Obtaining of experimental constructionally similar sample of the nozzle assembly sector and carrying out its tests at temperature of 1500 °С
UDC
666.3:620.1
DOI
10.18577/2307-6046-2020-0-10-51-62
Article PDF (Russian)
(1005.97 KB)
How to cite
Lebedeva Yu.E., Afanasiev-Khodykin A.N., Prokopchenko G.M., Shavnev A.A., Serebryakov D.I. Obtaining of experimental constructionally similar sample of the nozzle assembly sector and carrying out its tests at temperature of 1500 °С // Proceedings of VIAM. 2020. No. 10. DOI: 10.18577/2307-6046-2020-0-10-51-62. URL: https://www.viam-works.ru/en/journal/2020/10/6
Keywords
ceramic composite material, silicon carbide, nozzle assembly sector, alloy EP648, soldering, high temperature tests.
Abstract
The interaction of the SiC–SiCw–B4C–AlN system ceramic composite material (CCM) with the EP648 alloy in the process of high-temperature brazing was studied. The smallest erosion activity both in relation to CCM, and to the EP648 alloy, has HMP solder VPr50. An experimental constructionally similar sample of the nozzle assembly sector was made using uncooled nozzle blade prototypes from CCM. Tests of an experimental constructionally similar sample of the nozzle assembly sector at a temperature of 1500 °C were carried out. No traces of material ablation from the surface of the CMC were found.
Reference list
- Lukin V.I., Rilnikov V.S., Afanasyev-Khodykin A.N. Nickel-based solders for soldering heat-resistant alloys and steels. Svarochnoe proizvodstvo, 2014, no. 7, pp. 36–42.
- Efimochkin I.Yu., Fedotov S.V., Rilnikov V.S., Afanasiev-Khodykin A.N. High-temperature solders obtained by mechanical alloying. Svarochnoe proizvodstvo, 2015, no. 3, pp. 25–28.
- Ospennikova O.G., Lukin V.I., Afanasyev-Khodykin A.N., Galushka I.A., Shevchenko O.V. Advanced developments in the field of the high-temperature soldering of heat resisting alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 144–158. DOI: 10.18577/2071-9140-2017-0-S-144-158.
- Kablov E.N., Folomeykin Yu.I., Stolyarova V.L., Lopatin S.I. Processes of interaction of niobium-silicon melt with refractory ceramics. Zhurnal Obshchey Khimii, 2016, vol. 86, no. 9, pp. 1542–1546.
- Evdokimov S.A., Shchegoleva N.E., Sorokin O.Yu. Ceramic materials aviation engineering (review). Trudy VIAM, 2018, no. 12 (72), paper no. 06. Available at: http://www.viam-works.ru (accessed: January 09, 2020). DOI: 10.18577/2307-6046-2018-0-12-54-61.
- Krenkel W., Berndt F. C/C–SiC composites for space applications and advanced friction systems. Materials Science and Engineering A, 2005, vol. 412, no. 1-2, pp. 177–181.
- Jacobson N.S. Corrosion of silicon-based ceramics in combustion environments. Journal of European Ceramic Society, 1993, vol. 76, pp. 3–28.
- Van Roode M., Price J., Miriyala N., Leroux D. Ceramic matrix composite combustor liners: A summary of field evaluations. Journal of Engineering for Gas Turbines and Power, 2007, vol. 129, no. 1, pp. 21–30.
- Choi S.R., Bansal N.P. Shear Strength as a Function of Test Rate for SiCf / BSAS Ceramic Matrix Composite at Elevated Temperature. Journal of American Ceramic Society, 2004, vol. 87, no. 10, pp. 1912–1918.
- Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.St. Perspective high-temperature ceramic composite materials. Russian Journal of General Chemistry, 2011, vol. 81, no. 5. P. 986–991.
- Ceramic matrix composite and method of manufacturing the same: pat. US 5990025 A; filed 28.03.97; publ. 23.11.99.
- Naslain R.R. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview. Composites Science and Technology, 2004, vol. 64, pp. 155–170.
- Karimbaev T.D., Mezentsev M.A., Yezhov A.Yu. Development and experimental research of non-metallic parts and assemblies of the hot part of a promising gas turbine engine. Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta, 2015, vol. 14, no. 3-1, pp. 128–138.
- Corman G. Melt infiltrated ceramic matrix composites for shrouds and combustor liners of advanced industrial gas turbines: Final Report. New York, 2010. 503 p.
- Corman G. Melt infiltrated composites (HIPERCOMP) for gas turbine engine applications. New York, 2005.499 p.
