Decoratively finishing materials for wall panels of passenger cab and the crew cockpit of air vehicles (review)

Shuldeshov Е.М., Nazarov I.A., Ivanov M.S., Donskih I.N.
Shuldeshov Е.М., Nazarov I.A., Ivanov M.S., Donskih I.N. Decoratively finishing materials for wall panels of passenger cab and the crew cockpit of air vehicles (review) // Proceedings of VIAM. 2020. No. 11. DOI: 10.18577/2307-6046-2020-0-11-38-47. URL: https://www.viam-works.ru/en/journal/2020/11/5
Keywords
decorative films, decorative laminate materials, fire safety, surface density, multi-layer material, way of manufacturing.
Abstract

Questions of development of decorative and finishing materials for wall panels of passenger cab and the crew cockpit of air vehicles in the Russian Federation and abroad are considered. The structure and structure of such materials are described, examples of implementation of their different options are given. The main ways of manufacturing of materials, and also requirements to them which performance is necessary for the admission to application in aviation engineering, and the requirements providing competitive advantage of materials in comparison with analogs are provided. The main directions of development of decorative and finishing materials are evaluated.

Reference list
  1. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577 / 2071-9140-2020-0-1-3-11.
  2. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α+β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  3. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  4. Shuldeshova P.M., Zhelezina G.F. An influence of atmospheric condition and dust loading on properties of structural organic plastics. Aviacionnye materialy i tehnologii, 2014, no. 1, pp. 64–68. DOI: 10.18577/2071-9140-2014-0-1-64-68.
  5. Lexan F6000. Available at: www.sabic.com (accessed: May 18, 2020).
  6. Nesterova T.A., Barbotko S.L., Nikolaeva M.F., Gerter Yu.A. Multi-layer protective and decorative material for decorating details in the cabin of aircraft and helicopters. Trudy VIAM, 2013, no. 8, paper no. 04. Available at: http://www.viam-works.ru (accessed: May 18, 2020).
  7. Decorative-sheet manufacturing method: pat. US2017217145А1; filed 21.10.15; publ. 03.08.17.
  8. Decorative multilayer material: pat. RU141769U1; filed 28.08.13; publ. 10.06.14.
  9. Product decorative laminates: pat. FR2380879A1; filed 18.02.77. publ. 15.09.78.
  10. Decorative element and decorative item: pat. RU65530U1; filed 09.03.07; publ. 10.08.07.
  11. Decorative layered material and method of obtaining it (options): pat. RU2151063C1; filed 09.07.99; publ. 20.06.00.
  12. Flexible laminate for coating and protection of surfaces, and manufacturing method of the same: pat. US2005042438A1; filed 24.09.03; publ. 24.02.05.
  13. Soft decorative film and UV coating technology and application thereof: pat. CN107471788 (A); filed 07.06.16; publ. 15.12.17.
  14. Coating mechanism of base layer in PVC decorative film forming device: pat. CN209502108 (U); filed 14.01.19; publ. 18.10.19.
  15. Laminate film made of polyolefin-based resin: pat. JP2004002825A; filed 18.04.03; publ. 08.01.04.
  16. Composite system of nano protective film, PVC decorative layer and aluminum-manganese alloy layer and composite method of composite system: pat. CN109334014 (A); filed 15.11.18; publ. 15.02.19.
  17. Decorative film and method for producing same and decorated molded article: pat. US2019077134А1; filed: 23.05.16; publ. 14.03.19.
  18. Decorative and finishing coatings that imitate the texture and relief of natural or artificial ornamental stones, shell rock or wood of various species: pat. RU2004133200A; filed 15.11.04; publ. 20.04.06.
  19. A method of obtaining a protective coating on materials and products made of polycarbonate: pat. RU2561406C1; filed 05.05.14; publ. 27.08.15.
