Metal fibers for new aircraft engine materials

Farafonov D.P., Serov M.M., Patrushev A.Yu., Leschev N.E., Yaroshenko A.S.
Farafonov D.P., Serov M.M., Patrushev A.Yu., Leschev N.E., Yaroshenko A.S. Metal fibers for new aircraft engine materials // Proceedings of VIAM. 2020. No. 12. DOI: 10.18577/2307-6046-2020-0-12-23-34. URL: https://www.viam-works.ru/en/journal/2020/12/3
Keywords
fiber, melt quenching, heat-resistant alloys, sealing materials, porous-fiber materials, sound-absorbing materials, brush seals.
Abstract

Presents the results of work carried out at the Federal state unitary enterprise «VIAM» in the framework of a new material science direction – metallurgy of metal fibers. This work was made possible by the development of a method for producing metal fibers called the hanging melt drop extraction method (EUCR). This method is high-performance and allows you to obtain fibers from almost any material. Research has shown that it is possible to improve the performance and environmental characteristics of modern and advanced engines by introducing new classes of materials based on metal fibers.

Reference list
  1. Inozemtsev A.A., Sandratsky V.L. Gas turbine engines. Perm: Aviadvigatel, 2006, pp. 278–280.
  2. Farafonov D.P., Degovets M.L., Serov M.M. The investigation of the properties and technological parameters producing metallic fibers for abradable sealing materials of aircraft GTE. Trudy VIAM, 2014, no. 7, paper no. 02. Available at: http://viam-works.ru (accessed: August 15, 2020). DOI: 10.18577/2307-6046-2014-0-7-2-2.
  3. Sobolev A.F., Ushakov V.G., Filippova R.D. Sound-absorbing structures of homogeneous type for aircraft engine channels. Acoustic journal, 2009, vol. 55, no. 6, pp. 749–759.
  4. Sun F.G., Chen H.L., Wu J.H., Feng K. Sound absorbing characteristics of fibrous metal materials at high temperatures. Applied Acoustics, 2010, vol. 711, pp. 221–235. DOI: 10.1016/J.APACOUST.2009.09.001.
  5. Felten E.J. Use of platinum and rhodium to improve oxide adherence on Ni–8Cr–6Al alloys. Oxidation of Metals, 1976, vol. 10, no. l, pp. 23–28.
  6. Allam I.M., Akuezue H.C., Whittle D.P. Influence of Small Pt Additions on Al2O3 Scale Adherence. Oxidation of Metals, 1980, vol. 14, no. 6, pp. 517–530. DOI: 10.1007/BF00611696.
  7. Fei W., Kuiry S.C., Seal S. Inhibition of Metastable Alumina Formation on Fe–Cr–Al–Y Alloy Fibers at High Temperature Using Titania Coating. Oxidation of Metals, 2004, vol. 62, is. 1–2, pp. 29–44. DOI: 10.1023/B: OXID.0000038784.73316.A4.
  8. Smarsly W., Zheng N., Buchheim C.S. et al. Advanced High Temperature Turbine Seals Materials and Designs. Material Science Forum, 2005, vol. 492–493, pp. 21–26. DOI: 10.4028/www.scientific.net/MSF.492-493.21.
  9. Heidloff A.J., Tang Z., Zhang F., Gleeson B.C. A combined mapping process for the development of platinum-modified Ni-based superalloys. The Journal of the Minerals, 2010, vol. 62, pp. 48–53. DOI: 10.1007/s11837-010-0156-x.
  10. Ballard D.L., Plichak A.L. The use of precious-metal-modified Nickel-based superalloys for thin gage apllications. The Journal of the Minerals, 2010, vol. 62, pp. 45–47.
  11. Amano T., Takezawa Y., Shiino A., Shishido T. Surface morphology of scale on FeCrAl (Pd, Pt, Y) alloys. Journal of alloys and Compounds, 2008, vol. 452, is. 1, pp. 16–22. DOI: 10.1016/J.Jallcom.2007.01.170.
