Carbon fiber reinforced thermoplastic on the basis of polyetheretherketones
Kirin B.S., Sorokin A.E., Boychuk A.S. Carbon fiber reinforced thermoplastic on the basis of polyetheretherketones // Proceedings of VIAM. 2020. No. 4-5. DOI: 10.18577/2307-6046-2020-0-45-22-31. URL: https://www.viam-works.ru/en/journal/2020/4-5/3
Keywords
polyetheretherketone, carbon fiber reinforced thermoplastic, polymer composite material, pressing carbon plastics.
Abstract
The article is devoted to the development of polymer composite materials (PCMs) based on carbon fabrics of sarge weaving and polyester ether ketones. Film and prepreg technologies for production of thermoplastic PCMs based on polyether ether ketones of foreign manufacture have been tested. Requirements for fluidity of polyether ether ketones for obtaining carbon plastic are formulated. In order to assess the potential of obtained sheet carbon plastics as structural materials, studies were carried out on the defect of their structure and determination of strength characteristics of samples from normal and defective areas.
Reference list
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Komarov G.A. Status, prospects and problems of using PCM in technology. Polimernye materialy, 2009, no. 2, pp. 5–9.
- Kerber M.L., Vinogradov V.M., Golovkin G.S. et al. Polymer composite materials: structure, properties, technology. St. Petersburg: Professiya, 2011, pp. 32–33.
- Petrova G.N., Bader E.Ya. Structural materials based on reinforced thermoplastics. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 30–40.
- Nefedov N.I., Kondrashov E.K., Semenova L.V., Lebedeva T.A. Erosion-resistant coatings for protection of articles from polymer composite materials. Aviacionnye materialy i tehnologii, 2014, no. S3, pp. 25–27. DOI: 10.18577/2071-9140-2014-0-s3-25-27.
- Kraev I.D., Shuldeshov E.M., Platonov M.M., Yurkov G.Yu. Composite materials combining acoustic and radio shielding properties. Aviacionnye materialy i tehnologii, 2016, No. 4 (45), pp. 60–67. DOI: 10.18577/2071-9140-2016-0-4-60-67.
- Gunyaev G.M., Chursova L.V., Komarova O.A., Gunyaeva A.G. Constructional carbon the plastics modified by nanoparticles. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 277–286.
- Beider E.Ya., Petrova G.N., Izotova T.F., Gureeva E.V. Thermoplastic composite materials and foam polyimides. Trudy VIAM, 2013, no. 11, paper no. 01. Available at: http://www.viam-works.ru (accessed: January 20, 2020).
- Bejder E.Ya., Petrova G.N. The thermoplastic binder for polymeric composite materials. Trudy VIAM, 2015, no. 11, paper no. 05. Available at: http://viam-works.ru. (accessed: January 20, 2020). DOI: 10.18577/2307-6046-2015-0-11-5-5.
- Golovkin G.S. Regulation of the mechanical properties of PCM by the methods of targeted formation of the interphase zone. Polimernye materialy, 2009, no. 11, pp. 26–28.
- Sorokin A.E., Bejder E.Ya., Perfilova D.N. Effect of climatic factors on properties of carbon fiber reinforced plastic based on polyphenylenesulfide resin. Trudy VIAM, 2015, no. 1, paper no. 10. Available at: http://www.viam-works.ru (accessed: January 20, 2020). DOI: 10.18577/2307-6046-2015-0-1-10-10.
- Sorokin A.E., Bejder E.Ya., Izotova T.F., Nikolaev E.V., Shvedkova A.K. Investigation of carbon fiber reinforced plastic on polyphenylenesulfide resin after accelerated and natural climatic test. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 66–72. DOI: 10.18577/2071-9140-2016-0-3-66-72.
- Mikhaylin Yu.A. Heat-resistant polymers and polymer materials based on them. St. Petersburg: Professiya, 2006, pp. 33–346.