  20. Decorative laminate: pat. RU2039661C1; filed 05.03.92; publ. 20.07.95.
  21. Means of transport having a film for the coating of at least one of its surfaces: pat. WO2014/114566A1; filed 17.01.14; publ. 31.07.14.
  22. Film from polyester resin for lamination of decorative material: pat. TW537962B; filed 30.11.99; publ. 21.06.03.
  23. Bondable and tape/label-releasable top-coated overlays useful in the manufacture of decorative laminate panels: pat. US 5985595; filed 24.03.97; publ. 28.09.99.
  24. Embossed reflective laminates: pat. US2003161997A1; filed 16.01.03; publ. 28.08.03.
  25. Laminate floor panel: pat. EP2263867A1; filed 13.07.09; publ. 22.12.10.
  26. Designed coating film: pat. JP09169933A; filed 19.12.95; publ. 30.06.97.
  27. Laminated film or sheet substituted for coating, method for manufacturing the same, and laminate including laminated film or sheet substituted for coating: pat. JP2003034006A; filed 17.05.02; publ. 04.02.03.
  28. Protective and decorative coating of a non-metallic product: pat. RU49738U1; filed 28.03.05; publ. 10.12.05.
  29. Laminate film for decorating molded article, paint composition and decorative molded article: pat. JP2015145103 (A); filed 03.02.14; publ. 18.03.15.
  30. Multilayer laminate having amorphous fluororesin coating film formed on water-repellent surface: pat. JP2016150584А; filed 19.02.15; publ. 22.08.16.
  31. A method of producing films with a layer of mixtures of fluoropolymers and polyacrylates: pat. RU2254238C2; filed 03.12.99; publ. 20.06.05.
  32. Method of applying fluoropolymer coatings for surface protection: pat. RU2394860C1; filed 24.10.08; publ. 20.07.10.
  33. Laminate film for decorating three-dimensional molded article for vacuum molding, method for decorating three-dimensioanal molded article and decorative molded article: pat. JP2017007109А; filed 17.06.15; publ. 12.01.17.
  34. Laminated polyester film: pat. JP2012223984A; filed 20.04.11; publ. 15.11.12.
  35. Multilayer film: pat. RU2381104C2; filed 09.06.05; publ. 10.02.10.
  36. Wiping coating method: pat. JP0833866A; filed 22.07.94; publ. 06.02.96.
  37. Barbotko S.L. Fire safety of aviation materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 431–439.
  38. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Assessment of fire safety of polymer materials for aviation purposes: state analysis, test methods, development prospects, methodological features: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2018, 424 p.
  39. Volny O.S., Kirienko O.A., Shurkova E.N., Barbotko S.L. Investigation of the influence of operational factors on the fire safety characteristics of decorative and finishing polymer materials for aviation purposes. Sovremennyye tekhnologii obespecheniya grazhdanskoy oborony i likvidatsii posledstviy chrezvychaynykh situatsiy, 2015, no. 1-1 (6), pp. 69–72.
  40. Polyvinyl chloride of reduced combustibility, including organophosphorus polymers containing organophosphorus fragments, and a method for their preparation: pat. RU2385327C1; filed 04.08.08; publ. 27.03.10.
  41. Decorative laminates incorporating flame retardant engineering thermoplasticfilms: pat. US2010/0272976A1; filed. 27.04.10, publ. 28.10.10.
  42. Decorative film having low gross heat of combustion: pat. US2014/0322473A1; filed 30.09.11; publ. 30.10.14.
  43. Decorative laminate with graffiti resistance and improved combustion reaction properties: pat. US7939163B2; filed 03.05.05; publ. 10.05.11.
  44. NF P 92-501/NF992-501: M classification combustion test. Available at: www.rssp.ru (accessed: May 18, 2020).
  45. NF F 16-101/102: Fire testing to railway components. Available at: www.rssp.ru (accessed: May 18, 2020).
  46. NF F 31-112: Protection in relation to graffiti – test procedures and methods of valuation. Available at: www.rssp.ru (accessed: May 18, 2020).
