The effect of reinforcing epoxy film adhesive VK-51 with non-woven fibrous material on its properties

Petrova A.P., Lukina N.F., Rubtsova E.V., Isaev A.Yu.
Petrova A.P., Lukina N.F., Rubtsova E.V., Isaev A.Yu. The effect of reinforcing epoxy film adhesive VK-51 with non-woven fibrous material on its properties // Proceedings of VIAM. 2019. No. 9. DOI: 10.18577/2307-6046-2019-0-9-47-56. URL: https://www.viam-works.ru/en/journal/2019/9/5
Keywords
adhesive, adhesive primer, reinforced adhesive, resource characteristics, adhesive joints, strength of adhesive joints
Abstract

The properties of VK-51 high-strength film adhesive are given. The effect of reinforcement with nonwoven fabric based on mylar and viscose fibers on the properties of VK-51 adhesive is shown and the properties of reinforced adhesive (VK-51A) are given. A comparison of the properties of VK-51A adhesive with an imported analogue of AF-126 adhesive is given. The effect of the adhesive primer EP-0234 on the resource characteristics of adhesive joints made with VK-51A adhesive in combination with soil is shown.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Rossiya na rynke intellektualnykh resursov [Russia in the market of intellectual resources] // Ekspert. 2015. №28 (951). S. 48–51.
  3. Kablov E.N. Iz chego sdelat budushchee? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future of? Materials of a new generation, technologies for their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  4. Dementeva L.A., Bocharova L.I., Lukina N.F., Petrova A.P. Vysokoprochnye plenochnye klei VK-51 i VK-51A [High-strength film adhesives VK-51 and VK-51A] // Klei. Germetiki. Tekhnologii. 2015. №4. S. 17–19.
  5. Zhadova N.S., Tyumeneva T.Yu., Sharova I.A., Lukina N.F. Perspektivnye tehnologii dlya vremennogo operativnogo remonta aviacionnoj tehniki [Perspective technologies for field repair if aviation engineering] // Aviacionnye materialy i tehnologii. 2013. №2. S. 67–70.
  6. Laptev A.B., Barbotko S.L., Nikolaev E.V. Osnovnye napravleniya issledovanij sokhranyaemosti svojstv materialov pod vozdejstviem klimaticheskikh i ekspluatatsionnykh faktorov [The main research areas of the persistence properties of materials under the influence of climatic and operational factors] // Aviacionnye materialy i tehnologii. 2017. №S. S. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
  7. Lukina N.F., Petrova A.P., Muhametov R.R., Kogtjonkov A.S. Novye razrabotki v oblasti kleyashhih materialov aviacionnogo naznacheniya [New developments in the field of adhesive aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 452–459. DOI: 10.18577/2071-9140-2017-0-S-452-459.
  8. Petrova A.P., Lukina N.F., Pavlyuk B.F., Isaev A.Yu., Besednov K.L. Napolniteli dlya tokoprovodyashchikh kleEv (obzor literatury) [Fillers for conducting glues (literature review)] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2017. №5–6 (28). St. 06. Available at: http://www.materialsnews.ru (accessed: August 09, 2019).
  9. Petrova A.P., Nikolaev E.V., Lukina N.F., Isaev A.Yu. Klimaticheskaya stoykost kleevykh soedineniy, vypolnennykh epoksidnymi kleyami, v razlichnykh klimaticheskikh zonakh [Climatic resistance of adhesive joints made with epoxy adhesives in various climatic zones] // Klei. Germetiki. Tekhnologii. 2019. №4. S. 16–22.
  10. Sorokin A.E., Beyder E.Ya., Perfilova D.N. Vliyanie klimaticheskikh faktorov na svoystva ugleplastika na polifenilensulfidnom svyazuyushchem // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2015. №1. St. 10. URL: http://viam-works.ru (data obrashcheniya: 09.08.2019). DOI: 10.18577/2307-6046-2015-0-1-10-10.