- Kablov E.N. Trends and guidelines for the innovative development of Russia: coolection of scientific-inform. materials. 3rd ed. Moscow: VIAM, 2015, 720 p.
- Kablov E.N. What to make the future of? Materials of a new generation, technologies for their creation and processing - the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
- Nikolaev A.F. Heat resistant polymers. Leningrad: LTI im. Lensovieta, 1988, pp. 3–11.
- Golovkin G.S. Technological properties of thermoplastic binders for reinforced plastics. Plasticheskiye massy, 2005, no. 1, pp. 35–40.
- Mazhirin P.Yu. Polyphenylene sulfide in the aircraft industry. Polimernyye materialy, 2003, no. 2, pp. 22–24.
- Li J. Effect of silane coupling agent on the tensile properties of carbon fiber-reinforced thermoplastic polyimide. Composites A: Polymer-Plastics Technology and Engineering, 2010, vol. 49, pp. 337–340.
- Trostyanskaya E.B., Stepanova M.I., Rassokhin G.I. Heat resistant linear polymers. Rostov-on-Don: RGASKhM, 2002, pp. 3–22.
- Kablov E.N. Russia needs new generation materials. Redkiye zemli, 2014, no. 3, pp. 8–13.
- Buznik V.M., Kablov E.N. Arctic materials science: current state and prospects. Herald of the Russian Academy of Sciences, 2017, vol. 87, no. 5, pp. 397–408.
- Lazareva T.K., Ermakin S.N., Kostyagina V.A. Problems of creating composite materials based on structural thermoplastics. Uspekhi v khimii i khimicheskoy tekhnologii, 2010, vol. 24, no. 4, pp. 58–63.
- Kablov E.N. Aerospace materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
- Kerber M.L., Vinogradov V.M., Golovkin G.S. Polymer composite materials: structure, properties, technology: textbook. allowance. St. Petersburg: Professiya, 2011, pp. 545–549.
- Jones Fr. A review of interphase formation and design in fiber-reinforced composites. Journal of adhesion Science and Technology, 2010, vol. 24, no. 1, pp. 171–202.
- Drzal L., Raghavendran V. Adhesion of thermoplastic matrices to carbon fibers: effect of polymer molecular weight and fiber surface chemistry. Journal of Thermoplastic Composite Materials, 2003, vol. 16, pp. 21–30.
- Beider E.Ya., Petrova G.N., Dykun M.I. Dressing of carbon fibers – fillers of thermoplastic carbon reinforced plastics. Trudy VIAM, 2014, no. 10, paper no. 03. Available at: http://www.viam-works.ru (accessed: January 20, 2020). DOI: 10.18577/2307-6046-2014-0-10-3-3.
- Thostenson E.T., Chou T.-W. Aligned multi-walled carbon nanotube-reinforced composites: processing and mechanical characterization. Journal of Physics D: Applied Physics, 2002, vol. 35, p. L77–L80.
- Chuang L., Chu N.-J. Effect of polyamic acids on interfacial shear strength in carbon fiber / aromatic thermoplastics. Journal of Applied Polymer Science, 1990, vol. 41, pp. 373–382.
- Sorokin A.E., Petrova G.N. Sizing and dressing in the processes of «liquid-phase» surface modification of coal and fiberglass fillers in the production of structural materials. Overview. Khimicheskaya tekhnologiya, 2019, vol. 20, no. 6, pp. 257–264. DOI: 10.31044/1684-5811-2019-20-6-257-264.
- Sorokin A.E., Petrova G.N., Donskikh I.N. Chemical and electrochemical processing in the processes of «liquid-phase» surface modification of carbon and fiberglass in the production of structural materials (Review). Khimicheskaya tekhnologiya, 2019, vol. 20, no. 7, pp. 316–323. DOI: 10.31044/1684-5811-2019-20-7-316-323.
- Mikhailin Yu.A. Heat-resistant polymers and polymeric materials. St. Petersburg: Professiya, 2006, 624 p.