Improvement of materials for sliding bearings of internal combustion engines (review)

Burkovskaya N.P., Sevostyanov N.V., Bolsunovskaya T.A., Efimochkin I.Yu.
Burkovskaya N.P., Sevostyanov N.V., Bolsunovskaya T.A., Efimochkin I.Yu. Improvement of materials for sliding bearings of internal combustion engines (review) // Proceedings of VIAM. 2020. No. 1. DOI: 10.18577/2307-6046-2020-0-1-78-91. URL: https://www.viam-works.ru/en/journal/2020/1/8
Keywords
sliding bearing, liner, sleeve, internal combustion engine, friction coefficient, wear, antifriction material, tribology, friction pair, tribological unit.
Abstract

The process of improving the materials of sliding bearings of internal combustion engines of cars is considered, depending on the requirements: from cast, multilayer, composite bearings to promising ceramic. The main world and domestic manufacturers of bearings of internal combustion engines are presented. Various types of bearing structures and manufacturing techniques for their manufacture are shown. The most efficient multilayer plain bearings are described. The paper presents the requirements for sliding bearing materials that determine the development of materials science in the field of antifriction materials for internal combustion engines.

Reference list
  1. Kragelsky I.V., Shchedrov V.S. The development of friction science. Moscow: Izd-vo AN SSSR, 1956. 235 p.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. GLYCO Engine Bearings: Catalogues // Federal-Mogul Motorparts. 2018. Available at: https://www.fmmotorparts.eu/support/pdf-catalogues.html?_ga=2.102842432.1741875717.1577256718-1992142891.1577256718 (accessed: October 08, 2019).
  4. Support sliding. Suspension and steering. Auto components: business, technology, service: multifunctional portal Max Media Group Publishing House, 2005. Available at: https://a-kt.ru/articles/opory-skolzheniya (accessed: October 08, 2019).
  5. Friction. Wear and Lubrication: handbook in 2 books / ed. I.V. Kragelsky, V.V. Alisin. Mocow: Mashinostroyeniye, 1978, book 1, 400 p.
  6. Kopeliovich D. Engine Bearing materials, 2019. Available at: http://www.subtech.com/docuwiki/doku.php?id=engine_bearing_materials (accessed: September 04, 2019).
  7. Kablov E.N. Materials of a new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  8. Kablov E.N. Without new materials – there is no future. Metallurg, 2013, no. 12, pp. 4–8.
  9. Climate and energy. Reducing emissions of CO2 and other greenhouse gases. WWF, 2019.Available at: https://wwf.ru/what-we-do/climate-and-energy/snizhenie-vybrosov-so2/ (accessed: October 08, 2019).
  10. Reducing emissions and friction... ABS Auto, 2014. Available at: https://abs-magazine.ru/article/snijaya-vibrosi-i-trenie (accessed: October 08, 2019).
  11. Multilayer composite material, manufacture and use: pat. 2354865 Rus. Federation; filed 05.08.04; publ. 10.05.09.
  12. Sliding element: pat. 2521854 Rus. Federation; filed 28.12.09; publ. 07.10.14.
  13. A method of manufacturing a composite material with a metal matrix: pat. 2536847 Rus. Federation; filed 27.10.10; publ. 27.12.14.
  14. A multilayer material for bearings: 2247658 Rus. Federation; filed 12.27.00; publ. 10.03.05.
  15. Multilayer composite material for plain bearings, manufacture and use: pat. 2354864 Rus. Federation; filed 05.08.04; publ. 10.05.09.
  16. The slip element and method of its manufacture (options): pat. 2573851 Rus. Federation; filed 12.10.11; publ. 27.01.16.
  17. Layered composite material for anti-friction structural elements and method for its production: pat. 2218277 Rus. Federation; filed 24.11.98; publ. 10.12.03.
  18. Calameo. Auto components, no. 7, 2015. Available at: https://ru.calameo.com/read/0047968704cb07bd44549 (accessed: October 08, 2019).
  19. Schichtverbundwerkstoff für Gleitelemente, Verfahren zu dessen Herstellung und Verwendung: раt. DE 102009019601; filed 30.04.09; publ. 12.05.10.
  20. Method for producing a spherical sliding surface of a plain bearing: pat. DE 102012209373; filed 04.06.12; publ. 21.07.16.
  21. Three-material roll-bonded sliding bearing having two aluminium layers: WO 2018177919; filed 23.03.18; publ. 04.10.18.
  22. Lead-free CuFe2P slide bearing material having a chip breaker: WO 2015158807; filed 16.04.15; publ. 22.10.15.