  47. Soft touch laminates constructed with improved fire retardant properties for transportation: pat. US9492988B2; filed 14.05.14; publ. 15.11.16.
  48. Integrated lavatory pan for commercial aircraft: pat. US2013/0099055A1; filed 24.10.85; publ. 25.04.13.
  49. Dimensionally stable laminate with removable web carrier and method of manufacture: pat. US7052761B2; filed 22.04.04; publ. 30.05.06.
  50. Blade coating type PVC decorative film for ceramic substrate surface: pat. CN107629235 (A); filed 14.07.16; publ. 26.01.18.
  51. Decorative sheet and decorative element in which it is applied: pat. RU2618885C1; filed 17.03.15; publ. 11.05.17.
  52. Damage resistant decorative laminate having excellent appearance and cleanability and production method thereof: pat. JP05237972А; filed 19.06.92; publ. 17.09.93.
  53. Decorative article and process for producing the same: pat. US6025064A; filed 12.01.98; publ. 15.02.00.
  54. Scratch and wear resistant coatings on polymer surfaces: pat. RU2009100625A; filed 09.05.07; publ. 20.07.10.
  55. Decorative film: pat. RU2230671C2; filed 04.04.00; publ. 20.06.04.
  56. Three-layer UV protection film for decorative high pressure laminates (hpl): pat. RU2687941C2; filed 19.05.15; publ. 16.05.19.
  57. Polyurethane compositions, films and methods: pat. RU2682551 C2; filed 23.03.15; publ. 19.03.19.
  58. Anti-microbial decorative laminate: pat. СA3050774A1; filed 10.08.18; publ. 10.02.20.
  59. Magina S., Santos M.D., Ferra J. et al. High pressure laminates with antimicrobial properties. Materials (Basel), 2016, vol. 9 (2). Available at: ncbi.nlm.nih.gov/pmc (дата обращения: 18.05.2020). DOI: 10.3390/ma9020100.
  60. Coating film laminate: pat. JP2007290377A; filed 26.03.07; publ. 08.11.07.
  61. Coating composition and coated decorative member: pat. JP2001072924A; filed 03.09.99; publ. 21.03.01.
  62. Extruded polymeric high transparency films: pat. US2001052385A1; filed 03.07.01; publ. 20.12.01.
  63. Extruded polymeric high transparency films: pat. US2008113148; filed 05.09.07; publ. 15.05.08.
  64. Yellowing-resistant decorative film for coating a holder, in particular a component of an automobile or a piece of furniture, with a coating compound comprising at least one bar-rier coating and a decorative coating: pat. EP2556966А1; filed 12.08.11; publ. 13.02.13.
  65. Decorative film for use in plastics molding, process for preparing the same and injection-molded part by use of the same: pat. US6444317B1; filed 06.08.99; publ. 03.09.02.
  66. Balamurugan G., Pukadyil R., Nielsen K. et al. Role of a micro-patterned adhesive interface on the performance of thermoformable multi-layered decorative polymeric film laminates. International Journal of Adhesion and Adhesives, 2013, vol. 44, pp. 78–90.
  67. Decorative molden product and method for manufacturing same: pat. JP2006315330A; filed: 13.05.05; publ. 24.11.06.
  68. Multilayer Composition, Film, and Related Methods: pat. RU2628388C2; filed 28.08.12; publ. 16.08.17.
  69. Kimura T., Aoki S. Aplication of silk composite to decorative laminate. Advanced Composite Materials, 2007, vol. 16, is. 4, p. 349–360.
  70. Decorative sheet and manufacture thereof: pat. JP04128041А; filed 19.09.90; publ. 28.04.92.
  71. Preparation of laminated composite substrares using coated oriented polymeric film: pat. WO2008/002360 A1; filed 15.05.07; publ. 03.01.08.
  72. Aerfilm LHR. Available at: http://www.schneller.com (accessed: May 18, 2020).