Technologies of magneto-optical information recording in thin films of rare-earth magnetically soft alloys

Part I. Thermo-optical information recording
Piskorsky V.P., Valeev R.A., Korolev D.V., Stolyankov Yu.V., Morgunov R.B.
Piskorsky V.P., Valeev R.A., Korolev D.V., Stolyankov Yu.V., Morgunov R.B. Technologies of magneto-optical information recording in thin films of rare-earth magnetically soft alloys. Part I. Thermo-optical information recording // Proceedings of VIAM. 2020. No. 1. DOI: 10.18577/2307-6046-2020-0-1-24-37. URL: https://www.viam-works.ru/en/journal/2020/1/3
Keywords
magnetic anisotropy, rare-earth magnets, thin films, magnetic hysteresis.
Abstract

A review of the basics of modern thermo-magnetic and spin-polarization laser magneto-optical information recording technologies is presented. Alloys based on rare-earth (RE) and transition (TM) metals, due to the high degree of homogeneity of their magnetic and optical properties, have found practical application in superdense magneto-optical recordings. Discusses the principles and mechanism of magneto-optical recording and storage of information in thin RE–TM films. The magneto-optical characteristics for polycrystalline and amorphous alloys are compared depending on the film thickness, composition, and other structural parameters. The advantages of Gd–Fe–Co alloys for use in ultrafast optical magnetization reversal storage devices are formulated.

