Application of the active brazing method for connecting fiber materials with ceramic materials (review)

Krasnov E.I., Kurbatkina E.I., Shavnev A.A., Serpova V.M., Zhabin A.N.
Krasnov E.I., Kurbatkina E.I., Shavnev A.A., Serpova V.M., Zhabin A.N. Application of the active brazing method for connecting fiber materials with ceramic materials (review) // Proceedings of VIAM. 2020. No. 10. DOI: 10.18577/2307-6046-2020-0-10-63-72. URL: https://www.viam-works.ru/en/journal/2020/10/7
Keywords
fiber composite material based on titanium alloys, aluminum oxide ceramics Al2O3, zirconium dioxide ceramics ZrO2, brazing, titanium alloy, connecting zone, reaction layer
Abstract

Рresents a review of the application of the active brazing method for joining fibrous compo-site materials based on titanium alloy with ceramics based on aluminum oxide and zirconium dioxide. The basic problem arising from the combination of metals and ceramics, examples of solving problems compounds represented by the relationship of the microstructure of the connection zone with mechanical properties and shows the effect of additives Ti, B and W on microstructure and mechanical properties. Conclusions are made about the possibility of obtaining high-quality and durable compounds and factors affecting them.

Reference list
  1. Dai J., Zhu J., Chem C., Weng F. High temperature oxidation behavior and research status of modifications on improving high temperature oxidation resistance of titanium alloys and titanium aluminides: A review. Journal of Alloys and Compounds, 2016, vol. 685, pp. 784–798. DOI: 10.1016/j.jallcom.2016.06.212.
  2. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  3. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  4. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: June 2, 2020). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  6. Kablov E.N. Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations. Kryliya Rodiny, 2016, no. 5, pp. 8–18.
  7. Hayat M.D., Singh H., He Z., Cao P. Titatium metal matrix composites: An overiew. Composites, part A: Applied Science and Manufacturing, 2019, vol. 121. P. 418–438. DOI: 10.1016/j.compositesa.2019.04.005.
  8. Smith P.R., Graves J.A., Rhodes C. Comparison of orthorhombic and alpha-two titanium aluminides as matrices for continuous SiC-reinforced composites. Metallurgical Materials Transaction A, 1994, vol. 25A, pp. 1267–1283. DOI: 10.1007/BF02652301.
  9. Aldinger F., Weberruss V.A. Advanced Ceramics and Future Materials: An Introduction to Structures, Properties, Technologies, Methods. Weinheim: WILEY-VCH Verlag GmbH & Co KGaA, 2010, pp. 170–260.
  10. Richerson D.W., Lee W.E. Composites Manufacturing. Modern Ceramic Engineering: Properties, processing, and Use in Design, Composites Manufacturing, 2018, vol. 5, is. 1, pp. 58–59. DOI: 10.1016/0956-7143(94)90021-3.
  11. Micari F., Buffa G., Pellegrino S., Fratini L. Friction Stir Welding as an Effective Alternative Technique for Light Structural Alloys Mixed Joints. Proceedings of 11th International Conference on Technology of Plasticity, 2014, vol. 81, pp. 74–83. DOI:10.1016/j.proeng.2014.09.130.
  12. Darsell J.T., Weil K.S. High temperature strength of YSZ joints brazed with palladium silver copper oxide filler metals. International Journal of Hydrogen Energy, 2011, vol. 36, is. 7, pp. 4519–4524.
  13. Si X.Q., Cao J., Song X.G. et al. Reactive air brazing of YSZ ceramic with novel Al2O3 nanoparticles reinforced Ag–CuO–Al2O3 composite filler: micro-structure and joint properties. Materials and Design, 2017, vol. 114, pp. 176–184.
  14. Wakelkamp W., van Loo F., Metselaar R. Phase relation in the Ti–Si–C system. Journal of the European Ceramic Society, 1991, vol. 8, p. 135–139.
  15. Mizuhara H., Huebel E., Oyama T. High-reliability joining of ceramic to metal. American Ceramic Society Bulletin, 1989, vol. 68, is. 9, pp. 1591–1599.
  16. Uday M.B., Ahmad-Fauzi M.N., Noor A.M., Rajoo S. Current Issues and Problems in the Joining of Ceramic Metal. Materials Science, 2016. P. 169–175. DOI: 10.5772/64524.
  17. Nakahashi M. Joining of ceramics to metals (1): Interfacial reactions between ceramics and metals. Welding International, 1996, vol. 10, is. 10, pp. 765–770.
  18. Yang Z., Lin J., Wang Y., Wang D. Characterization of microstructure and mechanical properties of Al2O3/TiAl joints vacuum-brazed with Ag–Cu–Ti+W composite filler. Vacuum, 2017, vol. 143, pp. 294–302.
  19. Niu G.B., Wang D.P., Yang Z.W., Wang Y. Microstructure and mechanical properties of Al2O3 ceramic and TiAl alloy joints brazed with Ag–Cu–Ti filler metal. Materials Science Ceramics International, 2016, vol. 42, pp. 6924–6934.
  20. Qiu Q., Wang Y., Yang Z., Wang D. Microstructure and mechanical properties of Al2O3 ceramic and Ti6Al4V alloy joint brazed with inactive Ag–Cu and Ag–Cu+B. Journal of the European Ceramic Society, 2016, vol. 36, pp. 2067–2074. DOI: 10.1016/J.CERAMINT.2016.01.078.
  21. Feng J., Dai X., Wang D. et al. Microstructure evolution and mechanical properties of ZrO2/TiAl joints vacuum brazed by Ag–Cu filler metal. Materials Science and Engineering A, 2015, vol. 639, pp. 739–746.
  22. Dai X., Cao J., Liu J. et al. Effect of holding time on microstructure and mechanical properties of ZrO2/TiAl joints brazed by Ag–Cu filler metal. Materials and Design, 2015, vol. 87, pp. 53–59.
  23. Dai X., Cao J., Wang Z. et al. Brazing ZrO2 ceramic and TC4 alloy by novel WB reinforced Ag–Cu composite filler. Microstructure and properties. Ceramics International, 2017, vol. 43, pp. 15296–15305.