071-9140-2017-0-S-379-387.
  12. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  13. Marketing of materials science, aircraft construction and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
  14. Carlo Al. Strategic Approach to Fire Safety. The 7th Triennial International Fire & Cabin Safety Research Conference. 2013. 13 p. Available at: http://www.fire.tc.faa.gov/2013Conference/files/ Aircraft_Fire_Safety/CarloStrategicApproach/CarloStrategicApproachPres.pdf (accessed: July 10, 2020).
  15. Maloney T., Dadia D.D. Passive Protection of Lithium Battery Shipments. Available at: http://www.fire.tc.faa.gov/pdf/TC-15-38.pdf (accessed: March 02, 2020).
  16. Allen St. J. What's Behind the Increase in Lithium-Ion Battery Fires on Planes?: The FAA reports that, on average, one of these fires occurs every 10 days. Here’s what passengers need to know. Available at: http://www.consumerreports.org/product-safety/whats-behind-the-increase-in-lithium-ion-battery-fires-on-planes (accessed: March 02, 2020).
  17. Dadia D. Class E Cargo Compartment Mitigation Strategies Subjected to Class-A Fires. Available at: http://www.fire.tc.faa.gov/2016Conference/files/Cargo_Fire_I/DadiaFCCsFRCsClassA/DadiaFCCsFRCsClassAPres.pptx (accessed: March 02, 2020).
  18. Barbotko S.L. Fire safety of polymer materials for aviation and structural elements based on them: thesis, Dr. Sc. (Tech.). Available at: http: www.viam.ru/disser (accessed: April 01, 2019).
  19. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Analysis of the main directions of research carried out by foreign organizations dealing with fire safety of aviation equipment and materials for aerospace purposes (review). Problemy bezopasnosti poletov, 2018, no. 2, pp. 3–35.
  20. Barbotko S.L. Development of the fire safety test methods for aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  21. Barbotko S.L. Requirements of aviation standards and methods for assessing the fire safety of aviation materials: history, current state and development prospects. Vestnik Voronezhskogo instituta GPS MCHS Rossii, 2014, no. 3 (12), pp. 23–33.
  22. Barbotko S.L., Kirienko O.A., Volny O.S., Lutsenko A.N. Fire hazard analysis of aircraft engine nacelles and other fire hazardous areas; used methods of fire tests of materials and structural elements for compliance with the requirements of aviation standards. Problemy bezopasnosti poletov, 2017, no. 5, no. 3–24.
  23. 9th Triennial International Aircraft Fire and Cabin Safety Research Conference. Available at: http://www.fire.tc.faa.gov/2019Conference/conference.asp (accessed: July 10, 2020).
  24. Marker T.R. Short Takes and Current Projects. Available at: http://www.fire.tc.faa.gov/pdf/materials/June19Meeting/Marker-0619-Shorttakes.pdf (accessed: March 02, 2020).
  25. Marker T.R. Aircraft Materials Fire Test Handbook, Revision 3. Available at: https://www.fire.tc.faa.gov/pdf/TC17-55.pdf (accessed: March 02, 2020).
  26. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  27. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing are the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  28. Barbotko S.L. Fire safety of aviation materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 431–439.
  29. Aeronautics and Space. Federal Register. 1964. P. 18289–18353.
  30. Standards of airworthiness of civil aircraft of the USSR. Second edition. Moscow: TsAGI, 1974, 344 p.
  31. Standards of airworthiness of civil aircraft of the USSR. Third edition. Moscow: TsAGI, 1984, 464 p.
  32. Aviation regulations 25. Standards of airworthiness of transport category aircraft. 3rd ed. Moscow: Aviaizdat, 2009, 267 p.
  33. Transport Category Airplanes: Airworthiness Standards. Part 25. Available at: http://www.ecfr.gov/cgi-bin/text-idx?SID=d7f8803c7bd1d50b6d68749e0b42d848&node=14:1.0.1.3.11&rgn=div5 (accessed: March 11, 2020).
  34. Certification Specifications and Acceptable Means of Compliance for Large Aeroplanes. Available at: https://www.easa.europa.eu/sites/default/files/dfu/CS-25%20Amendment%2024.pdf (accessed: March 11, 2020).
