Structure and properties of plasma electrolytic oxide coating formed on aluminum alloy of Al–Cu–Mg–Li system

Fomina M.A., Kozlov I.A., Kutyrev A.E.
Fomina M.A., Kozlov I.A., Kutyrev A.E. Structure and properties of plasma electrolytic oxide coating formed on aluminum alloy of Al–Cu–Mg–Li system // Proceedings of VIAM. 2020. No. 4-5. DOI: 10.18577/2307-6046-2020-0-45-70-79. URL: https://www.viam-works.ru/en/journal/2020/4-5/8
Keywords
aluminum alloys, conversion coatings, oxidation, coatings, plasma electrolytic oxidation, microhardness of the coating, mechanism of coating growth.
Abstract

In work researches of the plasma electrolytic oxide covering formed with application of silicate and phosphatic electrolit on samples of a sheet semi-finished product from aluminum – a lithium alloy 1441-Т1 are conducted. It is established that thickness of a covering has linear dependence on time in the range from 30 till 165 min. The analysis of a chemical composition and the mechanism of formation of a plasma electrolytic covering is carried out. Research of structure of a covering allowed to establish dependence of properties (microhardness, breakdown resistance) from porosity and other internal defects.

Reference list
  1. Kablov E.N., Antipov V.V., Klochkova Yu.Yu. New-generation aluminum-lithium alloys and layered aluminum-glass-reinforced plastics based on them. Tsvetnyye metally, 2016, no. 8, pp. 86–91. DOI: 10.17580/tsm.2016.08.13.
  2. Kablov E.N., Lukina E.A., Sbitneva S.V., Khokhlatova LB, Zaitsev D.V. The formation of metastable phases during the decomposition of a solid solution in the process of artificial aging Al-alloys. Tekhnologiya legkikh splavov, 2016, no. 3, pp. 7–17.
  3. Han L.N., Sui Y.D., Wang Q.D. et al. Effects of Nd on microstructure and mechanical properties of cast Al – Si – Cu – Ni – Mg piston alloys. Alloys Compound, 2017, no. 695, pp. 1566–1572.
  4. Klochkov G.G., Grushko O.E., Klochkova Ju.Ju., Romanenko V.A. Industrial development of strength alloy V-1469 of Al–Cu–Li–Mg. Trudy VIAM, 2014, no. 7, paper no. 1. Available at: http://viam-works.ru (accessed: January 16, 2020). DOI: 10.18577/2307-6046-2014-0-7-1-1.
  5. Shiju L., Chen H., Jinyu F. et al. Evolution of microstructure and properties of novel aluminum-lithium alloy with different roll casting process parameters during twin-roll casting. Materials Characterization. Available at: http://www.semanticscholar.org/paper/Evolution-of-microstructure-and-properties-of-novel-Li-He (accessed: January 16, 2020). DOI: 10.1016/j.mtla.2018.100203.
  6. Jiaqiang H., Junsheng W., Mingshan Z., Kangmin N. Susceptibility of lithium containing aluminum alloys to cracking during solidification. Materialia. 2019, vol. 5. Article 100203. DOI: 10.1016/j.mtla.2018.100203.
  7. Meriç C. Physical and mechanical properties of cast under vacuum aluminum alloy 2024 containing lithium additions. Materials Research Bulletin, 2000, vol. 35, is. 9, pp. 1479–1494.
  8. Ghosh A., Adesola A., Szpunar J.A. Effect of tempering conditions on dynamic deformation behavior of an aluminum-lithium alloy. Materials & Design, 2015, vol. 81, pp. 1–10.
  9. Niraj N., Gurao N.P., Murty N. et al. Microstructure and micro-texture evolution during large strain deformation of an aluminum-copper-lithium alloy AA 2195. Materials & Design, 2015, vol. 65, pp. 862–868.
  10. Odeshi A.G., Tiamiyu A.A., Das D. et al. High strain-rate deformation of T8-tempered, cryo-rolled and ultrafine grained AA 2099 aluminum alloy. Materials Science and Engineering: A, 2019, vol. 754, pp. 602–612.