  23. Wear resistant lead free alloy bushing and method of making: WO 2009017501; filed 01.08.07; publ. 05.02.09.
  24. Nikishin V.N., Belokon K.G., Sibiryakov S.V. Sliding bearings in a car and engine building: textbook. Naberezhnye Chelny: Izd-vo Kamskoy gos. inzh.-ekon. akad, 2012, 213 p.
  25. Miba. Innovation in motion. Available at: https://www.miba.com/en/ (accessed: 10.24.2019).
  26. Vidin D.V., Kozyrev I.P., Korotkova L.P. Current trends in the production of liners of crankshafts of internal combustion engines // Tez. IX Vseros. nauch.-praktich. konf. molodykh uchenykh «Rossiya Molodaya» (Kemerovo, 18–21 apr. 2017). Kemerovo: KuzGTU, 2017. Available at: http://www.kuzstu.ru (accessed: October 08, 2019).
  27. Automotive industry. Aviation and astronautics. Koyo. Available at: https://www.koyo.eu/ru/2016-06-06-08-37-19/2016-06-06-08-31-30.html (accessed date: 08/10/2019).
  28. Slide bearing composite material: pat. US 7993758; filed 13.05.06; publ. 09.08.11.
  29. Sliding Bearing: pat. JP2004076756; filed 09.08.02; publ. 11.03.04.
  30. Sintered antifriction material based on copper: pat. 2326952 Rus. Federation; filed 07.11.06; publ. 20.06.08.
  31. A method of manufacturing products from aluminum bronze: pat. 2461447 Rus. Federation; filed 14.06.11; publ. 20.09.12.
  32. Anti-friction dispersion-hardened composite material: pat. 2203973 Rus. Federation; filed 04.08.99; publ. 10.05.03.
  33. Composite powder material for friction units: US Pat. 2245386 Ros. Federation; filed 16.12.03; publ. 27.01.05.
  34. Anti-friction composite powder material: US Pat. 2331685 Ros. Federation; filed 25.09.06; publ. 20.08.08.
  35. A method of manufacturing a high temperature composite antifriction material: pat. 2695854 Ros. Federation; filed 15.01.18; publ. 29.07.19.
  36. Copper-based alloy sliding-bearing material and preparation method thereof: pat. CN103602849; filed 10.10.13; publ. 09.03.16.
  37. Ceramic bearings. BearingCentre.RU. 2015. Available at: http://podshipnikcentr.ru/spravochnik/keramicheskie-podshipniki.html (accessed: October 08, 2019).
  38. Panov A.D., Panova I.M. Tribological features of structural ceramic materials in sliding bearings. Naukovedeniye: internet-zhurnal, 2015, vol. 7, no. 1. Available at: http://naukovedenie.ru/PDF/78TVN115.pdf (accessed: October 08, 2019). DOI: 10.15862/78TVN115.
  39. Bearings. TsIAM. Available at: http://www.ciam.ru/press-center/news/innovative-design-ciam-awarded-silver-medal-of-international-saloon-archimedes/ (accessed: October 22, 2019).
  40. Sliding bearing with nanostructured functional gradient gradient antifriction coating: pat. 2578840 Rus. Federation; filed 25.12.14; publ. 27.03.16.
  41. Wemhöner J., Bergrath B., Kreuser J. RolaMot – Erforschung des Einsatzes von Siliciumnitrid-Wälzlagern in einem Ottomotor zur Herabsetzung der inneren Motorreibung mit dem Ziel der Reduzierung des Kraftstoffverbrauchs und der CO2-Emissionen // Fraunhofer. Available at: http://edok01.tib.uni-hannover.de/edoks/e01fb08/558765742.pdf (accessed: October 22, 2019).
  42. Kuznetsov B.Yu., Sorokin O.Yu., Vaganova M.L., Osin I.V. Synthesis of model high-temperature ceramic matrices by the method of spark plasma sintering and the study of their properties for the production of composite materials. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 37–44. DOI: 10.18577/2071-9140-2018-0-4-37-44.
  43. Plastic Glide layer and Sliding Element with such: pat. US8357622; filed 14.09.07; publ. 22.01.13.
  44. Solomentseva A.V., Fadeeva V.M., Zhelezina G.F. Antifriktsionnye organoplastiki dlya tyazhelonagruzhennykh uzlov treniya skolzheniya aviatsionnykh konstruktsij [Antifriction organoplastics for heavy loaded sliding friction units of aircraft structures] // Aviacionnye materialy i tehnologii. 2016. №2 (41). S. 30–34. DOI: 10.18577/2071-9140-2016-0-2-30-34.
  45. Gatskov V.S., Gatskov S.V. Progressive technology for the manufacture of parts from antifriction materials: textbook, Moscow: NRNU MEPhI, 2011. 152 p.
  46. Farafonov D.P., Migunov V.P., Aleshina R.Sh. Tribotechnical characteristics research of materials used for gas turbine engines blade shroud hardening. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 24–30. DOI: 10.18577/2071-9140-2016-0-S1-24-30.