Perspective welding technologies of aluminum-lithium alloy V-1469 applied to fuselage panels

Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S.
Panteleev M.D., Sviridov A.V., Skupov A.A., Odintsov N.S. Perspective welding technologies of aluminum-lithium alloy V-1469 applied to fuselage panels // Proceedings of VIAM. 2020. No. 12. DOI: 10.18577/2307-6046-2020-0-12-35-46. URL: https://www.viam-works.ru/en/journal/2020/12/4
Keywords
laser welding, friction stir welding, fuselage panel, aluminum-lithium alloy V-1469, mechanical properties, welded joints.
Abstract

In this work, we investigated the technological features of promising technologies for laser welding and friction stir welding of high-strength aluminum-lithium alloy V-1469. The modes of laser welding and friction stir welding have been carried out. In this article, we showed the perspective welding methods provide high values of ductility and impact toughness, while the strength of welded joints is not less than 0,8 of the strength of the base material and values of low cycle fatigue is not less than 110·103 cycles. The results allows to propose laser welding and friction stir welding processes as an alternative to riveted joint for aluminum-lithium alloy V-1469 as applied to the elements of the fuselage.

Reference list
  1. Kablov E.N. Materials for aerospace technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, pp. 7–27.
  2. Fridlyander I.N., Drits A.M., Krymova T.V. Possibility of creating weldable alloys based on the Al–Cu–Li system. Metallovedenie i termicheskaya obrabotka metallov, 1991, no. 9, pp. 30–32.
  3. Kablov E.N., Antipov V.V., Klochkova Yu.Yu. Aluminum-lithium alloys of a new generation and layered aluminum-glass-fiber-reinforced plastics based on them. Tsvetnye metally, 2016, no. 8 (884), pp. 86–91. DOI: 10.17580/tsm.2016.08.13.
  4. Skupov A.A. Increase of weldability of alloys of the Al–Cu–Li system by fusion welding methods: thesis abstract, Cand. Sc. (Tech.). Moscow: VIAM, 2019, 21 p.
  5. Grushko O.E., Ovsyannikov B.V., Ovchinnikov V.V. Aluminum-lithium alloys: metallurgy, welding, metallurgy. Moscow: Nauka, 2014, 296 p.
  6. Klochkova Yu.Yu. Formation of the structure and properties of cold-rolled sheets from high-strength aluminum-lithium alloy V-1469: thesis abstract, Cand. Sc. (Tech.). Moscow: VIAM, 2014.17 p.
  7. Khokhlatova L.B., Lukin V.I., Kolobnev N.I. et al. Promising aluminum-lithium alloy 1424 for welded structures of products of aerospace technology. Svarochnoe proizvodstvo, 2009, no. 3, pp. 7–10.
  8. Fridlyander I.N. Memories of the creation of aerospace and nuclear technology from aluminum alloys. Moscow: Nauka, 2006, 287 p.
  9. Elagin V.I., Zakharov V.V. Modern Al-Li alloys and prospects for their development. Metallovedenie i termicheskaya obrabotka metallov, 2013, no. 4, pp. 17–23.
  10. Denisov B.S., Meilakh A.I. Welding in aircraft construction. Welded structures of MiGs. Moscow: Rusavia, 2007, 360 p.
  11. Panteleev M.D. Features of the formation of the structure of welded joints in friction welding with stirring of high-strength aluminum-lithium alloys: thesis abstract, Cand. Sc. (Tech.). Moscow: VIAM, 2019.23 p.
  12. Shalin R.E., Efremov I.S., Yarovinsky Yu.L., Lukin V.I. Experience in the design and manufacture of large-sized structures made of aluminum-lithium alloys for rocket and space technology. Svarochnoe proizvodstvo, 1996, no. 11, pp. 14–18.
  13. Shalin R.E., Efremov I.S., Yarovinskii Yu.U., Lukin V.I. Design and fabrication of large structures of aluminum-lithium alloys for aerospace technology. Welding International, 1997, vol. 11, no. 5, p. 387–392.
  14. Lukin V.I., Kulik V.I., Betsofen S.Ya., Lukina E.A., Sharov A.V., Panteleyev M.D., Samorukov M.L. Friction stir welding of high-strength aluminum-lithium V-1469 alloy semiproducts. Trudy VIAM, 2017, no. 12 (60), paper no. 2. Available at: http://viam-works.ru (accessed: October 14, 2020). DOI: 10.18577/2307-6046-2017-0-12-2-2.
  15. Fridlyander I.N., Fedorovich A.P., Archakova Z.N. et al. Welded aluminum alloys. Metallurgiya, 1969, is. 6, pp. 91–94.
  16. Prasad N.E., Gokhale A.A., Wanhill R.J.H. Aluminum-Lithium Alloys. Processing, Properties, and Applications. Elsevier Inc. 2014, pp. 555–558.
  17. Huang Y. A novel dual-channel weld seam tracking system for aircraft T-joint welds. The International journal of advanced manufacturing technology, 2017, no. 91, pp. 751–761.
  18. Grigoryants A.G., Shiganov I.N., Misyurov A.I. Technological processes of laser processing. Moscow: Publ. house of MSTU im. N.E. Bauman, 2008, 650 p.
  19. Serebrennikova N.Yu., Antipov V.V., Senatorova O.G., Erasov V.S., Kashirin V.V. Hybrid multilayer materials based on aluminum-lithium alloys applied to panels of plane wing. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 3–8. DOI: 10.18577/2071-9140-2016-0-3-3-8.
  20. Han B. Double-sided laser beam welded T-joints for aluminum-lithium alloy aircraft fuselage panels: Effects of filler elements on microstructure and mechanical properties. Optics & Laser Technology, 2017, no. 93, pp. 99–108.
  21. Antipov V.V., Serebrennikova N.Yu., Shestov V.V., Sidelnikov V.V. Laminated hybrid materials on basis of Al–Li alloy sheets. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 212–224. DOI: 10.18577/2071-9140-2017-0-S-212-224.
  22. Hohlatova L.B., Blinkov V.V., Kondratyuk D.I., Ryabova E.N., Kolesenkova O.K. Structure and properties of welded joints of sheets from 1424 and V-1461 alloys made by laser welding. Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 9–13. DOI: 10.18577/2071-9140-2015-0-4-9-13.
  23. Shiganov I.N., Kholopov A.A. Laser welding of aluminum alloys. Fotonika, 2010, no. 3, pp. 6–10.
  24. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  25. Skupov A.A., Panteleev M.D., Ioda E.N. Microstructure and mechanical properties of V-1579 and V-1481 laser welds. Trudy VIAM, 2017, no. 7 (55), paper no. 7. Available at: http://www.viam-works.ru (accessed: October 14, 2020). DOI: 10.18577/2307-6046-2017-0-7-7-7.
  26. Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Peculiarities of high-strength aluminum-lithium alloys laser welding. Trudy VIAM, 2016, no. 10, paper no. 7. Available at: http://www.viam-works.ru (accessed: October 14, 2020). DOI: 10.18577/2307-6046-2016-0-10-7-7.