Studying the effect of silicon carbide particle size on the thermal coefficient linear expansion of the composite material based on aluminum alloy

Nyafkin A.N., Shavnev A.A., Kurbatkina E.I., Kosolapov D.V.
Nyafkin A.N., Shavnev A.A., Kurbatkina E.I., Kosolapov D.V. Studying the effect of silicon carbide particle size on the thermal coefficient linear expansion of the composite material based on aluminum alloy // Proceedings of VIAM. 2020. No. 2. DOI: 10.18577/2307-6046-2020-0-2-41-49. URL: https://www.viam-works.ru/en/journal/2020/2/5
Keywords
highly filled metal composite material, vacuum-compression impregnation of porous blanks, aluminium alloy, silicon carbide, temperature coefficient of linear expansion.
Abstract

A metal composite material (MMC) based on an aluminum cast alloy of the Al–Mg–Cu–Si system containing 65±1% (vol.) silicon carbide and obtained using vacuum compression impregnation technology was developed and studied. Porous preforms with different particle sizes of silicon carbide were obtained by cold compaction followed by melt impregnation of an aluminum alloy. The temperature coefficient of linear expansion (TCLE) was measured in the temperature range from -100 to +400 °С, and the density and volume content of a composite material with various particle sizes of silicon carbide were measured. It was found that with increasing particle size, the TCLE fraction decreases by 15–20% at 20 °C, due to the low content of interphase boundaries of theheterogeneous structure of the composite.

Reference list
  1. Kablov E.N., Shchetanov B.V., Shavnev A.A., Nyafkin A.N. i dr. Increase of reliability of power IGBT-modulus by means of high filled metal matrix composite of Al-SiC system. Aviacionnye materialy i tehnologii, 2010, no. 4, pp. 3–6.
  2. Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metalmatrix composite materials on the basis of Al–SiC. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 373–380.
  3. Kablov E.N., Shchetanov B.V., Shavnev A.A., Nyafkin A.N. et al. Properties and application of a highly filled metal matrix composite material Al–SiC. Tekhnologiya mashinostroyeniya, 2011, no. 3 (105), pp. 5–7.
  4. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Kablov E.N., Chibirkin V.V., Vdovin S.M. Manufacturing, properties and application of the heat-removing bases from Al–SiC MMK in power electronics and converting equipment. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 20–22.
  6. Igarashi T. Characteristics of the flow around a square prism. Bulletin of JSME, 1984, vol. 27, issue 231, pp. 1858–1865. DOI: 10.1299/jsme1958.27.1858.
  7. Crowe C.R., Hasson D.F. Strength Metals and Alloys. Proceedings of the JCSMA-6 (Melbourne, Aug. 16–20, 1982), 1982, vol. 2, pp. 859–862.
  8. Berezhnoy V.L. Technological principles of maximizing strength in the case of production of press quenched Al–Mg–Si alloy extrusions. Light Metal Age, 2000, vol. 58, no. 5-6, pp. 46–53.
  9. Ohori K., Watanabe H., Takeuchi Y. Silicon Carbide Whisker Reinforced Aluminum Composites - Fabrication and Properties. Materials Science and Engineering, 1992, vol. 3, pp. 57–60. DOI: 10.1179 / mst.1987.3.1.57.
  10. Maltseva L.A., Sharapova V.A. Liquid-phase technology for producing composite materials. Matrices. Strengtheners: textbook. Ekaterinburg: Publishing House Ural University, 2013, 120 p.
  11. Nair S.V., Tien J.K., Bates R.C. SiC-reinforced aluminium metal matrix composites // International Metals Reviews. 1985, vol. 30, issue 1, pp. 275–290. DOI: https://doi.org/10.1179/imtr.1985.30.1.275.
  12. Device for identifying user passwords: pat. US 4419389; declared 03.05.88; publ. 30.07.91.
  13. A device for producing products from a metal matrix composite material: pat. 110310 Rus. Federation; filed 31.05.11; publ. 20.11.11.
  14. The method of obtaining products from composite material: pat. 2448808 Rus. Federation; filed 05.10.10; publ. 27.04.12.
  15. ASTM E228. Standard test method for linear thermal expansion of solid materials with a push-rod dilatometer. West Conshohocken, PA: ASTM International, 2017, pp. 1–10. DOI: 10.1520/E0228-17.
  16. ASTM E831. Standard test method for linear thermal expansion of solid materials by thermomechanical analysis. West Conshohocken, PA: ASTM International, 2019, pp. 1–5. DOI: 10.1520/E0831-19.
  17. State Standatd 18898–89 (ISO 2738–87). Powder products. Methods for determining density, oil content and porosity. Moscow: Publishing house of standards, 1990, 10 p.
  18. Nyafkin A.N., Loshchinin Yu.V., Kurbatkina E.I., Kosolapov D.V. Investigation of influence of silicon carbide fractional composition on thermal conductivity of compo-site material based on aluminium alloy. Trudy VIAM, 2019, no. 11 (83), paper no. 06. Available at: http://www.viam-works.ru (accessed: November 22, 2019). DOI: 10.18577/2307-6046-2019-0-11-53-59.
  19. Nyafkin A.N., Grishina O.I., Shavnev A.A., Loshchinin Yu.V., Pakhomkin S.I. The influence of composition of heterogeneous systems with a high of the carbide phase on thermo-physical properties. Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 28–34. DOI: 10.18577/2071-9140-2014-0-s6-28-34.
  20. Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Aluminium casting alloys Trudy VIAM, 2014, no. 4, paper no. 02. Available at: http://www.viam-works.ru (accessed: November 13, 2019). DOI: 10.18577/2307-6046-2014-0-4-2-2.