  35. Interior Parts and Components Fire Protection for Transport Category Airplanes. Available at: https://www.federalregister.gov/documents/2019/07/03/2019-13646/interior-parts-and-components-fire-protection-for-transport-category-airplanes (accessed: March 11, 2020).
  36. Flammability Requirements for Transport Category Airplanes. Available at: https://www.regulations.gov/document?D=FAA-2019-0491-0018 (accessed: March 11, 2020).
  37. Flammability Requirements for Aircraft Seat Cushions. Available at: https://www.regulations.gov/document?D=FAA-2019-0491-0019 (accessed: March 11, 2020).
  38. Flammability Testing Requirements for Commonly Constructed Parts, Construction Details, and Materials Used on Transport Category Airplanes. Available at: https://www.regulations.gov/document?D=FAA-2019-0491-0020 (accessed: March 11, 2020).
  39. Vertical Bunsen Burner Tests. Available at: https://www.regulations.gov/document?D=FAA-2019-0491-0021 (accessed: March 11, 2020).
  40. Flammability Requirements for Materials in Inaccessible Areas of Transport Category Airplanes. Available at: https://www.regulations.gov/document?D=FAA-2019-0491-0022 (accessed: March 11, 2020).
  41. Flammability Requirements for Escape System Materials for Transport Category Airplanes. Available at: https://www.regulations.gov/document?D=FAA-2019-0491-0023 (accessed: March 11, 2020).
  42. Flammability Requirements of Cargo Liners for Transport Category Airplanes. Available at: https://www.regulations.gov/document?D=FAA-2019-0491-0024 (accessed: March 11, 2020).
  43. Thermal/Acoustic Insulation Flame Propagation Test Method Details. Available at: https://www.regulations.gov/document?D=FAA-2019-0491-0025 (accessed: March 11, 2020).
  44. Fuselage Burnthrough Protection. Available at: https://www.regulations.gov/ document?D=FAA-2019-0491-0026 (accessed: March 11, 2020).
  45. Electrical Fault and Fire Prevention and Protection. Available at: https://www.faa.gov/regulations_policies/advisory_circulars/index.cfm/go/document.information/documentID/22502 (accessed: July 10, 2020).
  46. Transport Airplane Interiors Crashworthiness Handbook. Available at: http://www.faa.gov/documentLibrary/media/Advisory_Circular/AC_25-17A_CHG-1.pdf (accessed: July 10, 2020).
  47. Development of Transport Category Airplane Electrical Wiring Interconnection Systems Instructions for Continued Airworthiness Using and Enhanced Zonal Analysis Procedure. Available at: https://www.faa.gov/regulations_policies/advisory_circulars/index.cfm/go/ document.information/documentID/319197 (accessed: July 10, 2020).
  48. Fire Protection: Systems. Available at: https://www.faa.gov/regulations_policies/ advisory_circulars/index.cfm/go/document.information/documentID/74393 (accessed: July 10, 2020).
  49. Certification of Electrical Wiring Interconnection Systems on Transport Category Airplanes. Available at: https://www.faa.gov/regulations_policies/advisory_circulars/index.cfm/go/ document.information/documentID/73476 (accessed: July 10, 2020).
  50. Engine fire Protection. Available at: https://www.faa.gov/regulations_policies/ advisory_circulars/index.cfm/go/document.information/documentID/99608 (accessed: July 10, 2020).
  51. Powerplant Installation and Propulsion System Component Fire Protection Test Methods, Standards, and Criteria. Available at: https://www.faa.gov/regulations_policies/ advisory_circulars/index.cfm/go/document.information/documentID/22194 (accessed: July 10, 2020).
  52. Flammability Testing of Interior Materials. Available at: https://rgl.faa.gov/ Regulatory_and_Guidance_Library/rgPolicy.nsf/0/2e766e58ed65176d86257baa0063eca7/$FILE/PS-ANM-25.853-01-R2.pdf (accessed: July 10, 2020).
  53. Aircraft Materials Fire Test Handbook. Available at: http://www.fire.tc.faa.gov/handbook.stm (accessed: 31.01.2020).