Construction of the diagram of isothermal transformations of thermosetting polymers on the example of the adhesive matrix

Naydenov D.D., Khaskov M.A., Petrova A.P.
Naydenov D.D., Khaskov M.A., Petrova A.P. Construction of the diagram of isothermal transformations of thermosetting polymers on the example of the adhesive matrix // Proceedings of VIAM. 2020. No. 1. DOI: 10.18577/2307-6046-2020-0-1-47-57. URL: https://www.viam-works.ru/en/journal/2020/1/5
Keywords
adhesive composition, curing, time–temperature–transformation diagram, curing curve, DSC, gelation, degree of conversion.
Abstract

The paper gives an idea of the processes taking place in the epoxy adhesive system during its curing. Kinetics of curing of thermosetting component of adhesive system by DSC method is investigated. A kinetic model of curing is proposed and experimentally confirmed. The dependence of the glass transition temperature on the degree of curing was determined experimentally. The analysis of the obtained experimental data is carried out and the diagram of isothermal transformations (TTT-diagram) of the studied composition is constructed. Isoconversion curves are applied to the resulting curve, which can be used to predict the storage time of the adhesive composition.

Reference list
  1. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE VIAM in the field of melt binders for polymer composite materials. Polimernyye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  2. Muhametov R.R., Dolgova E.V., Merkulova Yu.I., Dushin M.I. Development of heat-resistant bismaleimide binder for composites for aeronautical application. Aviacionnye materialy i tehnologii, 2014, No. 4, pp. 53–57. DOI: 10.18577/2071-9140-2014-0-4-53-57.
  3. Starostina I.V., Petrova A.P., Shevchenko Yu.N., Shishimirov M.V. Control thermoplastic binding for PCM (review). Trudy VIAM, 2019, no. 4 (76), paper no. 11. Available at: http://viam-works.ru (accessed: November 11, 2019). DOI: 10.18577 / 2307-6046-2019-0-4-99-107.
  4. Haskov M.A. The use of thermal analysis methods for constructing temperature – time – transformation diagrams of thermosetting polymers. Vysokomolekulyarnyye soyedineniya. Ser.: B, 2017, vol. 59, no. 1, pp. 37–48.
  5. Aleksashin V.M., Antyufeeva N.V., Bolshakov V.A. An experimental study of the relationship between calorimetric and rheological conversion during curing of an epoxy binder in adhesive rheology. Plasticheskiye massy, 2018, no. 9–10, pp. 29–32.
  6. Wendlandndt W. Thermal methods of analysis. Moscow: Mir, 1978. 527 p.
  7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  8. Kablov E.N. New Generation Materials. Zashchita i bezopasnost, 2014, no. 4, pp. 28–29.
  9. Grashhenkov D.V., Chursova L.V. Strategy of development of composite and functional materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 231–242.
  10. Enns J.B., Gillham J.K. Time-temperature-transformation (TTT) cure diagram: Modeling the cure behavior of thermosets. Journal of Applied Polymer Science, 1983, vol. 28, no. 8, pp. 2567–2591.
  11. Flammersheim H.-J., Opfermann J.R. Investigation of Epoxide Curing Reactions by Differential Scanning Calorimetry – Formal Kinetic Evaluation. Macromolecular Materials and Engineering, 2001, vol. 286, no. 3, pp. 143–150.
  12. Williams M., Landel R.F., Ferry J.D. The Temperature Dependence of Relaxation Mechanisms in Amorphous Polymers and Other Glass-forming Liquids. Journal of American Chemical Society, 1955, vol. 77, no. 14, pp. 3701–3707.
  13. Menczel J.D., Prime R.B. Thermal analysis of polymers: fundamentals and applications. Hoboke: John Wiley & Sons, 2009.68 p.
  14. Pascault J.P., Sautereau H., Verdu J. et al. Thermosetting polymers. New-York: Marcel Dekker AG, 2002. 447 p.
  15. Shatalova T.B., Shlyakhin O.A., Veryaeva E.V. Methods of thermal analysis: textbook.-method. allowance. Moscow: Moscow State University, 2011. 72 p.
  16. Zheleznyak V.G., Chursova L.V. Modification of binders and matrixes based on them to increase fracture toughness. Aviacionnye materialy i tehnologii, 2014, no. 1, pp. 47–50. DOI: 10.18577/2071-9140-2014-0-1-47-50.