  11. Yang H.L., Ji S.X., Fan Z.Y. Effect of heat treatment and Fe content on the microstructure and mechanical properties of die-cast Al-Si-Cu alloys. Materials & Design, 2015, no. 85, pp. 823–832.
  12. Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Heat treatment influence on characteristics of welding joints of high-strength aluminum-lithium alloys. Trudy VIAM, 2015, no. 4, paper no. 6. Available at: http://www.viam-works.ru (accessed: January 01, 2020). DOI: 10.18577/2307-6046-2015-0-4-6-6.
  13. Yoganandan G., Balaraju J.N., Christopher H.C. et al. Electrochemical and long term corrosion behavior of Mn and Mo oxyanions sealed anodic oxide surface developed on aerospace aluminum alloy (AA2024). Surface & Coatings Technology, 2016, no. 288, pp. 115–125.
  14. Antipov V.V., Chesnokov D.V., Kozlov I.A., Volkov I.A., Petrova A.P. Surface preparation aluminum alloy V-1469 before use in the composition of layered hybrid material. Trudy VIAM, 2018, no. 4 (64), paper no. 07. Available at: http://www.viam-works.ru (accessed: February 17, 2020). DOI: 10.18577/2307-6046-2018-0-4-59-65.
  15. Ma Y., Zhou X., Liao Y. et al. Effect of anodizing parameters on film morphology and corrosion resistance of AA2099. Journal of The Electrochemical Society, 2016, no. 163 (7), pp. 369–376.
  16. Fridlyander I.N., Drits A.M., Vovnyanko A.G. New aluminum alloys for critical power structures of aircraft. Aviatsionnaya promyshlennost, 1985, no. 6, pp. 56–58.
  17. Shalin R.E., Fridlyander I.N., Leshchiner L.N., Butusova I.V., Kuznetsova N.B. Aluminum alloys for passenger aircraft. Aviatsionnaya promyshlennost, 1988, no. 6, pp. 88–89.
  18. Fridlyander I.N., Leshchiner L.N., Sandler V.S., Latushkina L.V., Vorobyev O.I., Nikolskaya T.I. Structure and properties of alloys of the Al–Cu–Mg–Li system. Aviatsionnaya promyshlennost, 1986, no. 8, pp. 59–61.
  19. Fridlyander I.N., Grushko O.E., Antipov V.V., Kolobnev N.I., Khokhlatova L.B. Aluminum-lithium alloys. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 8, pp. 22–27.
  20. Antipov V.V., Serebrennikova N.Yu., Nefedova Yu.N., Kozlova O.Yu., Panteleev M.D., Osipov N.N., Klychеv A.V. Manufacturing capability of Al–Li 1441 alloy details. Trudy VIAM, 2018, no. 10 (70), paper no. 03 Available at: http://www.viam-works.ru (accessed: February 17, 2020). DOI: 10.18577/2307-6046- 2018-0-10-17-26.
  21. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  22. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2107-9140-2017-0-S-195-211.
  23. Kablov E.N., Antipov V.V., Senatorova O.G. SIAL-1441 laminated aluminoglassplastics and cooperation with AIRBUS and TU DELFT. Tsvetnyye metally, 2013, no. 9, pp. 50–53.
  24. Pavlovskaya T.G., Volkov I.A., Kozlov I.A., Naprienko S.A. Ecologically improved technology of aluminum alloys surface treatment. Trudy VIAM, 2016, no. 7, paper no. 02. Available at: http://viam-works.ru (accessed: February 17, 2020). DOI: 10.18577/2307-6046-2016-0-7-2-2.
  25. Antipov V.V., Petrova A.P., Kozlov I.A., Fomina M.A., Volkov I.A. Influence of technological heatings and ways of surface preparation under pasting on mechanical properties of aluminum foil from alloy AMg2N. Trudy VIAM, 2018, no. 7 (67), paper no. 02. Available at: http://www.viam-works.ru (accessed: February 17, 2020). DOI: 10.18577/2307-6046-2018-0-7-10-24.
