Application of gas atomization technology to obtain high-quality metal powder compositions for applying atmospheric plasma coatings
Iatsyuk I.V., Artemenko N.I., Doronin O.N., Nerush S.V. Application of gas atomization technology to obtain high-quality metal powder compositions for applying atmospheric plasma coatings // Proceedings of VIAM. 2020. No. 2. DOI: 10.18577/2307-6046-2020-0-2-3-9. URL: https://www.viam-works.ru/en/journal/2020/2/1
Keywords
metal powder composition, gas atomization, atmospheric plasma spraying, nickel alloy.
Abstract
FSUE «VIAM», using gas atomization technology, has mastered the full cycle of producing metal powder compositions (MPC) from alloys of the Ni–Cr–Al–Y system, which are unique materials of a new generation and are applicable in the technology of atmospheric plasma spraying of coatings on critical parts and assemblies, including large ones. The obtained MPC are intended to replace foreign powders, the import of which is limited due to the introduction of economic sanctions against Russia. Studies of the structure and properties of the obtained MPC are carried out. Thermal coatings applied using the obtained MPC are characterized by high uniformity and uniform structure.
Reference list
- Budinovskij S.A., Chubarov D.A., Matveev P.V. Modern methods for deposition of thermal barrier coatings on GTE turbine blades. Aviacionnye materialy i tehnologii, 2014, no. S5, pp. 38–44.
- Khasui A. Spraying technique. Moscow: Mashinostroyeniye, 1975, 288 p.
- Ospennikova O.G., Evgenov A.G., Nerush S.V., Afanasyev-Khodykin A.N. The study of finely dispersed powders of solders on a nickel basis in relation to obtaining high-tech semi-finished product in the form of a self-adhesive tape on an organic binder. Vestnik UGATU, 2012, vol. 16, no. 5 (50), pp. 137–144.
- Nerush S.V., Evgenov A.G. Research of fine-dispersed metal powder of the heat resisting alloy of the EP648-VI brand for laser metal deposition (LMD) and also the assessment quality of welding of powder material on the nickel basis on working blades THP. Trudy VIAM, 2014, no. 3, paper no. 01. Available at: http://www.viam-works.ru (accessed: December 20, 2019). DOI: 10.18577/2307-6046-2014-0-3-1-1.
- Kuklin A.A., Michkova E.S., Bulanov V.Ya. et al. Technology and economics of powder metallurgy. Moscow: Nauka, 1989, 223 pp.
- Kablov E.N., Muboyadzhyan S.A. Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 60–70.
- Kablov E.N., Muboyadzhyan S.A., Budinovsky S.A., Lutsenko A.N. Ion-plasma protective coatings for gas turbine engine blades. Metally, 2007, no. 5, pp. 23–34.
- Kablov E.N., Muboyadzhyan S.A. Protective coatings for turbine blades of prospective gas turbine engines. Gazoturbinnyye tekhnologii, 2001, no. 2 (12). S. 30–32.
- Kolomytsev P.T. Heat resistant diffusion coatings. Moscow: Metallurgiya, 1979, 272 p.
- Kolomytsev P.T. Gas corrosion and the strength of nickel alloys. Moscow: Metallurgiya, 1984, 216 p.
- Abraimov N.V. High temperature materials and coatings for gas turbines. Moscow: Mashinostroyeniye, 1993, 336 p.
- Nikitin V.I. Corrosion and protection of gas turbine blades. Leningrad: Mashinostroyeniye, 1987, 272 p.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.VModern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 97–105.
- Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
- Muboyadzhyan S.A., Kablov E.N., Budinovsky S.A. Vacuum-plasma technology for producing protective coatings from complex alloyed alloys. Metallovedeniye i termicheskaya obrabotka metallov, 1995, no. 2, pp. 15–18.