Research of the biological and corrosion resistance of samples of aluminum alloy after natural tests in the Gelenjik bay

Part 1
Varchenko E.A., Vetrova E.Yu.
Varchenko E.A., Vetrova E.Yu. Research of the biological and corrosion resistance of samples of aluminum alloy after natural tests in the Gelenjik bay. Part 1 // Proceedings of VIAM. 2020. No. 6-7. DOI: 10.18577/2307-6046-2020-0-67-91-100. URL: https://www.viam-works.ru/en/journal/2020/6-7/10
Keywords
fouling, field exposure, biological stability of materials, marine tests.
Abstract

The main goal in the formulation of this work was to study the influence of biological and physico-chemical factors of sea water on the change in the properties of metallic and nonmetallic materials in the coastal zone of the Gelendzhik Bay. In this part of the article, the biological component of this work is considered, a qualitative and quantitative assessment of biofouling materials after a seasonal (summer) exposure is given. Separately, attention is focused on the lack of reliable, simple and, most importantly, reliable experimental techniques to unambiguously distinguish the biological component from the general corrosion background.

Reference list
  1. Ivanov V.A., Belokopytov V.N. Oceanography of the Black Sea. Sevastopol: EKOSI-Gidrofizika, 2011.212 p.
  2. Mikheev A.I. Influence of fouling and low temperatures on the safe operation of ships. Vodniy transport, 2013, Issue, 3, pp. 56–61.
  3. Shkabara N.A. Ecological and technological study of barrier-type coating for protection against corrosion and marine fouling of oil and gas pipelines, floating facilities and port facilities (on the example of Gelendzhik Bay): thesis abstracts Cand. Sc. (Tech). Krasnodar, 2015, 113 p.
  4. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Kablov E.N. The key problem is materials. Trends and guidelines for innovative development in Russia. Moscow: VIAM, 2015, pp. 458–464.
  6. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  7. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  8. Laptev A.B., Barbotko S.L., Nikolaev E.V. The main research areas of the persistence properties of materials under the influence of climatic and operational factors. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
  9. Leonov V.V., Denisova O.A. Electrochemical method for studying the processes of microbial corrosion. Electrotechnical and information complexes and systems, 2016, vol. 12, no.4, pp. 111–118.
  10. Karpov V., Kovalchuk Yu., Ilyin I., Poltarukha O. An integrated approach to protection from marine fouling and corrosion. Moscow: T-vo nauchnykh izdaniy KMK, 2007, 152 p.
  11. Reznichenko O.G., Soldatova I.N., Tsikhon-Lukanina E.A. Fouling in the World Ocean. Zoology of invertebrates. Results of Science and Technology. Moscow: VINITI, 1976, vol. 4, 120 p.
  12. Oshurkov V.V. Dynamics and structures of some communities of fouling and benthos of the White Sea. Ecology of fouling in the White Sea. Leningrad: Zoological Institute of the USSR Academy of Sciences, 1985, pp. 44–59.
  13. Lyublinsky E.Ya., Yakubenko A.R. Strategy and tactics of protection against marine fouling. Reports of the All-Union. scientific and technical conf. «Protection of ships and technical equipment from fouling». Leningrad: Sudostroenie, 1990, pp. 5–16.
  14. Zvyagintsev A.Yu. Marine fouling in the northwestern Pacific. Vladivostok: Dalnauka, 2005.432 p.
  15. Marine fouling and the fight against it. Eds. V.N. Nikitin, N.I. Tarasov. Moscow: Voenizdat, 1957, 502 p.
  16. Zevina G.B. Biology of marine fouling. Moscow: MSU, 1994, 134 p.
  17. Ilyin I.N. Ecology of oceanic fouling in the pelagic zone. Moscow: T-vo nauchnykh izdaniy KMK, 2007. S. 42–68.
  18. Bocharov B.V., Zevina G.B., Ilyin I.N. et al. Fouling in the southern part of Vietnam. Biological damage, fouling and protection from it. Moscow: Nauka, 1996, pp. 37–39.
  19. Grigorieva N.D., Danilovskaya L.P., Talanova E.I. Corrosion of metals and ship structures: method. directions. St. Petersburg ITs SPbGMTU, 2005, pp. 32.
  20. Petrova N.E., Baeva L.S. Biocorrosion of ship hulls. Vestnik MGTU, 2006, vol. 9, no. 5, pp. 890–892.
  21. Filippov D.M. Circulation and structure of the Black Sea waters. Moscow: Nauka, 1968., 136 p.
  22. Blatov A.S., Bulgakov N.P., Ivanov V.A. et al. Variability of the Black Sea hydrophysical fields. Leningrad: Gidrometeoizdat, 1984. 239 p.
  23. Blatov A.S., Kosarev A.N., Tuzhilkin V.S. Variability of the hydrological structure of the Black Sea waters and its relationship with external factors. Vodniye resursy, 1980, no. 6, pp. 71–82.
  24. Ovchinnikov I.M., Titov V.B., Krivosheya V.G. New data on the temporal variability of currents based on the results of long-term measurements from a stabilized buoy on the shelf of the Black Sea. Doklady AN SSSR, 1986, vol. 286, no. 5, pp. 1250–1254.
  25. Petrov K.M. Phytobenthos as an indicator of the state of the water area of the Absheron archipelago (Caspian Sea). Advances in Biology & Earth Sciences, 2018, vVol. 3, no. 2, pp. 140–151.
  26. Gontar V.I. Life strategies of bryozoans in periphyton communities. Materials of All-Rus. conf. from int. participation «Physiological, biochemical and molecular-genetic mechanisms of adaptation of aquatic organisms». Borok, 2012, pp. 105–110.