  11. Sorokin A.E., Bejder E.Ya., Izotova T.F., Nikolaev E.V., Shvedkova A.K. Issledovanie svojstv ugleplastika na polifenilensulfidnom svyazuyushhem posle uskorennyh i naturnyh klimaticheskih ispytanij [Investigation of carbon fiber reinforced plastic on polyphenylenesulfide resin after accelerated and natural climatic test] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 66–72. DOI: 10.18577/2071-9140-2016-0-3-66-72.
  12. Sytov V.A., Verstakov A.E., Voronin A.E., Sytov V.V. Sovremennye sinteticheskie klei na osnove epoksikauchukovykh kompozitsiy [Modern synthetic adhesives based on epoxy rubber compositions] // Klei. Germetiki. Tekhnologii. 2012. №9. S. 6–9.
  13. Sytov V.A., Sytov V.V., Vettegren V.I. Temperaturnaya zavisimost prochnosti kleevykh soedineniy stali na osnove epoksikauchukovykh kleev [Temperature dependence of the strength of adhesive joints of steel based on epoxy rubber adhesives] // Tez. dokl. Mezhdunar. nauch.-tekhnich. konf. «SovremennyE dostizheniya v oblasti kleev i germetikov. Materialy, syre, tekhnologii» (Dzerzhinsk, 17–19 sent., 2013 g.), 2013. S. 50–52.
  14. Tkachuk A.I., Terekhov I.V., Kudryavtseva A.N., Grigoreva K.N. Ispolzovanie reologicheskikh metodov issledovaniya pri otverzhdenii epoksidnykh svyazuyushchikh [The use of rheological research methods in the curing of epoxy binders] // Klei. Germetiki. Tekhnologii. 2018. №2. S. 15–20.
  15. Tsverava V.G., Rusin M.Yu., Nepovinnykh V.I., Khimitsaev A.S. Analiz vliyaniya uskorennogo klimaticheskogo stareniya na prochnost kleevykh soedineniy [Analysis of the effect of accelerated climatic aging on the strength of adhesive joints] // Klei. Germetiki. Tekhnologii. 2018. №8. S. 28–31.
  16. Kochergin Yu.S., Grigorenko T.I. Dinamicheskie mekhanicheskie svoystva epoksidnykh kleevykh kompozitsiy, napolnennykh molotym karbonatom kaltsiya [Dynamic mechanical properties of epoxy adhesive compositions filled with ground calcium carbonate] // Klei. Germetiki. Tekhnologii. 2018. №2. S. 35–44.
  17. Petrova A.P., Anikhovskaya L.I. Vliyanie adgezionnogo grunta EP-0234 na svoystva kleevykh soedineniy, vypolnennykh fenolno-kauchukovym kleem VK-50 [Effect of adhesive primer EP-0234 on the properties of adhesive joints made with phenolic-rubber adhesive VK-50] // Klei. Germetiki. Tekhnologii. 2016. №1. S. 19–24.
  18. Lukina N.F., Dementeva L.A., Petrova A.P., Anihovskaya L.I. Kleyashhie materialy v konstrukcii lopastej vertoletov [Gluing materials in the design of blades of helicopters] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 07. Available at: http://www.viam-works.ru (accessed: August 12, 2019). DOI: 10.18577/2307-6046-2016-0-7-7-7.
  19. Khrychev Yu.I., Shkodinova E.P., Magin N.A., Dementeva L.A., Khayretdinov R.Kh., Kutsevich K.E. Razrabotka tekhnologicheskogo protsessa izgotovleniya radioprozrachnogo obtekatelya iz kleevykh prepregov tipa KMKS-2M.120 [Development of a technological process for manufacturing a radiolucent fairing from adhesive prepregs of the KMKS-2M.120 type] // Klei. Germetiki. Tekhnologii. 2013. №2. S. 27–30.
  20. Startsev V.O., Kutsevich K.E., Khrulev K.A., Molokov M.V. Prognozirovanie temperatury poverkhnosti obraztsov kompozitsionnykh materialov na osnove kleevykh prepregov pri eksponirovanii v klimaticheskikh usloviyakh [Prediction of surface temperature of samples of composite materials based on adhesive prepregs when exposed to climatic conditions] // Klei. Germetiki. Tekhnologii. 2017. №9. S. 24–31.