Methods of physical vapor deposition for the manufacture of metal matrix composites (review)

Zhabin A.N., Nyafkin A.N., Serpova V.M., Krasnov E.I.
Zhabin A.N., Nyafkin A.N., Serpova V.M., Krasnov E.I. Methods of physical vapor deposition for the manufacture of metal matrix composites (review) // Proceedings of VIAM. 2020. No. 11. DOI: 10.18577/2307-6046-2020-0-11-68-75. URL: https://www.viam-works.ru/en/journal/2020/11/8
Keywords
metal matrix composite, magnetron sputtering, electron beam deposition, silicon carbide fibers, composite material, fiber, silicon carbide, physical vapor deposition.
Abstract

A review of the scientific and technical literature in the field of the most used methods of physical vapor deposition for the manufacture of metal matrix composites (MMCs) reinforced silicon carbide fibers is presented. The most widespread methods of solid-phase technology for the manufacture of MMCs are briefly considered, and methods of electron-beam deposition and magnetron sputtering of a matrix titanium alloy on silicon carbide fibers are discussed in detail. The morphological structure of the surface of the deposited matrix alloy on fibers, obtained by different methods, is investigated.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
  3. Kablov E.N. There is no future without new materials. Metallurg, 2013, no. 12, pp. 4–8.
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2071-9140-2017-0-S-186-194.
  6. Chubarov D.A., Budinovskiy S.A., Smirnov A.A. Magnetron sputtering method for applying ceramic layers for thermal barrier coatings. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 23–30. DOI: 10.18577/2071-9140-2016-0-4-23-30.
  7. Serpova V.M., Kosolapov D.V., Zhabin A.N., Shavnev A.A. Methods for forming semi-finished products for the production of continuous fiber reinforced metal matrix composites (review). Trudy VIAM, 2017, no. 7 (55), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 8, 2020). DOI: 10.18577/2307-6046-2017-0-7-8-8.
  8. Subramanian P.R., Krishnamurthy S., Keller S.T., Mendiratta M.G. Processing of continuously reinforced Ti-alloy metal matrix composites (MMC) by magnetron sputtering. Materials Science and Engineering, A, 1998, vol. 244, pp. 1–10.
  9. Ma Z., Yang Y., Du J. et al. The effect of magnetron sputter parameter on fiber coating character. Materials Letters, 2004, vol. 58, pp. 2118–2121.
  10. Leucht R., Dudek H. J. Properties of SiC-fiber reinforced titanium alloys processed by fiber coat-ing and hot isostatic pressing. Materials Science and Engineering, A, 1994, vol. 188, pp. 201–210.
  11. Zhang W., Yang Y.Q., Zhao G.M. et al. Microstructure evolution of TiAl matrix in the process of magnetron sputtering and hot isostatic pressing for fabricating TiAl/SiCf composites. Intermetallics, 2013, vol. 39, pp. 5–10.
  12. Xu K., Yumin W., Qing Y. et al. Enhanced effect of matrix growth texture on the longitudinal modulus of a titanium matrix composite prepared from magnetron sputtering. Materials Letters, 2019, vol. 245, pp. 37-40.
  13. Rastogi R.S., Pourrezaei K. Deposition, characterization, thermo-chemical compatibility and failure analysis of multi-layer coated silicon-carbide fiber-reinforced metal-matrix composites. Journal of Materials Processing Technology, 1994, vol. 43, pp. 89-107.
  14. Zhang R., Zhang Y., Liu Q. et al. Effect of a ductility layer on the tensile strength of TiAl-based multilayer composite sheets prepared by EB-PVD. Materials Characterization, 2014, vol. 95, pp. 157-163.
  15. Movchan B.A., Lemkey F.D. Some approaches to producing microporous materials and coatings by EBPVD. Surface and Coatings Technology, 2003, vol. 165, pp. 90–100.
  16. Wood M., Ward-Close M. Fiber-reinforced intermetallic compounds by physical vapor deposition. Materials Science and Engineering, A, 1995, vol. 192-193, pp. 590–596.
  17. Chawla V., Jayaganthan R., Chawla A.K., Chandra R. Morphological study of magnetron sput-tered Ti thin films on silicon substrate. Materials Chemistry and Physics, 2008, vol. 111, pp. 414–418.
  18. Zhang H., Liu L., Pei Z. et al. An effective strategy towards construction of CVD SiC fiber-reinforced superalloy matrix composite. Journal of Materials Science & Technology, 2020, vol. 49, pp. 179–185.