  12. Amano T. High-temperature oxidation of FeCrAl (Y, Pt) alloys in oxygen-water vapor. Materials at high temperatures, 2011, vol. 28, is. 4, pp. 342–348. DOI: 10.3184/096034011X13190156331030.
  13. Amano T. High-temperature oxidation resistance of Al2O3-forming heat-resisting alloys with noble metal and rare earth additions. Materials and Corrosion, 2011, vol. 62, no. 7, pp. 659–667. DOI: 10.1002/MACO.201005855.
  14. Migunov V.P., Farafonov D.P. Research of the main operational properties of new class of sealing materials for flowing path of GTE. Aviacionnye materialy i tehnologii, 2011, no. 3, pp. 15–20.
  15. Buznik V.M., Kablov E.N. Arctic materials science: current state and prospects. Herald of the Russian Academy of Sciences, 2017, vol. 87, no. 5, pp. 397–408.
  16. Simms N.J., Norton J.F., McColvin G. Performance of candidate gas turbine abradeable seal materials in high temperature combustion atmospheres. Materials and Corrosion, 2005, vol. 56, pp. 765–777. DOI: 10.1002/maco.200503877.
  17. Afanasev-Khodykin A.N., Rylnikov V.S., Farafonov D.P. Technology soldering porous fibrous material of the alloy of the «fehral» to seal the flow part of GTE. Trudy VIAM, 2014, no. 1, paper no. 02. Available at: http://www.viam-works.ru (accessed: August 15, 2020). DOI: 10.18577/2307-6046-2014-0-1-2-2.
  18. Farafonov D.P., Migunov V.P., Sarayev A.A., Leshchev N.E. Abradability and erosion resistance of seals in turbine engine air-gas channel. Trudy VIAM, 2018, no. 8 (68), paper no. 7. Available at: http://www.viam-works.ru (accessed: August 17, 2020). DOI: 10.18577/2307-6046-2018-0-8-70-80.
  19. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRM and MI. Kompetentnost, 2017, no. 2 (143), pp. 40–46.
  20. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  21. Shuldeshov E.M., Kraev I.D., Petrova A.P. Polymeric sound-absorbing material design for environmental noise abatement of aircraft engines. Trudy VIAM, 2018, no. 2, paper no. 06. Available at: http://www.viam-works.ru (accessed: August 31, 2020). DOI: 10.18577/2307-6046-2018-0-2-6-6.
  22. Mahaptara R.N., Varma S.K., Lei C.S. Thermal Stability and Oxidation Resistance of Pt–10Al–4Cr Alloy at Super-High Temperatures. Oxidation of Metals, 2006, vol. 66, no. 3/4, pp. 127–135. DOI: 10.1007/s11085-006-9020-3.
  23. Odusote J.K., Cornish L.A., Chown L.H., Erasmus R.M. Isothermal Oxidation Behavior of a Two-Phase γ. Precipitation-Hardened Quaternary Pt-Based Alloys in Air at 1,350°С. Oxidation of Metals, 2012, vol. 78, pp. 123–143. DOI: 10.1007/s11085-012-9295-5.
  24. Shuldeshov E.M. Sound-proof properties of aviation heatsound-proof materials. Trudy VIAM, 2019, no. 12 (84), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 27, 2020). DOI: 10.18577/2307-6046-2019-0-12-37-45.
  25. Borisov B.V. Development of a technology for producing fibers and porous materials from heat-resistant alloys by extracting a hanging drop of the melt: thesis,. Cand. Sc. (Tech.). Moscow: Moscow. Aviation Tech. Inst., 2011, pp. 21–25.
  26. Letnikov M.N., Lomberg B.S., Ospennikova O.G., Bakradze M.M. The influence of quench rate on microstructure and mechanical properties of nickel-based wrought superalloy VZh175-ID. Aviacionnye materialy i tehnologii, 2019, No. 2 (55), pp. 21–30. DOI: 10.18577/2071-9140-2019-0-2-21-30.