- Corman G., Upadhyay R., Sinha S. et al. General Electric company: selected applications of ceramics and composite materials. Materials Research for Manufacturing, 2016. P. 59–91.
- Shaoming D. Preparation of SiC/SiC composites by hot pressing, using Tyranno-SA fiber as reinforcement. Journal of American Ceramic Society, 2003, vol. 86, no. 1, p. 26–32.
- Kablov E.N., Karachevtsev F.N., Stolyarova V.L., Vorozhtcov V.A., Lopatin S.I. Vaporization and thermodynamics of ceramics in the Y2O3–ZrO2–HfO2 system. Rapid Communications in Mass Spectrometry, 2019, vol. 33, no. 19, pp. 1537–1546.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Ceramic composite material: pat. 2689947 Rus. Federation; filed 25.04.18; publ. 29.05.19.
- Torresillas S.M.R., Solis P.N.V., Okunkova A.A., Peretyagin P.Yu. Fundamentals of the process of spark plasma sintering of nanopowders. Moscow: Tekhnosfera, 2014.96 p.
- Khasanov A.O. Development of compositions and technology for spark-plasma sintering of ceramic materials, composites based on micro- and nanopowders B4C: thesis, Cand. Sc. (Tech.). Tomsk, 2015. 201 p.
- Chuvildeev V.N., Boldin M.S., Nokhrin A.V. et al. Structure and properties of advanced materials obtained by Spark Plasma Sintering. Acta Astronautica, 2015, vol. 109, pp. 172–176.
- Chuvildeev V.N., Boldin M.S., Dyatlova Ya.G. et al. Comparative study of hot pressing and high-speed electropulse plasma sintering of Al2O3/ZrO2/Ti (C, N) powders. Russian Journal of Inorganic Chemistry, 2015, vol. 60, no. 8, pp. 987–993.
- Avramenko V.A., Papynov E.K., Shichalin O.O. et al. Spark plasma sintering as an innovative approach to the creation of new generation nanostructured ceramics. Nanomaterials and technologies: collection of articles. tr. VI Int. conf. «Nanomaterials and Technologies», V Int. conf. on materials science and II Intern. conf. on functional materials. Ulan-Ude, 2016, pp. 82–90.
- Barinov V.Yu., Rogachev A.S., Vadchenko S.G., Moskovskikh D.O., Kolobov Yu.R. Spark plasma sintering of complex-shaped objects using quasi-isostatic pressing. Mezhdunarodniy zhurnal prikladnykh i fundamentalnykh issledovaniy, 2016, no. 1–3, pp. 312–315.
- Vaganova M.L., Sorokin O.Yu., Osin I.V. Joining of ceramic materials by the method of spark plasma sintering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 306–317. DOI: 10.18577 / 2071-9140-2017-0-S-306-317.
- Batienkov R.V., Efimochkin I.Yu., Khudnev A.A. The research of a specific electrical conductivity of Mo–W powder alloys obtained by SPS. Trudy VIAM, 2019, no. 7 (79), paper no. 06. Available at: http://www.viam-works.ru (accessed: January 09, 2020). DOI: 10.18577/2307-6046-2019-0-7-50-58.
- Sorokin O.Yu., Solntsev S.St., Evdokimov S.A., Osin I.V. Hybrid spark plasma sintering method: principle, possibilities, future prospects, Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 11–16. DOI: 10.18577/2071-9140-2014-0-s6-11-16.
- Noviyaanto A. Characteristics of SiCf/SiC hybrid composites fabricated by hot pressing and spark plasma sintering. Advances in Applied Ceramics, 2011, vol. 110, no. 7, pp. 375–382.
- Boldin M.S., Sakharov N.V., Shotin S.V. et al. Composite ceramics based on aluminum oxide, obtained by the method of electro-pulse plasma sintering for tribological applications. Vestnik Nizhegorodskogo universiteta named N.I. Lobachevsky, 2012, no. 6 (1), pp. 32–37.
- Sakharov K.A., Simonenko E.P., Simonenko N.P., Vaganova M.L., Lebedeva Yu.E., Chaynikova A.S., Osin I.V., Sorokin O. Yu., Grashchenkov D.V., Sevastyanov V.G., Kuznetsov N.T., Kablov E.N. Glycol-citrate synthesis of fine-grained oxides La2−xGdxZr2O7 and preparation of corresponding ceramics using FAST / SPS process. Ceramics International, 2018, vol. 44, no. 7, pp. 7647–7655.