Paint coatings on the basis of epoxy and acrylic diphasic polymeric system for coloring of elements of cabin of pilots and dashboards

Kuznetsova V.A., Shapovalov G.G., Marchenko S.A., Kovrizhkina N.A., Silaeva A.A.
Kuznetsova V.A., Shapovalov G.G., Marchenko S.A., Kovrizhkina N.A., Silaeva A.A. Paint coatings on the basis of epoxy and acrylic diphasic polymeric system for coloring of elements of cabin of pilots and dashboards // Proceedings of VIAM. 2020. No. 12. DOI: 10.18577/2307-6046-2020-0-12-87-95. URL: https://www.viam-works.ru/en/journal/2020/12/9
Keywords
epoxy and acrylic polymeric matrix, filler, matte coating, adhesion, elasticity, hardness and shine of covering.
Abstract

Influence of the maintenance of filler on adhesion, physicomechanical properties, and also shine of the coverings received on the basis of epoxy and acrylic of film-forming, cured by organic silicon ammine and low-molecular polyamide in initial condition and after artificial aging on the cycle LI-14 (-60D+100) is investigated by °С. Hardness and scratch resistance of systems of coverings on the basis of the developed opaque enamels which in comparison with serial system on the basis of first coat AK-070 and opaque HS-5245 enamel have shown the best results is investigated.

Reference list
  1. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: October 17, 2020). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  2. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  3. Merkulova Yu.I., Kuznetsova V.A., Novikova T.A. Investigation of properties of coating system based on fluorine polyurethane enamel and primer with low toxical pigment content. Trudy VIAM, 2019, no. 5 (77), paper no. 08. Available at: http://www.viam-works.ru. (accessed: September 16, 2020). DOI: 10.18577/2307-6046-2019-0-5-68-75.
  4. Gerasimova L. G., Skorokhodova O.N. Fillers for the paint and varnish industry. Moscow: LKM-press, 2010, 224 p.
  5. Kuleznev V.N. Polymer mixtures (structure and properties). Moscow: Chemistry, 1980, 304 p.
  6. Lipatov Yu.S. Physical chemistry of filled polymers. Moscow: Chemistry, 1977, 603 p.
  7. Poluektova E.A. Wollastonite – a unique paintwork filler. Paints and varnishes and their application, 2012, no. 6, pp. 24–26.
  8. Nazarenko V.V. Anisotropic silicate fillers: special properties in paintwork materials and coatings. Lakokrasochnyye materialy i ikh primeneniye, 2012, no. 1–2, pp. 25–33.
  9. Sosnina S.A., Kuleshova I.D. Regulation of the interaction of components in filled paint and varnish compositions. Lakokrasochnyye materialy i ikh primeneniye, 2011, no. 1–2, pp. 60–62.
  10. Korobschikova T.S., Orlova N.A. Modeling of mechanical properties of paint and varnish material filled with wollastonite. Lakokrasochnyye materialy i ikh primeneniye, 2011, no. 1–2, pp. 62–64.
  11. Strekachinskaya E.S., Verkholantsev V.V., Grozinskaya Z.P. Regularities of delamination of solutions of mixtures of oligomers. Lakokrasochnyye materialy i ikh primeneniye, 1980, no. 4, pp. 13–15.
  12. Muller B., Pot U. Paints and varnishes and coatings. Formulation principles. Moscow: Paint-Media, 2007, 237 p.
  13. Gerasimova L.G., Maslova M.V. Titanium hydroxides and compositions based on them. Receiving, application. Moscow: LKM-press, 2011, 90 p.
  14. Problems of protective coatings: Review of materials of the European conference «Protective coating». Lakokrasochnye materialy i ikh primeneniye, 2013, no. 9, pp. 33–35.
  15. Kablov E.N. Aviation materials science: results and prospects. Vestnik Rossiyskoy akademii nauk, 2002, vol. 72, no. 1, pp. 3–12.
  16. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  17. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  18. Semenova L.V., Malova N.E., Kuznetsova V.A., Pozhoga A.A. Paint and varnish materials and coatings. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 315–327.
  19. Kozlova A.A., Kondrashov Je.K. Systems of paint coatings for anticorrosive protection of magnesium alloys. Aviacionnye materialy i tehnologii, 2014, no. 2, pp. 44–47. DOI: 10.18577/2071-9140-2014-0-2-44-47.
  20. Filichkina V.N. Current state and trends in the development of production and consumption of epoxy resins. Chemical industry abroad: review. inform. Moscow: NIITEKHIM, 1988, is. 8, 18 p.
  21. Moshinsky L.Ya. Epoxy resins and hardeners (structure, properties, chemistry and topology of curing). Tel Aviv, 1995, 370 p.
  22. Kuznetsova V.A., Kuznetsov G.V., Shapovalov G.G. Investigation of epoxy resin molecular mass influence by physiomechanical property and erosive resistant of coatings. Trudy VIAM, 2014, no. 8, paper no. 08. Available at: http://www.viam-works.ru (accessed: November 19, 2020). DOI: 10.18577/2307-6046-2014-0-8-8-8.
  23. Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Marchenko S.A. Ways to improve the properties of paint coatings by adding different fillers (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 41–48. DOI: 10.18577/2071-9140-2019-0-4-41-48.
  24. Kalinskaya T.V., Drinberg A.S., Itsko E.F. Nanotechnology. Application in the paint and varnish industry. Moscow: LKM-press, 2011, 184 p.
  25. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A., Malova N.E. Development of aviation paints and varnishes. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 5, pp. 49–54.