Reference list
  1. Chen D., Ready J.F., Bernal G.E. MnBi Thin Films: Physical Properties and Memory Applications. Journal of Applied Physics, 1968, vol. 39 (8), pp. 3916–3927. DOI: 10.1063/1.1656875.
  2. Williams H.J., Sherwood R.C., Foster F.G., Kelley E.M. Magnetic Writing on Thin Films of MnBi. Journal of Applied Physics, 1957, vol. 28 (10), pp. 1181–1184. DOI: 10.1063/1.1722603.
  3. Huth B.G. Calculations of Stable Domain Radii Produced by Thermomagnetic Writing. IBM Journal of Research and Development, 1974, vol. 18 (2), pp. 100–109. DOI: 10.1147/rd.182.0100.
  4. Mansuripur M. The Physical Principles of Magneto-optical Recording. Cambridge: Cambridge University Press, 1995. 776 p. DOI: 10.1017/CBO9780511622472.
  5. Beaurepaire E., Merle J.-C., Daunois A., Bigot J.-Y. Ultrafast Spin Dynamics in Ferromagnetic Nickel. Physical Review Letters, 1996, vol. 76 (22), pp. 4250–4253. DOI: 10.1103/physrevlett.76.4250.
  6. Egashira K., Yamada T. Kerr-effect enhancement and improvement of readout characteristics in MnBi film memory. Journal of Applied Physics, 1974, vol. 45 (8), pp. 3643–3648. DOI: 10.1063/1.1663831.
  7. Mansfield S.M., Kino G.S. Solid immersion microscope. Applied Physics Letters, 1990, vol. 57 (24), pp. 2615–2616. DOI: 10.1063/1.103828.
  8. Mansfield S.M., Studenmund W.R., Kino G.S., Osato K. High-numerical-aperture lens system for optical storage. Optics Letters, 1993, vol. 18 (4), pp. 305. DOI: 10.1364/ol.18.000305.
  9. Terris B.D., Mamin H.J., Rugar D., Studenmund W.R., Kino G.S. Near-field optical data storage using a solid immersion lens. Applied Physics Letters, 1994, vol. 65 (4), pp. 388–390. DOI: 10.1063/1.112341.
  10. Katayama H., Sawamura S., Ogimoto Y. et al. New Magnetic Recording Method Using Laser Assisted Read/Write Technologies. Journal of the Magnetics Society of Japan. 1999, vol. 23 (S_1_MORIS_99), pp. S1_233–236. DOI: 10.3379/jmsjmag.23.s1_233.
  11. Nemoto H., Saga H., Sukeda H., Takahashi M. High Density Thermomagnetic Recording on Flux Detectable RE-TM Media. Journal of the Magnetics Society of Japan. 1999. Vol. 23 (S_1_MORIS_99), pp. 229–232. DOI: 10.3379/jmsjmag.23.s1_229.
  12. Saga H., Nemoto H., Sukeda H., Takahashi M. A New Perpendicular Magnetic Recording Method with a Magnetic-Optical Common Preformat. Journal of the Magnetics Society of Japan, 1999, vol. 23, pp. 225. DOI: 10.3379/jmsjmag.23.S1_225.
  13. Chaudhari P., Cuomo J.J., Gambino R.J. Amorphous metallic films for magneto‐optic applications. Applied Physics Letters, 1973, vol. 22, pp. 337. DOI: 10.1063/1.1654662.
  14. Brown B.R. Optical Data Storage Potential of Six Materials. Applied Optics, 1974, vol. 13 (4). P. 761. DOI: 10.1364/ao.13.000761.
  15. Hasegawa R., Argyle B.E., Tao L.-J. Temperature dependence of magnetization in amorphous Gd–Co–Mo films. AIP Conference Proceedings, 1975, vol. 24, pp. 110. DOI: 10.1063/1.30006.
  16. Hiroyoshi H., Fukamichi K. Ferromagnetic-spin glass transition in Fe–Zr amorphous alloy system. Journal of Applied Physics, 1982, vol. 53 (3), pp. 2226–2228. DOI: 10.1063/1.330779.
  17. Ryan D.H., Coey J.M.D., Batalla E. et al. Magnetic properties of iron-rich Fe–Zr glasses. Physical Review B. 1987, vol. 35 (16), pp. 8630–8638. DOI: 10.1103/physrevb.35.8630.
  18. Takahashi M., Niihara T., Ohta N. Study on recorded domain characteristics of magneto-optical TbFeCo disks. Journal of Applied Physics, 1988, vol. 64 (1), pp. 262–269. DOI: 10.1063/1.341419.
  19. Oechsner H. Energieverteilungen bei der Festkörperzerstäubung durch Ionenbeschuß. Zeitschrift För Physik, 1970, vol. 238 (5), pp. 433–451. DOI: 10.1007/bf01409427.
  20. Suzuki Y., Takayama S., Kirino F., Ohta N. Single ion model for perpendicular magnetic anisotropy in RE–TM amorphous films. IEEE Transactions on Magnetics, 1987, vol. 23 (5), pp. 2275–2277. DOI: 10.1109/tmag.1987.1065290.
  21. Rhyne J.J. Bulk Magnetic Properties. Magnetic Properties of Rare Earth Metals, 1972, vol. 4. P. 129–182. DOI: 10.1007/978-1-4757-5691-3_4.
  22. Yu X.Y., Tsunashima S., Ban Y. et al. Simulation of thermomagnetic recording in rare earth-transition magnetic film using very small laser spot. Magnetics Society of Japan, 1998, vol. 22. P. 129–132. DOI: 10.3379/jmsjmag.22.S2_129.
  23. Carcia P.F., Meinhaldt A.D., Suna A. Perpendicular magnetic anisotropy in Pd/Co thin film layered structures. Applied Physics Letters, 1985, vol. 47 (2), pp. 178–180. DOI: 10.1063/1.96254.
  24. Zeper W.B., van Kesteren H.W., Jacobs B.A.J. et al. Hysteresis, microstructure, and magneto-optical recording in Co/Pt and Co/Pd multilayers. Journal of Applied Physics, 1991, vol. 70 (4), pp. 2264–2271. DOI: 10.1063/1.349419.
  25. Fujiwara Y., Masaki T., Yu X. et al. Structural and Magnetic Anisotropy of Tb/Fe Multilayers. Japanese Journal of Applied Physics, 1997, vol. 36. Part 1. No. 8, pp. 5097–5102. DOI: 10.1143/jjap.36.5097.
  26. Kablov E.N., Piskorsky V.P., Burkhanov G.S., Valeev R.A., Moiseeva N.S., Stepanova S.V., Petrakov A.F., Tereshina I.S., Repina M.V. Thermostable ring magnets with a radial texture based on Nd (Pr)–Dy–Fe–Co–B. Physics and chemistry of materials processing, 2011, vol. 3, pp. 43–47. Available at: viam.ru/public/files/2011/2011-205746.pdf (accessed: September 18, 2019).
  27. Kablov E.N., Ospennikova O.G., Rezchikova I.I., Piskorskij V.P., Valeev R.A., Korolev D.V. Properties dependence of the Nd–Dy–Fe–Co–B sintered materials on technological parameters. Aviacionnye materialy i tehnologii, 2015, no. S2 (39), pp. 24–29. DOI: 10.18577/2071-9140-2015-0-S2-24-29.
  28. Kablov E.N., Ospennikova O.G., Korolev D.V., Piskorskij V.P., Valeev R.A., Rezchikova I.I. Influence mechanisms of boron content and heat treatment on the properties of Nd–Fe–Al–Ti–B magnets. Aviacionnye materialy i tehnologii, 2015, no. S2 (39), pp. 30–34. DOI: 10.18577/2071-9140-2015-0-S2-30-34.
  29. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  30. Piskorsky V.P., Valeev R.A., Korolev D.V., Morgunov R.B., Rezchikova I.I. Terbium and gadolinium dopin g influence on thermal stability and magnetic properties of sintered magnets Pr–Tb–Gd–Fe–Co–B. Trudy VIAM, 2019, no. 7 (79), paper no. 07. Available at: http://www.viam-works.ru (accessed: September 18, 2019). DOI: 10.18577/2307-6046-2019-0-7-59-66.