  26. A method of obtaining a coating on aluminum alloys: pat. 2547983 Rus. Federation; filed 14.04.14; publ. 10.04.15.
  27. A solution for sealing the anodic oxide coating of aluminum alloys: pat. 2447201 Rus. Federation; declared 05.04.11; publ. 10.04.12.
  28. Alekseev A.V., Rastegaeva G.Yu., Pakhomkina T.N., Razmakhov M.G. Determination sulfur, carbon, nitrogen and oxygen in alloys of system Co–Fe–Co–B and Gd–Fe–Co–B. Trudy VIAM, 2019, No. 8 (80), paper No. 10. Available at: http://www.viam-works.ru (accessed: January 01, 2020). DOI: 10.18557/2307-6046-2019-0-8-90-97.
  29. Suminov I.V., Epelfeld A.V., Lyudin V.B. et al. Microarc oxidation (theory, technology, equipment). Moscow: ECOMET, 2005, 368 p.
  30. Suminov I.V., Belkin P.N., Epelfeld A.V. et al. Plasma-electrolytic surface modification of metals and alloys: in 2 vols. Moscow: Tekhnosfera, 2011, vol. 2, 512 p.
  31. Rakoch A.G., Bardin I.V. Microarc oxidation of light alloys. Metallurg, 2010, no. 6, pp. 58–61.
  32. Markov G.A., Terleeva O.P., Shulepko E.K. Microarc and arc methods of applying protective coatings. Tr. Mosk. in-ta nefti i gaza im. I.M. Gubkina. Moscow, 1985, pp. 54–56.
  33. Jovović J., Stojadinović S., Šišović N.M., Konjević N. Spectroscopic characterization of plasma during electrolytic oxidation (PEO) of aluminum. Surface and Coatings Technology, 2011, vol. 206, pp. 24–28.
  34. Parfenov E.V., Yerokhin A., Nevyantseva R.R., Gorbatkov M.V. Towards smart electrolytic plasma technologies: An overview of methodological approaches to process modeling. Surface and Coatings Technology, 2015, vol. 269, pp. 2–22.
  35. Hussein R.O., Northwood D.O., Nie X. Coating growth behavior during the plasma electrolytic oxidation process. Journal of Vacuum Science and Technology A: Vacuum, Surfaces and Films, 2010, no. 28, pp. 766–773.
  36. Ying-liang S., Zhi-gang X., Qun W. New findings on properties of plasma electrolytic oxidation coatingsfrom study of an Al – Cu – Li alloy. Electrochimica Acta, 2013, no. 107, pp. 358–378.
  37. Ying-liang C., Jin-hui S., Moke M. High growth rate, wear resistant coatings on an Al – Cu – Li alloy by plasma electrolytic oxidation in concentrated aluminate electrolytes. Surface & Coatings Technology, 2015, no. 269, pp. 74–82.
  38. Voevodin A.A., Yerokhin A.L., Lyubimov V.V. et al. Characterization of wear protective Al – Si – O coatings formed on Al-based alloys by micro-arc discharge treatment. Surface & Coatings Technology, 1996, no. 516, pp. 86–87.
  39. Stojadinovic S., Vasilic R., Belca I. Characterization of the plasma electrolytic oxidation of aluminum in sodiumtungstate. Corrosion Science, 2015. no. 52, pp. 250–258.
  40. Kang L., Wenfang L., Guoge Z., Wen Z. Effects of Si phase refinement on the plasma electrolytic oxidation of eutectic Al – Si alloy. Journal of Alloys and Compounds, 2019, no. 790, pp. 650–656.
  41. Gulec A.E., Gencer Y., Tarakci M., The characterization of oxide based ceramic coating synthesized on Al-Si binary alloys by microarc oxidation. Surface & Coatings Technology, 2015, no. 269, pp. 100–107.
  42. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.