Influence of silicate fillers on operational properties of coatings based on protective polymeric pastes with the lowered content of strontium chromate

Kovrizhkina N.A., Kuznetsova V.A., Kozlov I.A., Vdovin A.I., Silaeva A.A.
Kovrizhkina N.A., Kuznetsova V.A., Kozlov I.A., Vdovin A.I., Silaeva A.A. Influence of silicate fillers on operational properties of coatings based on protective polymeric pastes with the lowered content of strontium chromate // Proceedings of VIAM. 2020. No. 4-5. DOI: 10.18577/2307-6046-2020-0-45-80-88. URL: https://www.viam-works.ru/en/journal/2020/4-5/9
Keywords
anticorrosive paint and varnish materials, silicate fillers, microwollastonite, microtalc, strontium chromate, impedance spectroscopy, physicomechanical properties, adhesive properties, protective properties, water absorption.
Abstract

In this article influence of silicate fillers on operational properties of coatings, based on protective polymeric pastes VP-1 and VZP-1 with the lowered content of strontium chromate is studied. It is shown that microwollastonite introduction positively affects the adhesive durability, hardness and water absorption of the received coatings. It is established that partial replacement strontium chromate on microwollastonite as a part of VP-1 paste does not lead to decrease in protective properties of coatings, and in case of VZP-1 paste - allows to increase protective properties of coatings. 

Reference list
  1. Lambourne R., Mashlyakovsky L.N., Frost A.M. Paints and coatings. Theory and practice. St. Petersburg: Himiya, 1991, 512 p.
  2. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  3. Kuznetsova V.A., Semenova L.V., Kondrashov E.K., Lebedeva T.A. Paint-and-lacquer materials with a low content of harmful and design of polymer composite materials. Trudy VIAM, 2013, no. 8, paper no. 05. Available at: http://www.viam-works.ru (accessed: February 05, 2020).
  4. Kablov E.N. Innovative development is the most important state priority. Metally Evrazii, 2010, no. 2, pp. 6–11.
  5. Kalininskaya T.V., Drinberg A.S. Color pigments. Moscow: LKM-press, 2013, 360 p.
  6. Sorokov A.V. Anticorrosive properties of synthetic manganese- and phosphonate-containing pigments and primers based on them: thesis, Cand. Sc. (Tech.). Kazan: Kazan. state technolog. univ., 2003, 118 p.
  7. Lavrukhina A.K., Yukina L.V. Analytical chemistry of chromium. Moscow: Nauka, 1979, 214 p.
  8. Kablov E.N., Karimov S.A., Semenova L.V. Corrosion activity of carbon plastics and the protection of metal power structures in contact with carbon fiber. Korroziya: materialy, zashchita, 2011, no. 12, pp. 1–7.
  9. Kuznetsova V.A., Semenova L.V., Shapovalov G.G., Chesnokov D.V. Polymeric compositions for protection against contact corrosion. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 70–76. DOI: 10.18577/2071-9140-2017-0-4-70-76.
  10. Kuznetsova V.A., Semenova L.V., Shapovalov G.G. Development trends in the field of anticorrosive polymeric systems for corrosion protection of fixing connections of contact couples of combined structures (review). Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 25–31. DOI: 10.18577/2071-9140-2017-0-1-25-31.
  11. Gerasimova L.G., Skorokhodova O.N. Fillers for the paint industry. Moscow: LKM-press, 2010, 224 p.
  12. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  13. Nazarenko V.V. Anisotropic silicate fillers: special properties in coatings and coatings. Lakokrasochnyye materialy i ikh primeneniye, 2012, no. 1–2, pp. 25–33.
  14. Akatieva L.V. The development of chemical and technological fundamentals of the processing of raw materials for calcium silicates and composite materials: thesis, Dr. Sc. (Tech.). Moscow: IONH RAS, 2014, 300 p.
  15. Poluektova E.A. Wollastonite – a unique filler for paintwork materials. Lakokrasochnyye materialy i ikh primeneniye, 2012, no. 6, pp. 24–26.
  16. Anticorrosive composition: pat. 2405012 Rus. Federation; filed 03.03.09; publ. 27.11.10.
  17. Khasanova A.R. The effect of the modification of epoxy compositions by wollastonite on the hardness of materials for mechanical engineering. Mezhdunar. molodezh. nauch. konf. «XXIII Tupolevskiye chteniya (shkola molodykh uchenykh)». Kazan, 2017, pp. 373–376.
  18. Koroboschikova T.S., Orlova N.A. Modeling the mechanical properties of a paint material filled with wollastonite. Lakokrasochnyye materialy i ikh primenenie, 2011, no. 1–2, pp. 62–64.
  19. Gnedenkov S.V., Sinebryukhov S.L. Impedance spectroscopy in the study of charge transfer processes. Vestnik DVO RAN, 2006, no. 5, pp. 6–16.
  20. Kozlova A.A., Kuznetsova V.A., Kozlov I.A., Naprienko S.A., Silaeva A.A. The effect of prolonged heating on the properties of protective coatings for aluminum alloy system Al–Si–Mg. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 74–80. DOI: 10.18577/2071-9140-2019-0-2-74-80.